A517 P sinfidagi po'lat plitalar

Nov 28, 2025 Xabar QOLDIRISH

ASTM A517 standart spetsifikatsiyasi bosimli idish plitalari, qotishma po'lat, yuqori-kuchli, söndürülmüş va temperli. Po'lat o'ldirilgan bo'lishi kerak va A20/A20M spetsifikatsiyasining nozik ostenitik don o'lchami talablariga javob berishi kerak.

 

Qalinligi: 6MM dan 300MM gacha,

Kengligi: 1500 mm dan 4050 mm gacha,

Uzunligi: 3000 mm dan 15000 mm gacha

 

A517 sinf P Kimyoviy tarkibi

Baho

Maksimal element (%)

C

Si

Mn

P

S

Ni

A517 sinf P

0.10-0.23

0.18-0.37

0.40-0.78

0.035

0.035

1.15-1.55

Cr

Mo

B

 

 

 

0.79-1.26

0.41-0.64

0.001-0.005

 

 

 

Uglerod ekvivalenti: Ceq=【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%

 

Baho

 

A517 sinf PMexanik xususiyat

Qalinligi

Yo'l bering

Kuchlanish

Cho'zilish

A517 sinf P

mm

Min Mpa

Mpa

Min %

6-65

690

795-930

16%

65-150

620

725-930

14%

 

Ilova

ASTM A517 darajali P (A517GR P) bosimli idish va qozon po'lat plitasi neft, gaz loyihasida bosimli idish, qozon, saqlash tanklari va issiqlik almashinuvchisida qo'llaniladi.

Boshqa ism

ASTM A517 sinf P(A517GR P) qozon po'lat plitasi, ASTM A517 sinf P(A517GR P) bosimli idish po'lat plitasi, ASTM A517 sinf P(A517GR P) saqlash tanklari po'lat plastinka. ASTM A517 sinf P(A517GR P) issiqlik almashinuvchisi po'lat plastinka.

Qo'shimcha shart

UT (Ultratovush tekshiruvi), AR (Faqat issiq haddelenmiş holda), TMCP (Termal mexanik nazoratni qayta ishlash), N (Normallashtirilgan), Q+T (O'chirilgan va Temperlangan), Z yo'nalishi testi (Z15, Z25, Z35), Charpy V-Notch ta'siri testi, Uchinchi tomon SG testi va sinovlari (shu kabilar),