S690QL Ultra yuqori quvvatli po'lat - GNEE po'latiga kirish

Dec 31, 2025 Xabar QOLDIRISH

S690QL po'latyuqori quvvatli, past qotishma konstruktiv po‘lat bo‘lib, u kranlar, ko‘priklar va boshqa tuzilmalar kabi og‘ir{0}}ulovlarda foydalanish uchun mo‘ljallangan. Ushbu po'lat navi, shuningdek, issiqlik bilan ishlov berish jarayoniga ishora qiluvchi "Quenched and Tempered Steel" nomi bilan ham tanilgan.

 

S690QL po'lati yuqori rentabellikga ega po'latdir, minimal oquvchanlik quvvati 690 MPa. U mukammal payvandlanadigan, shakllantiruvchanligi va mustahkamligi bilan ajralib turadi, bu esa uni turli xil ogʻir{3}}ulovlarda foydalanishga yaroqli qiladi. Ushbu po'lat navi, shuningdek, charchoq va aşınmaya yuqori qarshilik bilan mashhur.

 

S690QL toifasi quyidagicha:
S=Strukturaviy po'lat
690=minimal oqish quvvati (MPa)
Q=Söndürme va temperleme
L=Past tishli qattiqlik sinov harorati

 

S690QL ning afzalliklari

Yuqori kuch: S690QL po'latining yuqori oquvchanlik quvvati 690 MPa, bu uni yuqori quvvat va chidamlilikni talab qiluvchi og'ir{2}}majburiy ilovalarda foydalanishga moslashtiradi.

Yaxshi payvandlash qobiliyati: S690QL po'lati mukammal payvandlash qobiliyatiga ega, bu esa uni tayyorlash va yig'ishni osonlashtiradi.

Qattiqlik:S690QL po'lati yaxshi pishiqlikka ega bo'lib, u zarba va charchoqqa chidamliligini ta'minlaydi, bu esa uni og'ir{1}}burchaklarda foydalanish uchun mos qiladi.

Korroziyaga qarshilik:S690QL po'lati yaxshi korroziyaga chidamliligiga ega, bu uni dengiz tuzilmalarida va og'ir muhitga ta'sir qilish kutilayotgan boshqa ilovalarda foydalanishga yaroqli qiladi.

S690QL

S690QL barcha o'chirilgan va temperli gradusli materiallardan eng mashhur GNEE po'latdir. Masteel zaxirasi va qalinligi 250 mm gacha bo'lgan S690QL materialini etkazib beradi.

 

S690QL yuqori quvvatli po'lat plitalar kimyoviy tarkibi

 

Element Foiz % Element Foiz %
C 0.20 Cu 0.50
Si 0.80 Mo 0.70
Mn 1.70 Nb* 0.06
P 0.025 Ni 2.0
S 0.015 Ti* 0.05
N 0.015 V* 0.12
B 0.0050 Zr* 0.15
Cr 1.50    

 

S690QL yuqori quvvatli past qotishma HSLA po'latining mexanik xususiyatlari

 

Belgilash Mexanik xususiyatlar (atrof-muhit harorati)
Chelik nomi Chelik raqami Min. Hosildorlik kuchi Reh MPa Kuchlanish kuchi Rm MPa Min. Singandan keyin % cho'zilish
Nominal qalinligi (mm) Nominal qalinligi (mm)
3 dan katta yoki teng 50 dan kichik yoki teng 50 dan katta yoki teng 100 dan kichik yoki teng 100 dan katta yoki teng 150 dan kichik yoki teng 3 dan katta yoki teng 50 dan kichik yoki teng 50 dan katta yoki teng 100 dan kichik yoki teng 100 dan katta yoki teng 150 dan kichik yoki teng
S690QL 1.8931 690 650 630 770/940 760/930 710/900 14

 

S690QL - V Notch zarbasi sinovi

 

V Notch zarba sinovi tafsilotlari quyidagi jadvalda keltirilgan.

