A302 B darajali past haroratli bosimli idish po'lat plitasimarganets{0}}molibden qotishma po'lat plastinka bo'lib, payvandlash qozonlari va boshqa bosimli idishlar uchun maxsus mo'ljallangan. U neft, kimyo va energiya ishlab chiqarish kabi sohalarda reaktorlar, issiqlik almashtirgichlar va saqlash tanklari kabi uskunalar ishlab chiqarish uchun ishlatiladi. Materialning minimal oqish quvvati 345 MPa va kuchlanish kuchi 550-690 MPa.
A302 B darajali uglerodli po'lat plitalar Kimyoviy tarkibi
| ASTM A302 Kimyoviy tarkibi | |||||||
|---|---|---|---|---|---|---|---|
| Chelik darajasi | Maksimal element (%) | ||||||
| C | Si | Mn | P | S | Mo | Ni | |
| A302 B darajasi | 0.20-0.25 | 0.13-0.45 | 1.07-1.62 | 0.035 | 0.035 | 0.41-0.64 | |
ASTM A302 B darajali qozon po'lat plitasi Mexanik xususiyat
| Chelik darajasi | ASTM A302 Mexanik xususiyat | |||
|---|---|---|---|---|
| Qalinligi | Yo'l bering | Kuchlanish | Cho'zilish | |
| A302 B darajasi | 6-50 | 345 Mpa | 550-690 Mpa | 18% |
| 50-200 | 345 Mpa | 550-690 Mpa | 15% | |
A302 GrB bosimli idish po'lat plitasining qo'llanilishi
LNG saqlash va tashish
A302 GrB qozonlari va bosimli idish po'lat plitasining past haroratlarda chidamliligini saqlab turish qobiliyati uni LNG saqlash tanklari va kriogenli idishlarda foydalanish uchun ideal qiladi. U juda past haroratlarda suyultirilgan gazni saqlaydigan rezervuarlarni qurishda keng qo'llaniladi.
Kimyo va neft-kimyo sanoati
Yuqori mustahkamligi va payvandlanishi tufayli,A302 GrB issiq haddelenmiş po'lat plitalaryuqori bosim va o'rtacha haroratga duchor bo'lgan kimyo va neft-kimyo sanoati uchun bosimli idishlar ishlab chiqarishda tez-tez ishlatiladi. Bu, ayniqsa, reaktorlar, issiqlik almashinuvchilari va distillash ustunlarida foydalidir.
Energiya ishlab chiqarish sanoati
Po‘latning yuqori va past haroratlarda mustahkamligi va ishonchliligi uni elektr stansiyalarida bug‘ generatorlari va yuqori bosimli qozonlar kabi bosimli idishlar ishlab chiqarish uchun mos materialga aylantiradi. Po'latning yuqori bosim sharoitlariga chidamliligi-uzoq muddatli xavfsizlik va ish samaradorligini ta'minlaydi.
Dengiz va dengiz sanoati
A302 GrB issiq haddelenmiş qotishma po'lat plitalarBundan tashqari, u og'ir atrof-muhit sharoitlariga, shu jumladan sho'r suvning korroziyasiga va past haroratlarga duchor bo'lgan neft platformalari va dengiz kemalarini o'z ichiga olgan dengiz dasturlarida ham qo'llaniladi. Bunday sharoitlarda materialning chidamliligi va mustahkamligi uni dengizda qurilish uchun ideal qiladi.
Xavfli materiallarni saqlash uchun tanklar
A302 GrB qozon po'lat plitasiXavfsizlik muhim bo'lgan xavfli materiallarni saqlash tanklarini ishlab chiqarishda qo'llaniladi. Uning past -harorat ishlashi va chidamliligi potentsial uchuvchi kimyoviy moddalar va gazlarni saqlash va tashish uchun qoʻshimcha xavfsizlik qatlamini taʼminlaydi.
Agar siz GNEE mahsulotlari haqida ko'proq bilmoqchi bo'lsangiz, elektron pochta manziliga xat yuborishingiz mumkinalloy@gneesteelgroup.com. Biz sizga yordam berishdan xursandmiz.
