A516Gr70+316L qoplangan po'lat plitalar

A516Gr70+316L qoplangan po'lat plitalar

Kengligi: Maks 2500 mm
Qalinligi: Umumiy qalinligi: 5-50 mm
(qoplama materialining qalinligi: 1-10 mm)
Uzunligi: Maks 15000 mm
So'rov yuborish
Hozir chat
Ta'rif
Texnik parametrlar

A516Gr70+316L Qoplangan po'lat plitalar Kimyoviy tarkibi va mexanik xususiyatlari

 

ASTM A516 70-sinf Kimyoviy tarkibi

Baho

Maksimal element (%)

C

Si

Mn

P

S

ASTM A516 darajasi 70

         

Qalin<12.5mm

0,27 maks

0.15–0.40

0.85–1.20

0.035

0.035

Qalinligi 12,5-50 mm

0,27 maks

0.15–0.40

0.85–1.20

0.035

0.035

Qalinligi 50-100 mm

0,27 maks

0.15–0.40

0.85–1.20

0.035

0.035

Qalinligi 100-200 mm

0,27 maks

0.15–0.40

0.85–1.20

0.035

0.035

Thick>200 mm

0,27 maks

0.15–0.40

0.85–1.20

0.035

0.035

 

Element

Foiz (%)

Uglerod (C)

0,27 maks

Marganets (Mn)

0.85–1.20

Fosfor (P)

0,035 maksimal

Oltingugurt (S)

0,035 maksimal

Kremniy (Si)

0.15–0.40

Nikel (Ni)

0,40 maksimal (ixtiyoriy)

Xrom (Cr)

0,30 maksimal (ixtiyoriy)

Molibden (Mo)

0,08 maksimal (ixtiyoriy)

 

Baho

 

ASTM A516 70-sinfMexanik xususiyat

Qalinligi

Yo'l bering

Kuchlanish

Cho'zilish

ASTM A516 darajasi 70

mm

Min Mpa

Mpa

Min %

6-40

260

485-620

21%

40-100

260

485-620

17%

 

Baho

 

C

 

Mn

 

P

 

 

S

 

 

Si

 

Cr

Ni Mo Ni

 

Kuper

 

316L(S31603) 0.030 2.0 0.045 0.030 0.75 16.0-18.0 10.0-14.0 2.00-3.00 0.10 -
Baho

Hosildorlik kuchi

(N/mm2), min

Kuchlanish kuchi (N/mm2), min

2 dyuymda (50 mm) cho'zilish, %, min
Qattiqlik, maks
Brinell Rokvell B
Sovuq egilish

Ostenitik (xrom-nikel) (xrom-marganets-nikel)

316L(S31603)
25 170
70 485
40
217 95
shart emas

 

A516Gr70+316L Qoplangan po'lat plitalar Qo'llanilishi

 

Kimyo sanoati:

Kislota saqlash tanklari: 5–20% sulfat kislota va xlorid-to'ldirilgan oqava suvlarga chidamli.

Reaktorlar: Yuqori bosim va harorat ostida organik sintezni boshqaring.

 

Neft va gaz:

Hydrocracking birliklari: A516Gr70 strukturaning yaxlitligini ta'minlaydi, 316L esa H₂S va xlorid korroziyasiga qarshilik ko'rsatadi.

Dengiz osti quvurlari: Dengiz suvi va yuqori-bosimli uglevodorod suyuqliklariga bardosh beradi.

 

Dengiz muhandisligi:

Tuzsizlantirish oʻsimliklari: shoʻr suv va xlor{0}}asosidagi dezinfektsiyalash vositalariga qarshilik koʻrsatadi.

Kema tanklari: Yoqilg'i yoki dengiz suvini minimal korroziya bilan saqlang.

 

Oziq-ovqat va farmatsevtika:

Qayta ishlash uskunalari: gigiena bo'yicha FDA standartlariga javob bering (Ra 1,6 mkm dan kam yoki unga teng) va tozalash vositalariga qarshilik ko'rsating.

 

A516Gr70+316L Qoplangan po'lat plitalar Boshqa nomi

 

A516Gr70+316L Qoplangan po'lat plitalar, A516Gr70 po'lat plitalar, 316L po'lat plitalar

 

Maxsus ish sharoitida texnologik innovatsiyalar

 

Past haroratli-muhitlarda payvandlash
Atrof-muhit harorati bo'lganda<0°C, additional preheating to 200–250°C is required, and the "multi-layer and multi-pass welding" method should be adopted, with the interpass temperature maintained at 150–200°C.
Vodorod tarqalishini tezlashtirish uchun payvandlashdan keyin-post isitish (250–300 daraja, 1 soat ushlab turish) darhol amalga oshirilishi kerak.

 

Yuqori korroziv vositalardan himoya qilish
Transition Layer Upgrade: In environments with Cl⁻ concentration >1000ppm, o'tish qatlami uchun ER NiCrMo-3 (Inconel 625) dan foydalanish tavsiya etiladi, u 9-10% Mo ni o'z ichiga oladi va 40 dan katta yoki teng bo'lgan chuqurlikka qarshilik ekvivalent soniga (PREN) ega.
Yuzaki qoplama: Payvandlashdan so'ng, qoplama qatlamining yuzasi epoksi qatroni / alumina kompozit qoplamasi (qalinligi 150-200 mkm) bilan püskürtülür. Tuz purkash testida (ASTM B117) korroziyaga chidamlilik vaqti 5000 soatdan oshadi.

CSP Paramlarini so'rang

 

Farmatsevtika/oziq-ovqat sanoatidagi sanitariya bosimli idishlar uchun (masalan, steril dori saqlash idishlari, sut mahsulotlarini qayta ishlash uskunalari) biz Q345B+304L Qoplangan po'lat yoki TSG 21 va oziq-ovqat-standartlariga javob beradigan Q235B+304 Qoplangan po'latni taqdim etamiz. Agar siz sirt pürüzlülüğü talablarini, sanitariya armaturalari bilan payvandlashni bilishingiz yoki moslashtirilgan ichki bo'shliqlar uchun ishlov berish xarajatlarini hisoblashingiz kerak bo'lsa, professional maslahat va sertifikatlash hujjatlari uchun so'rov yuboring.

Email:alloy@gneesteelgroup.com

Whatsapp (WeChat): +86 15824687445

 

product-479-458product-407-398product-407-325product-420-297

Issiq teglar: a516gr70+316l qoplangan po'lat plitalar, Xitoy a516gr70+316l qoplangan po'lat plitalar ishlab chiqaruvchilari, etkazib beruvchilari, zavodi