Baho Namuna yo'nalishi @ 0 daraja @-20 daraja @-40 daraja @-60 daraja
S690QL Uzunlamasına 50 J 40 J 30 J ¨C¨C
O'tish 35 J 30 J 27 J ¨C¨C

 

Xulosa

 

S690QL yuqori rentabellikga chidamliligi EN 10025-6 po'lat plastinkazamonaviy konstruktiv muhandislik uchun ko'p qirrali va ishonchli materialdir. O'zining mukammal quvvati, chidamliligi va payvandlanishi bilan ishlash va narx o'rtasidagi optimal muvozanatni ta'minlaydi.

 

Agar siz manba bo'lsangizS690QL po'lat plitalar, aloqaGNEE po'latbugungi kunda mutaxassislar maslahati, tezkor kotirovkalar va ishonchli global yetkazib berish uchun.

GNEE Steel - Siz ishonishingiz mumkin bo'lgan kuch.

Narx so'rash

 

S690QL nima?

S690QL po'latdirkranlar, ko‘priklar va boshqa tuzilmalar kabi og‘ir{0}}uylarda foydalanish uchun mo‘ljallangan yuqori quvvatli, past qotishma konstruktiv po‘lat. Ushbu po'lat navi, shuningdek, issiqlik bilan ishlov berish jarayoniga ishora qiluvchi "Quenched and Tempered Steel" nomi bilan ham tanilgan.

 

S690 toifali po'lat nima?

S690 yuqori mahsuldor va nozik taneli po'lat plita - bu yuqori quvvatli, so'ndirilgan va temperlangan nozik-konstruktiv po'latdir. Strukturaviy po'lat S690 juda og'ir yuklarga bardosh berishi kerak bo'lgan tuzilmalarda qo'llaniladi. Bu daraja vaznni tejash muhim bo'lgan tuzilmalar uchun mo'ljallangan.

 

S690Q va S690QL o'rtasidagi farq nima?

S690Q: Minimal zarba chidamliligi -20 darajada sinovdan o'tkazildi (o'rtacha 30J). → Odatda foydalanish: Mo''tadil iqlim sharoitidagi kranlar, karer uskunalari. S690QL: -40 daraja va undan past daraja uchun sertifikatlangan (zarba chidamliligi 40J dan katta yoki unga teng).

 

S690QL nima uchun ishlatiladi?

S690QL belgisi 690 MPa minimal oqish quvvatiga ishora qiladi. Yaxshi mavjudlik, narx va yuqori mustahkamlik va ishlab chiqarish qulayligi kombinatsiyasi S690QL po'lat plitasini kranlar va yuk ko'tarish uskunalari va sobit po'lat konstruktsiyalar kabi mobil ilovalar uchun mashhur navga aylantirdi.

 

S690QL ning qattiqligi qanday?

Brinell qattiqligining qiymati 414HBW bo'lgan holda, yuqori{1}}kuchli S690ql po'lat navi yaratiladi.

 

Mahsulotlarni ko'rsatish

7

info-498-161

 

Qadoqlash va jo'natish

 

1

5

 

Ko'rgazmalar va mijozlar tashriflari

 

GNEE Global Exhibition Record

 

 

 
 

 

GNEE Steel shuningdek, A514 Grade F, A572 Grade 50, A588 Grade A, S355JR, S690Q, SS400, S690QL, Q345B, Q345E va boshqalar kabi yuqori{1}}bardoshli po'lat plitalarni ham yetkazib beradi. +8615824687445 yoki alloy@gneesteelgroup.com manziliga xat yuboring. Biz bilan maslahatlashishga xush kelibsiz va biz sizning savollaringizga javob berishga tayyormiz.