| GNEE tomonidan ta'minlangan bosimli idish plitalarining darajalari | |||||
| ASTM | ASTM A202/A202M | ASTM A202 A darajasi | ASTM A202 B darajasi | ||
| ASTM A203/A203M | ASTM A203 A darajasi | ASTM A203 B darajasi | ASTM A203 D darajasi | ASTM A203 E darajasi | |
| ASTM A203 F darajasi | |||||
| ASTM A204/A204M | ASTM A204 A darajasi | ASTM A204 B darajasi | ASTM A204 C darajasi | ||
| ASTM A285/A285M | ASTM A285 A darajasi | ASTM A285 B darajasi | ASTM A285 C darajasi | ||
| ASTM A299/A299M | ASTM A299 A darajasi | ASTM A299 B darajasi | |||
| ASTM A302/A302M | ASTM A302 A darajasi | ASTM A302 B darajasi | ASTM A302 C darajasi | ASTM A302 D darajasi | |
| ASTM A387/A387M | ASTM A387 5-sinf 1-sinf | ASTM A387 5-sinf 2-sinf | ASTM A387 11-sinf 1-sinf | ASTM A387 11-sinf 2-sinf | |
| ASTM A387 12-sinf 1-sinf | ASTM A387 12-sinf 2-sinf | ASTM A387 22-sinf 1-sinf | ASTM A387 22-sinf 2-sinf | ||
| ASTM A515/A515M | ASTM A515 60-sinf | ASTM A515 65-sinf | ASTM A515 70-sinf | ||
| ASTM A516/A516M | ASTM A516 55-sinf | ASTM A516 60-sinf | ASTM A516 65-sinf | ASTM A516 70-sinf | |
| ASTM A517/A517M | ASTM A517 A darajasi | ASTM A517 B darajasi | ASTM A517 E darajasi | ASTM A517 F darajasi | |
| ASTM A517 P darajasi | ASTM A517 J darajasi | ||||
| ASTM A533/A533M | ASTM A533 A sinfi 1 | ASTM A533 B sinfi 1 | ASTM A533 C sinf 1 | ASTM A533 D sinfi 1 | |
| ASTM A533 A sinfi 2 | ASTM A533 B sinfi 2 | ASTM A533 C sinfi 2 | ASTM A533 D sinfi 2 | ||
| ASTM A533 A sinfi 3 | ASTM A533 B sinfi 3 | ASTM A533 C sinfi 3 | ASTM A533 D sinfi 3 | ||
| ASTM A537/A537M | ASTM A537 1-sinf | ASTM A537 2-sinf | ASTM A537 sinf 3 | ||
| ASTM A612/A612M | ASTM A612 | ||||
| ASTM A662/A662M | ASTM A662 A darajasi | ASTM A662 B darajasi | ASTM A662 C darajasi | ||
| UZ | EN10028-2 | EN10028-2 P235GH | EN10028-2 P265GH | EN10028-2 P295GH | EN10028-2 P355GH |
| UZ10028-2 16MO3 | |||||
| EN10028-3 | EN10028-3 P275N | EN10028-3 P275NH | EN10028-3 P275NL1 | EN10028-3 P275NL2 | |
| EN10028-3 P355N | EN10028-3 P355NH | EN10028-3 P355NL1 | EN10028-3 P355NL2 | ||
| EN10028-3 P460N | EN10028-3 P460NH | EN10028-3 P460NL1 | EN10028-3 P460NL2 | ||
| EN10028-5 | EN10028-5 P355M | EN10028-5 P355ML1 | EN10028-5 P355ML2 | EN10028-5 P420M | |
| EN10028-5 P420ML1 | EN10028-5 P420ML2 | EN10028-5 P460M | EN10028-5 P460ML1 | ||
| EN10028-5 P460ML2 | |||||
| EN10028-6 | EN10028-6 P355Q | EN10028-6 P460Q | EN10028-6 P500Q | EN10028-6 P690Q | |
| EN10028-6 P355QH | EN10028-6 P460QH | EN10028-6 P500QH | EN10028-6 P690QH | ||
| EN10028-6 P355QL1 | EN10028-6 P460QL1 | EN10028-6 P500QL1 | EN10028-6 P690QL1 | ||
| EN10028-6 P355QL2 | EN10028-6 P460QL2 | EN10028-6 P500QL2 | EN10028-6 P690QL2 | ||
| JIS | JIS G3115 | JIS G3115 SPV235 | JIS G3115 SPV315 | JIS G3115 SPV355 | JIS G3115 SPV410 |
| JIS G3115 SPV450 | JIS G3115 SPV490 | ||||
| JIS G3103 | JIS G3103 SB410 | JIS G3103 SB450 | JIS G3103 SB480 | JIS G3103 SB450M | |
| JIS G3103 SB480M | |||||
| GB | GB713 | GB713 Q245R | GB713 Q345R | GB713 Q370R | GB713 12Cr1MoVR |
| GB713 12Cr2Mo1R | GB713 13MnNiMoR | GB713 14Cr1MoR | GB713 15CrMoR | ||
| GB713 18MnMoNbR | |||||
| GB3531 | GB3531 09MnNiDR | GB3531 15MnNiDR | GB3531 16MnDR | ||
| DIN | DIN 17155 | DIN 17155 HI | DIN 17155 HII | DIN 17155 10CrMo910 | DIN 17155 13CrMo44 |