A36 karbonli po'lat plitalar
A36 - kimyoviy tarkibi va mexanik xususiyatlari Amerika ASTM standartlariga mos keladigan uglerodli strukturaviy po'lat plitalar. Ushbu turdagi po'lat plitalar yaxshi mexanik xususiyatlarga, payvandlash ko'rsatkichlariga va korroziyaga chidamliligiga ega va qurilish, ko'priklar, mashinasozlik va boshqa sohalarda keng qo'llaniladi.
Q235Karbonli po'lat plitalar
Q235 steel is equivalent to Japenese steel grade SS400 in application, the only difference is that ss400 steel requires only S,P composition < 0.050, Q235 has requirements for More element C, Si, Mn, S, P. Yield strength of q235 is >235Mpa, bu SS400 245Mpa bilan deyarli bir xil. Q ushbu materialning rentabelligini bildiradi, ikkinchisi 235, bu materialning rentabellik qiymatini bildiradi, taxminan 235MPA. Po'lat plitaning qalinligi oshishi bilan rentabellik qiymati pasayadi. Qurilish va muhandislik inshootlarida keng qo'llaniladi.
S235JRKarbonli po'lat plitalar
S235JR Yevropa standarti EN 10025-2 boʻyicha{1}}qotishma boʻlmagan strukturaviy poʻlatdir., umumiy qurilish va muhandislik uchun ishlatiladi. "S" konstruktiv, "235" esa 235𝑁/𝑚𝑚2 minimal oqish quvvatini bildiradi., va "JR" 27𝐽 minimal zarba energiyasini bildiradida20 daraja 𝐶. Bu ko'p qirrali va tejamkor material bo'lib, yaxshi payvandlanishi bilan mashhur va mexanik xususiyatlari uni ko'priklar, binolar va mashinalar kabi ilovalar uchun mos qiladi.
Mahsulot parametrlari
| Mahsulot nomi | A36/Q235/S235JR Karbonli po'lat plitalar |
| Ishlab chiqarish jarayoni | Issiq prokat, sovuq prokat |
| Materiallar standartlari | AISI, ASTM, ASME, DIN, BS, EN, ISO, JIS, GOST, SAE va boshqalar. |
| Kengligi | 100-3000 mm |
| Uzunlik | 1m-12m yoki moslashtirilgan o'lcham |
| Qalinligi | 0,1 mm-400 mm |
| Yetkazib berish shartlari | Rolling, tavlanish, söndürme, temperli yoki standart |
| Yuzaki jarayon | Oddiy, simli chizilgan, laminatlangan plyonka |
Kimyoviy tarkibi
| C | Cu | Fe | Mn | P | Si | S |
| 0.25~0.290 | 0.20 | 98.0 | 1.03 | 0.040 | 0.280 | 0.050 |
Mexanik xususiyatlar
| A36 | Kuchlanish kuchini cheklash | Cho'zilish kuchi, hosildorlik kuchi | Uzilishdagi cho'zilish (birlik: 200 mm) | Uzilishdagi cho'zilish (birlik: 50 mm) | Elastiklik moduli | Ommaviy modul (po'lat uchun odatiy) | Puasson nisbati | Kesish moduli |
| Metrik | 400~550 MPa | 250 MPa | 20.0% | 23.0 % | 200 GPa | 140 GPa | 0.260 | 79,3 GPa |
| Imperator | 58000 ~ 79800 psi | 36300 psi | 20.0% | 23.0 % | 29000 ksi | 20300 ksi | 0.260 | 11500 ksi |
Jismoniy ishlash
| Jismoniy ishlash | Metrik | Imperator |
| Zichlik | 7,85 g/sm3 | 0,284 funt/dyuym3 |
Jismoniy ishlash
Ko'priklar, binolar va neft burg'ulash qurilmalari uchun murvatli, perchinli yoki payvandlangan konstruktsiyalar.
Saqlash tanklari, siloslar, rulman plitalari, armatura, halqalar, shablonlar, armatura, tishli tishli vintlar, tishli g'ildiraklar, pastki plitalar, zarblar, pardozlash muhandisligi, qoziqlar, qavslar, avtomobillar va qishloq xo'jaligi uskunalari, ramkalar, mexanik qismlar va boshqalarni shakllantirish uchun ishlatiladi.