 

 

 

GNEE tomonidan ta'minlangan uglerod va past{0}}qotishma yuqori-po'latlar navlari
ASTM/ASME ASTM A36/A36M ASTM A36      
ASTM A283/A283M ASTM A283 A darajasi ASTM A283 B darajasi ASTM A283 C darajasi ASTM A283 D darajasi
ASTM A514/A514M ASTM A514 A darajasi ASTM A514 B darajasi ASTM A514 C darajasi ASTM A514 E darajasi
ASTM A514 F darajasi ASTM A514 H darajasi ASTM A514 J darajasi ASTM A514 K darajasi
ASTM A514 M darajasi ASTM A514 P darajasi ASTM A514 Q darajasi ASTM A514 R darajasi
ASTM A514 S darajasi ASTM A514 T darajasi    
ASTM A572/A572M ASTM A572 42-sinf ASTM A572 50-darajali ASTM A572 55-sinf ASTM A572 60-sinf
ASTM A572 65-sinf      
ASTM A573/A573M ASTM A573 58-sinf ASTM A573 65-sinf ASTM A573 70-sinf  
ASTM A588/A588M ASTM A588 A darajasi ASTM A588 B darajasi ASTM A588 C darajasi ASTM A588 K darajasi
ASTM A633/A633M ASTM A633 A darajasi ASTM A633 C darajasi ASTM A633 D darajasi ASTM A633 E darajasi
ASTM A656/A656M ASTM A656 50-darajali ASTM A656 60-sinf ASTM A656 70-sinf ASTM A656 80-sinf
ASTM A709/A709M ASTM A709 36-sinf ASTM A709 50-darajali ASTM A709 50S darajasi ASTM A709 darajasi 50 Vt
ASTM A709 darajasi HPS 50W ASTM A709 darajasi HPS 70W ASTM A709 100-darajali ASTM A709 darajasi 100 Vt
ASTM A709 darajasi HPS 100W      
ASME SA36/SA36M ASME SA36      
ASME SA283/SA283M ASME SA283 A darajasi ASME SA283 B darajasi ASME SA283 C darajasi ASME SA283 D darajasi
ASME SA514/SA514M ASME SA514 A darajasi ASME SA514 B darajasi ASME SA514 C darajasi ASME SA514 E darajasi
ASME SA514 F darajasi ASME SA514 H darajasi ASME SA514 J darajasi ASME SA514 K darajasi
ASME SA514 M darajasi ASME SA514 P darajasi ASME SA514 Q darajasi ASME SA514 R darajasi
ASME SA514 S darajasi ASME SA514 T darajasi    
ASME SA572/SA572M ASME SA572 42-sinf ASME SA572 50-sinf ASME SA572 55-sinf ASME SA572 60-sinf
ASME SA572 65-sinf      
ASME SA573/SA573M ASME SA573 58-sinf ASME SA573 65-sinf ASME SA573 70-sinf  
ASME SA588/SA588M ASME SA588 A darajasi ASME SA588 B darajasi ASME SA588 C darajasi ASME SA588 K darajasi
ASME SA633/SA633M ASME SA633 A darajasi ASME SA633 C darajasi ASME SA633 D darajasi ASME SA633 E darajasi
ASME SA656/SA656M ASME SA656 50-sinf ASME SA656 60-sinf ASME SA656 70-sinf ASME SA656 80-sinf
ASME SA709/SA709M ASME SA709 36-sinf ASME SA709 50-sinf ASME SA709 50S darajasi ASME SA709 darajasi 50W
ASME SA709 darajasi HPS 50W ASME SA709 darajasi HPS 70W ASME SA709 100-sinf ASME SA709 darajasi 100 Vt
ASME SA709 darajasi HPS 100W      
