Astm A203 dona fanikel - qotishma plastinkamo''tadil yoki past haroratlarda ishlaydigan payvandlangan bosimli tomirlar uchun mo'ljallangan. Uning nikel tarkibiga 2,25% dan 2,75% gacha, yuqori quvvat va yaxshi - yuqori kuch va yaxshi {{}} - - - - - - - "LNG saqlash idishlari va kriogen zavodlari kabi dasturlarga mos keladi.
ASTM AK qozon go'shti floti kimyoviy tarkibi va mexanik mulk
|
Baho |
Kimyoviy tarkibi (%) |
||||
|
C |
Mn katta yoki teng |
Si |
P |
S |
|
|
A203 dona (A203GRF) |
0.20 |
0.7-0.8 |
0.13-0.45 |
0.035 |
0.035 |
|
Baho |
Mexanik mulk |
|
|||
|
Zinarli kuch (MPA) |
Kuch berish kuchi (MPA) |
% Lanaj 2 ichida (50mm) min |
Sinov haroratiga ta'sir ko'rsatish (daraja) |
|
|
|
A203 dona (A203GRF) |
485 |
380 |
20 |
-20,40,-60 |
|
ASTM AK (A203GRF) bosimli bosim va qozon po'lat plitasi
Kimyoviy reaktsiya tomirlari
A203 navli Fuln va bosimli plastinka sintez reaktsiyalarida ishlatiladi (o'g'itli o'simliklar va polimerizatsion reakorlarda ammiak sintezi va polimerizatsion reakorlarda). Bu yuqori harorat va bosimlarga bardosh berishi kerak (masalan, ammiak sintezi minorasi 30 daraja va 450 daraja bosimda ishlaydi) va o'rtacha (vodorod va kislota gazlari) reaktsiya jarayonida oqib chiqmaydi.
Nopok suvli saqlash idishlari va minoralari
A203 dona navli dog 'bosimi po'lat plitasi xom neft, suyultirilgan tabiiy gaz (LPG), shuningdek, tuzatish oqimlari va neftni saqlash uchun idishlar (masalan, xom neft tanklari) uchun saqlanadi; Kam - Harorat saqlash uchun idishlar (masalan,-} -}}} -}}} -}}} -- past haroratlarda po'lat plitalarni talab qiladi; yuqori bosimli vidrogenlash minoralari (neft-kimyo gidroefininlash jarayoni).
Issiqlik almashinuvi tomirlari
A203 navli f huquqi yuqori - O'rta issiqlik almashinuvi (- - {{}} {{}} {{}} {{}} {{}} {{}} {{}} {{}} {{}} {{{}} {- {{}} {{{}} {{- naychalari uchun ishlatiladi. Ularning qobig'i va naychalari issiq va sovuq zarbalar bilan aloqa qilish, charchoqning tez-tez o'zgarishi natijasida charchoqni buzishdan saqlaning va payvandlashning tez-tez o'zgarishi oldini oladi.
Metallurgiya sanoati
"Plaste pechida issiq portlash pechkasi" (0}}} haroratli havoni va 1200 daraja bosimli va 1200 daraja saqlaydi). "Avtoklav" rangli metall eritmadagi (masalan, gidrometallurgiya mis ermentida eritmali avtoklav) kislota korroziyaga chidamli bo'lishi kerak va A203 navli bosimi po'lat plita ishlatiladi.
ASTM AK (A203GRF) bosimli bosimli idish va qozon po'lat plitasi Boshqa nom
ASTM AK (A203GRF) qozon po'lat plitasi, Asti ASTM ASTM ASTM ASTM ASTM ASTM ASTM ASTM ASTM ASTM ASTM ASTM ASTM ASTM ASTM ASTM ASTM ASTM ASTM ASTM ASTM ASTM ASTM ASTM ASTM ASTM PRELL plastinkalari. ASTM AK (A203GRF) issiqlik almashtirgich po'lat plitasi.
Qo'shimcha shart
UT (ultratovik tekshiruv), Ar (faqat issiqlik), n (normallangan), q + t (z35, z35, z35), uchinchi tomon sinovi (SGS testi), qoplangan yoki bo'yash kabi rasm.