Ekvivalent material
| Milliy standart GB | Evropa standarti EN | Amerika standarti ASTM | Germaniya standarti DIN, WNr | Yaponiya standarti JIS | Fransuz standarti AFNOR | Britaniya standarti BS | Kanada HG |
| Q235B | S235JR | A283C | St37-2 | SM400A | E24-2 | 40A/40B | 230G |
| Italiya UNI | Hindiston IS | Shveytsariya SS | Avstraliya ONORM | Norvegiya NS | Ispaniya UNE | Xalqaro standartlar ISO | Portugaliya NP |
| Fe360B | IS2062 | 1311/1312 | RSt360B | NS12123 | AE235B-FN | E235B / Fe360B | FE360-B |
Birja ekrani

Tekshirish va qadoqlash


Agar siz GNEE mahsulotlari haqida ko'proq bilmoqchi bo'lsangiz, elektron pochta manziliga xat yuborishingiz mumkinalloy@gneesteelgroup.com. Biz sizga yordam berishdan xursandmiz.
TSS
Savol: Sizning kompaniyangizning asosiy mahsulotlari/xizmatlari nima?
Javob: Biz karbonli po'lat, qotishma po'lat va profil mahsulotlari uchun professional ishlab chiqaruvchilarmiz. Bizda 17+ yildan ortiq po'lat biznesi bo'yicha tajribamiz bor va mahsulotimiz O'rta Sharq, Janubiy Amerika, Janubi-Sharqiy Osiyo, Afrika, Janubiy va Sharqiy Osiyo va boshqalarga eksport qilinadi.
Savol: Sizning fabrikangizga tashrif buyurishim mumkinmi?
Javob: Albatta, biz butun dunyo bo'ylab mijozlarni fabrikamıza tashrif buyurish uchun kutib olamiz.
Savol: Sizning to'lov shartlari qanday?
Javob: 30% T / T depozit va jo'natishdan oldin 70% balans.
Savol: Sizning yetkazib berish vaqtingiz qancha?
Javob: Qimmatli qog'ozlar uchun biz depozitni olganimizdan keyin 7 kun ichida yukni yuklash portiga olib o'tishimiz mumkin; Ishlab chiqarish uchun odatda depozitni olgandan keyin taxminan 15-30 kun davom etadi.
Savol: Siz namunalar berasizmi? Ular bepulmi yoki pullikmi?
Javob: Namunalar bepul, ammo kurerlik yuki mijoz hisobi bilan qoplanadi.
Savol: Siz uchinchi tomon tekshiruvini qabul qilasizmi?
Javob: Ha, biz uchinchi tomon tekshiruvlarini-to‘liq qabul qilamiz.
Savol: Nega boshqa etkazib beruvchilardan emas, sizdan sotib olishim kerak?
Javob: Xitoy po‘lat sanoatining yuqori resurslarini birlashtirgan holda, biz mijozlarga yuqori sifatli po‘latdan yasalgan mahsulotlarni imtiyozli narxlarda-ta’minlaymiz va tovarlar mijozlarga o‘z vaqtida yetkazib berilishini ta’minlay olamiz.
Savol: Sifatga qanday kafolat bera olasiz?
