Tozalangan metall plitalar

Tozalangan metall plitalar

Ob-havoga chidamli po'lat plitalar, po'lat plitalar korroziyali po'latning atmosfera korroziyasiga chidamli bo'lib, manba Shimoliy Amerikaning Paxta po'lat plitasi bo'lib, u oddiy po'lat va zanglamaydigan po'lat plitalar orasidagi material orasidagi past qotishma po'lat plitalar qatoriga kiradi.
So'rov yuborish
Hozir chat
Ta'rif
Texnik parametrlar

Tozalangan metall plitalar


Ob-havoga chidamli po'lat plitalar, po'lat plitalar korroziyali po'latning atmosfera korroziyasiga chidamli bo'lib, manba Shimoliy Amerikaning Paxta po'lat plitasi bo'lib, u oddiy po'lat va zanglamaydigan po'lat plitalar orasidagi material orasidagi past qotishma po'lat plitalar qatoriga kiradi.

 

Ob-havoga chidamli po'lat plitalar odatda yuqori quvvatga ega, plastiklik ham juda yaxshi, noyob metall porlashi va boshqa xususiyatlarga ega, korroziyaga chidamli{0}} aşınmaya bardoshli, kundalik parvarishlash, mahsulot katta egiluvchanlikka ega, ayniqsa fabrikalarning-katta miqyosda foydalanish uchun mos keladi va ob-havoga chidamli po'lat plitalarni qayta ishlash-hali ham juda yaxshi atrof-muhit muhofazasi.

 

Fosfor, mis, nikel, xrom va boshqa korroziyaga chidamli-zararli elementlar kabi korroziyaga qarshi elementlar qo'shilganligi sababli, po'lat plastinka va zich zang qatlamining yuzasi o'rtasida kuchli yopishish hosil bo'lishi uchun zang qatlami etarlicha zich bo'lib, suvni sezilarli darajada izolyatsiya qilish, korroziyani sezilarli darajada tezlashtiradi. yuqori sifatli po'lat, qattiq, plastik cho'zish, qoliplash, payvandlash va kesish va boshqa xususiyatlarga ega.

 

 
Biz taqdim eta oladigan EN standart ob-havoga chidamli po'lat plitalar navlarini o'z ichiga oladi

 

UZ

S235J0W

S235J2W

S355J0WP

S355J2WP

S355J0W

S355J2W

S355K2W

S355J2G1W

S355J2G2W

S355J2G2W

S355K2G1W

S355K2G2W

1.8958

1.8961

1.8945

1.8946

1.8959

1.8965

1.8967

Fe360CKI

Fe360DKI

Fe510C1KI

Fe510D1KI

Fe510C2KI

Fe510D2KI

E24W3

E24W4

E36WA3

E36WA4

E36WB3

E36WB4

WR50A

WR50B

WR50C

WTSt37-3

WTSt52-3

 

 
EN standart korten po'lat materialining kimyoviy tarkibi

 

Ga binoan C %
maks.
Si %
maks.
Mn % P % S %
maks.
N %
maks.
Cr % Cu % V% Ni% Z% Mo%
EN standarti                        
S235J0W 0.13 0.40 0.20-0.60 0.04 0.04 0.01 0.40-0.80 0.25-0.55 - 0.65 - -
S235J2W 0.13 0.40 0.20-0.60 0.04 0.03 - 0.40-0.80 0.25-0.55 - 0.65 - -
S355J0W 0.12 0.75 1.00 0.06-0.15 0.04 0.01 0.30-1.25 0.25-0.55 - 0.65 - -
S355J2WP 0.12 0.75 1.00 0.06-0.15 0.03 - 0.30-1.25 0.25-0.55 - 0.65 - -
S355J0W 0.16 0.50 0.50-1.50 0.04 0.04 0.01 0.40-0.80 0.25-0.55 - 0.65 0.15 0.30
S355J2W 0.16 0.50 0.50-1.50 0.03 0.03 - 0.40-0.80 0.25-0.55 - 0.65 0.15 0.30
S355K2W 0.16 0.50 0.50-1.50 0.03 0.03 - 0.40-0.80 0.25-0.55 - 0.65 0.15 0.30

 

 
korten nurash po'lat Mahsulotlar tasviri

 

China weathering plate Distributors

 

 
GNEE guruhi jamoasi fotosurati

 

China corten sheet Suppliers

 

 
GNEE guruhi mijozlariga tashrif

 

China plate corten steel Manufacturers

 

 
GNEE Group xorijiy po'lat ko'rgazmalarida ishtirok etadi

 

China weathering corten steel Distributors