EN10025 EN10025-2 EN10025-2 S235J0 EN10025-2 S275J0 EN10025-2 S355J0 EN10025-2 S355K2
EN10025-2 S235JR EN10025-2 S275JR EN10025-2 S355JR EN10025-2 S420J0
EN10025-2 S235J2 EN10025-2 S275J2 EN10025-2 S355J2  
EN10025-3 EN10025-3 S275N EN10025-3 S355N EN10025-3 S420N EN10025-3 S460N
EN10025-3 S275NL EN10025-3 S355NL EN10025-3 S420NL EN10025-3 S460NL
EN10025-4 EN10025-4 S275M EN10025-4 S355M EN10025-4 S420M EN10025-4 S460M
EN10025-4 S275ML EN10025-4 S355ML EN10025-4 S420ML EN10025-4 S460ML
EN10025-6 EN10025-6 S460Q EN10025-6 S460QL EN10025-6 S460QL1 EN10025-6 S500Q
EN10025-6 S500QL EN10025-6 S500QL1 EN10025-6 S550Q EN10025-6 S550QL
EN10025-6 S550QL1 EN10025-6 S620Q EN10025-6 S620QL EN10025-6 S620QL1
EN10025-6 S690Q EN10025-6 S690QL EN10025-6 S690Q1 EN10025-6 S890Q
EN10025-6 S890QL EN10025-6 S890QL1 EN10025-6 S960Q EN10025-6 S960QL
EN 10149 EN 10149-2 S315MC S355MC S420MC S460MC
S500MC S550MC S600MC S650MC
S700MC S900MC S960MC  
JIS JIS G3101 JIS G3101 SS330 JIS G3101 SS400 JIS G3101 SS490 JIS G3101 SS540
JIS G3106 JIS G3106 SM400A JIS G3106 SM400B JIS G3106 SM400C JIS G3106 SM490A
JIS G3106 SM490YA JIS G3106 SM490B JIS G3106 SM490YB JIS G3106 SM490C
JIS G3106 SM520B JIS G3106 SM520C JIS G3106 SM570  
DIN DIN 17100 DIN17100 St52-3 DIN17100 St37-2 DIN17100 St37-3 DIN17100 RSt37-2
DIN17100 USt37-2      
DIN 17102 DIN17102 StE315 DIN17102 ESTE315 DIN17102 TStE315 DIN17102 WStE315
DIN17102 StE355 DIN17102 ESTE355 DIN17102 TStE355 DIN17102 WStE355
DIN17102 StE380 DIN17102 ESTE380 DIN17102 TStE380 DIN17102 WStE380
DIN17102 StE420 DIN17102 ESTE420 DIN17102 TStE420 DIN17102 WStE420
DIN17102 StE460 DIN17102 ESTE460 DIN17102 TStE460 DIN17102 WStE460
DIN17102 StE500 DIN17102 ESTE500 DIN17102 TStE500 DIN17102 WStE500
DIN17102 ESTE285      
GB GB/T700 GB/T700 Q235A GB/T700 Q235B GB/T700 Q235C GB/T700 Q235D
GB/T700 Q275      
GB/T1591 GB/T1591 Q345A GB/T1591 Q390A GB/T1591 Q420A GB/T1591 Q420E
GB/T1591 Q345B GB/T1591 Q390B GB/T1591 Q420B GB/T1591 Q460C
GB/T1591 Q345C GB/T1591 Q390C GB/T1591 Q420C GB/T1591 Q460D
GB/T1591 Q345D GB/T1591 Q390D GB/T1591 Q420D GB/T1591 Q460E
GB/T1591 Q345E GB/T1591 Q390E    
GB/T16270 GB/T16270 Q550C GB/T16270 Q550D GB/T16270 Q550E GB/T16270 Q550F
GB/T16270 Q620C GB/T16270 Q620D GB/T16270 Q620E GB/T16270 Q620F
GB/T16270 Q690C GB/T16270 Q690D GB/T16270 Q690E GB/T16270 Q690F
GB/T16270 Q800C GB/T16270 Q800D GB/T16270 Q800E GB/T16270 Q800F
GB/T16270 Q890C GB/T16270 Q890D GB/T16270 Q890E GB/T16270 Q890F
GB/T16270 Q960C GB/T16270 Q960D GB/T16270 Q960E GB/T16270 Q960F
GB/T16270 Q500