Javob: Har doim ommaviy ishlab chiqarishdan oldin{0}}ishlab chiqarishdan oldingi namuna; Yuk tashishdan oldin har doim 100% tekshiriladi
| GNEE tomonidan ta'minlangan uglerod va past{0}}qotishma yuqori-po'latlar navlari | |||||
| ASTM/ASME | ASTM A36/A36M | ASTM A36 | |||
| ASTM A283/A283M | ASTM A283 A darajasi | ASTM A283 B darajasi | ASTM A283 C darajasi | ASTM A283 D darajasi | |
| ASTM A514/A514M | ASTM A514 A darajasi | ASTM A514 B darajasi | ASTM A514 C darajasi | ASTM A514 E darajasi | |
| ASTM A514 F darajasi | ASTM A514 H darajasi | ASTM A514 J darajasi | ASTM A514 K darajasi | ||
| ASTM A514 M darajasi | ASTM A514 P darajasi | ASTM A514 Q darajasi | ASTM A514 R darajasi | ||
| ASTM A514 S darajasi | ASTM A514 T darajasi | ||||
| ASTM A572/A572M | ASTM A572 42-sinf | ASTM A572 50-darajali | ASTM A572 55-sinf | ASTM A572 60-sinf | |
| ASTM A572 65-sinf | |||||
| ASTM A573/A573M | ASTM A573 58-sinf | ASTM A573 65-sinf | ASTM A573 70-sinf | ||
| ASTM A588/A588M | ASTM A588 A darajasi | ASTM A588 B darajasi | ASTM A588 C darajasi | ASTM A588 K darajasi | |
| ASTM A633/A633M | ASTM A633 A darajasi | ASTM A633 C darajasi | ASTM A633 D darajasi | ASTM A633 E darajasi | |
| ASTM A656/A656M | ASTM A656 50-darajali | ASTM A656 60-sinf | ASTM A656 70-sinf | ASTM A656 80-sinf | |
| ASTM A709/A709M | ASTM A709 36-sinf | ASTM A709 50-darajali | ASTM A709 50S darajasi | ASTM A709 darajasi 50 Vt | |
| ASTM A709 darajasi HPS 50W | ASTM A709 darajasi HPS 70W | ASTM A709 100-darajali | ASTM A709 darajasi 100 Vt | ||
| ASTM A709 darajasi HPS 100W | |||||
| ASME SA36/SA36M | ASME SA36 | ||||
| ASME SA283/SA283M | ASME SA283 A darajasi | ASME SA283 B darajasi | ASME SA283 C darajasi | ASME SA283 D darajasi | |
| ASME SA514/SA514M | ASME SA514 A darajasi | ASME SA514 B darajasi | ASME SA514 C darajasi | ASME SA514 E darajasi | |
| ASME SA514 F darajasi | ASME SA514 H darajasi | ASME SA514 J darajasi | ASME SA514 K darajasi | ||
| ASME SA514 M darajasi | ASME SA514 P darajasi | ASME SA514 Q darajasi | ASME SA514 R darajasi | ||
| ASME SA514 S darajasi | ASME SA514 T darajasi | ||||
| ASME SA572/SA572M | ASME SA572 42-sinf | ASME SA572 50-sinf | ASME SA572 55-sinf | ASME SA572 60-sinf | |
| ASME SA572 65-sinf | |||||
| ASME SA573/SA573M | ASME SA573 58-sinf | ASME SA573 65-sinf | ASME SA573 70-sinf | ||
| ASME SA588/SA588M | ASME SA588 A darajasi | ASME SA588 B darajasi | ASME SA588 C darajasi | ASME SA588 K darajasi | |
| ASME SA633/SA633M | ASME SA633 A darajasi | ASME SA633 C darajasi | ASME SA633 D darajasi | ASME SA633 E darajasi | |
| ASME SA656/SA656M | ASME SA656 50-sinf | ASME SA656 60-sinf | ASME SA656 70-sinf | ASME SA656 80-sinf | |
| ASME SA709/SA709M | ASME SA709 36-sinf | ASME SA709 50-sinf | ASME SA709 50S darajasi | ASME SA709 darajasi 50W | |
| ASME SA709 darajasi HPS 50W | ASME SA709 darajasi HPS 70W | ASME SA709 100-sinf | ASME SA709 darajasi 100 Vt | ||
| ASME SA709 darajasi HPS 100W | |||||
| EN10025 | EN10025-2 | EN10025-2 S235J0 | EN10025-2 S275J0 | EN10025-2 S355J0 | EN10025-2 S355K2 |
