API standarti Okean konstruktiv plitasi 2HGr42, 2HGr50, 2WGr50, 2WGr60, 2YGr50, 2YGr60
Mahsulot yelkasi: Kema qurilishi po'lat plitalari / plitalari, kema qurish uchun po'lat plitalar, dengiz po'lat plitalari, Okean konstruktiv po'lat plitalari, Offshore po'lat, offshor muhandislik po'latlari, Okean qurilishi muhandisi uchun po'lat plitalar.
Yetkazib berish sharti: Normallashtirilgan, Q&T, TMCP, Ta'sir testi. Z15, Z25, Z35
Hajmi diapazoni: 3mm -120mm x 1000mm-4000mm x 1000mm-18000mm
Kimyoviy tarkibi va mexanik xususiyatlari
|
Baho |
C % |
Mn % |
P % |
S% |
Si% |
Nb |
Ti |
Al |
N |
V |
|
2HGr42 |
0.18 |
0.90-1.35 |
0.030 |
0.010 |
0.05-0.40 |
0,04 dan kam yoki unga teng |
0,02 dan kam yoki unga teng |
0.02-0.06 |
0.012 |
d |
|
Baho |
Hosildorlik kuchi, kis (Mpa) |
Kuchlanish kuchi, kis |
Cho'zilish |
|
2HGr42 |
t 2,5 dyuym dan kam yoki unga teng 42(289) t 2,5 dyuym 42(289) dan katta yoki unga teng |
62-82(427-565) |
2 dyuym (50 mm) 22 |
Ilova
API Spec Grade 2HGr42 Offshore Platforma po'lat plitalari asosan Offshore Strukturaviy va Okean Dengiz burg'ulash platformasi uchun ishlatiladi.
Boshqa ism
API Spec darajasi 2HGr42 Offshore platformasi Chelik plastinka, API Spec darajasi 2HGr42 Offshore Strukturaviy po'lat plitalar, API Spec darajasi 2HGr42 burg'ulash platformasi Chelik plitalar, API Spec darajasi 2HGr42 payvandlash strukturaviy po'lat plitalar
Qo'shimcha shart
UT (Ultratovush tekshiruvi), AR (Faqat issiq haddelenmiş holda), TMCP (Termal mexanik nazoratni qayta ishlash), N (Normallashtirilgan), Q+T (O'chirilgan va Temperlangan), Z yo'nalishi testi (Z15, Z25, Z35), Charpy V-Notch ta'siri testi, Uchinchi tomon SG testi va sinovlari (shu kabilar),