American standard A514GrF is a quenched and tempered high-strength weldable steel plate under ASTM standards. It is mainly used in places that require high tensile strength and high yield, such as engineering vehicle lifting gears, large excavators, and racks for offshore platforms. All use A514GrF. The hardness is between 235-290, the yield is >630MPa va kuchlanish kuchi 700MPa dan yuqori.
Yetkazib berish holati: Söndürülmüş va qattiqlashtirilgan holatda etkazib berish (söndürme + temperleme).
Funktsiya va foydalanish: Amerika standarti A514Gr.F - bu ASTM standartlari bo'yicha so'ndirilgan va temperlangan yuqori quvvatli payvandlanadigan po'lat plastinka. ASTM A514 po'lat plitasi yuqori quvvat va yaxshi payvandlash ko'rsatkichlari bilan ajralib turadi. A514Gr.F yuqori quvvatga ega, charchoqqa yaxshi qarshilik ko'rsatadi; yuqori qattiqlik va past mo'rt o'tish harorati; yaxshi sovuq shakllantirish ko'rsatkichlari va payvandlash ko'rsatkichlari; yaxshi korroziyaga chidamlilik va ma'lum aşınma qarshilik. Asosan yuqori kuchlanish va yuqori rentabellikni talab qiladigan joylarda, masalan, burg'ulash dastgohlari, yuk ko'taruvchi mexanizmlar, neft dastgohlari, ko'mir konining gidravlik tayanchlari, elektr belkuraklar, elektr g'ildirakli samosvallar, yuk ko'taruvchilar, buldozerlar va tog'-kon sanoati va turli muhandislik inshootlari uchun turli kranlar uchun ishlatiladi. . , muhandislik vositalari, yirik ekskavatorlar, okean burg'ulash platformalari, tog'-kon uskunalari va boshqalar.