| EN10025-2 S235JR | EN10025-2 S275JR | EN10025-2 S355JR | EN10025-2 S420J0 | ||
| EN10025-2 S235J2 | EN10025-2 S275J2 | EN10025-2 S355J2 | |||
| EN10025-3 | EN10025-3 S275N | EN10025-3 S355N | EN10025-3 S420N | EN10025-3 S460N | |
| EN10025-3 S275NL | EN10025-3 S355NL | EN10025-3 S420NL | EN10025-3 S460NL | ||
| EN10025-4 | EN10025-4 S275M | EN10025-4 S355M | EN10025-4 S420M | EN10025-4 S460M | |
| EN10025-4 S275ML | EN10025-4 S355ML | EN10025-4 S420ML | EN10025-4 S460ML | ||
| EN10025-6 | EN10025-6 S460Q | EN10025-6 S460QL | EN10025-6 S460QL1 | EN10025-6 S500Q | |
| EN10025-6 S500QL | EN10025-6 S500QL1 | EN10025-6 S550Q | EN10025-6 S550QL | ||
| EN10025-6 S550QL1 | EN10025-6 S620Q | EN10025-6 S620QL | EN10025-6 S620QL1 | ||
| EN10025-6 S690Q | EN10025-6 S690QL | EN10025-6 S690Q1 | EN10025-6 S890Q | ||
| EN10025-6 S890QL | EN10025-6 S890QL1 | EN10025-6 S960Q | EN10025-6 S960QL | ||
| JIS | JIS G3101 | JIS G3101 SS330 | JIS G3101 SS400 | JIS G3101 SS490 | JIS G3101 SS540 |
| JIS G3106 | JIS G3106 SM400A | JIS G3106 SM400B | JIS G3106 SM400C | JIS G3106 SM490A | |
| JIS G3106 SM490YA | JIS G3106 SM490B | JIS G3106 SM490YB | JIS G3106 SM490C | ||
| JIS G3106 SM520B | JIS G3106 SM520C | JIS G3106 SM570 | |||
| DIN | DIN 17100 | DIN17100 St52-3 | DIN17100 St37-2 | DIN17100 St37-3 | DIN17100 RSt37-2 |
| DIN17100 USt37-2 | |||||
| DIN 17102 | DIN17102 StE315 | DIN17102 ESTE315 | DIN17102 TStE315 | DIN17102 WStE315 | |
| DIN17102 StE355 | DIN17102 ESTE355 | DIN17102 TStE355 | DIN17102 WStE355 | ||
| DIN17102 StE380 | DIN17102 ESTE380 | DIN17102 TStE380 | DIN17102 WStE380 | ||
| DIN17102 StE420 | DIN17102 ESTE420 | DIN17102 TStE420 | DIN17102 WStE420 | ||
| DIN17102 StE460 | DIN17102 ESTE460 | DIN17102 TStE460 | DIN17102 WStE460 | ||
| DIN17102 StE500 | DIN17102 ESTE500 | DIN17102 TStE500 | DIN17102 WStE500 | ||
| DIN17102 ESTE285 | |||||
| GB | GB/T700 | GB/T700 Q235A | GB/T700 Q235B | GB/T700 Q235C | GB/T700 Q235D |
| GB/T700 Q275 | |||||
| GB/T1591 | GB/T1591 Q345A | GB/T1591 Q390A | GB/T1591 Q420A | GB/T1591 Q420E | |
| GB/T1591 Q345B | GB/T1591 Q390B | GB/T1591 Q420B | GB/T1591 Q460C | ||
| GB/T1591 Q345C | GB/T1591 Q390C | GB/T1591 Q420C | GB/T1591 Q460D | ||
| GB/T1591 Q345D | GB/T1591 Q390D | GB/T1591 Q420D | GB/T1591 Q460E | ||
| GB/T1591 Q345E | GB/T1591 Q390E | ||||
| GB/T16270 | GB/T16270 Q550C | GB/T16270 Q550D | GB/T16270 Q550E | GB/T16270 Q550F | |
| GB/T16270 Q620C | GB/T16270 Q620D | GB/T16270 Q620E | GB/T16270 Q620F | ||
| GB/T16270 Q690C | GB/T16270 Q690D | GB/T16270 Q690E | GB/T16270 Q690F | ||
| GB/T16270 Q800C | GB/T16270 Q800D | GB/T16270 Q800E | GB/T16270 Q800F | ||
| GB/T16270 Q890C | GB/T16270 Q890D | GB/T16270 Q890E | GB/T16270 Q890F | ||
| GB/T16270 Q960C | GB/T16270 Q960D | GB/T16270 Q960E | GB/T16270 Q960F | ||
| GB/T16270 Q500 | |||||
Issiq teglar: a36/q235/s235jr karbonli po'lat plitalar, Xitoy a36/q235/s235jr karbonli po'lat plitalar ishlab chiqaruvchilar, etkazib beruvchilar, zavod