Agar siz GNEE mahsulotlari haqida ko'proq ma'lumot olishni istasangiz, elektron pochta xabarini yuborishingiz mumkinalloy@gneesteelgroup.com.Biz sizga yordam berishdan ko'proq xursandmiz.
| Qozon va bosimli po'lat plastinka | |||||
| Askm | ASTM a202 / A202M | ASTM a202 sinf a | ASTM a202 dori b | ||
| ASTM a203 / A203M | ASTM AE203 sinfi a | Asti a203 sinf b | Asti a203 dyuym d d | ASTM A203 sinf | |
| Astm A203 dona f | |||||
| ASTM a204 / A204M | ASTM AE204 SAZI A | ASTM a204 sinf b | ASTM AK | ||
| ASTM A285 / A285M | ASTM A285 SLE A | ASTM A285 sinfi b | ASTM A285 sinf c | ||
| ASTM A299 / A299M | ASTM A299 sinfi a | ASTM A299 sinfi b | |||
| ASTM A302 / A302M | Ashm A302 | ASTM A302 sinf b | ASTM A302 sinf c | ASTM A302 dyali D | |
| ASTM A387 / A387M | ASTM A387-sinflar11 | ASTM A387-sinflar22 | ASTM A387 11-sinf11 | ASTM A387 SLOY2 | |
| ASTM A387-sinf 12 sinf11 | ASTM A387-sinf 12 sinf2 | ASTM A387-sinflar11 | ASTM A387-sinf 22-sinf2 | ||
| ASTM A515 / A515M | ASTM A515 60 | ASTM A515-sinf 65 | ASTM A515 70 | ||
| ASTM A516 / A516M | ASTM A516-sinf 55 | ASTM A516 60 | ASTM A516-sinf 65 | ASTM A516 70 | |
| ASTM A517 / A517M | ASTM A517 SAYTI A | ASTM A517 sinf b | ASTM A517 sinf E | ASTM A517 SAF F | |
| Asti a517 sinf | ASTM A517 SLEH J | ||||
| ASTM A533 / A533M | ASTM A533 sinfi1 | ASTM A533 sinf B sinf11 | ASTM A533 sinf c clact1 | ASTM A533 sinf d clas11 | |
| ASTM A533 sinfi2 | ASTM A533 sinf B sinf2 | ASTM A533 sinf c clac2 | ASTM A533 sinf d clas22 | ||
| ASTM A533 sinfi | ASTM A533 sinf b sinflari3 | ASTM A533 sinf c clact3 | ASTM A533 sinf d clas3 | ||
| ASTM A537 / A537M | ASTM A537 sinf11 | ASTM A537 Clas22 | ASTM A537 Classi3 | ||
| ASTM A612 / A612M | ASTM A612 | ||||
| ASTM A662 / A662M | ASTM A662 sinf a | ASTM A662 sinf b | ASTM A662 sinf c | ||
| Ro'mol | En10028--- | En10028-2 p235g | En10028-2 p265g | En10028-2 p295g | En10028-2 p355gh |
| En 10028-2 16 Mo3 | |||||
| En10028-3 | En10028-3 p275n | En10028-3 p275nh | En10028-3 p275n1 | En10028-3 p275n22 | |
| En10028-3 p355n | En10028-3 p355nh | En10028-3 p355n1 | En10028-3 p355n22 | ||
| En10028-3 p460n | En10028-3 p460nh | En10028-3 p460nl1 | En10028-3 p460n22 | ||
| En10028-5 | En10028-5 p355m | En10028-5 p355l1 | En10028-5 p355l2 | En10028-5 p420M | |
| En10028-5 p420l1 | En10028-5 p420l22 | En10028-5 p460m | En10028-5 p460l1 | ||
| En10028-5 p460l2 | |||||
| En10028-6 | En10028-6 p355q | En10028-6 p460q | En10028-6 p500q | En10028-6 p690q | |
| En10028-6 p355qh | En10028-6 p460Qh | En10028-6 p500qh | En10028-6 p690Qh | ||
| En10028-6 p355ql1 | En10028-6 p460ql1 | En10028-6 p500ql1 | En10028-6 p690ql1 | ||
| En10028-6 p355ql22 | En10028-6 p460ql22 | En10028-6 p500ql22 | En10028-6 p690ql22 | ||
| Jis | Jis g3115 | Jis g3115 SPV235 | Jis g3115 SPV315 | Jis g3115 SPV355 | Jis g3115 SPV410 |
| Jis g3115 SPV450 | Jis g3115 SPV490 | ||||
| Jis g3103 | Jis g3103 sb410 | Jis g3103 sb450 | Jis g3103 sb480 | Jis g3103 sb450m | |
| Jis g3103 sb480m | |||||
| Gb | Gb713 | Gb713 Q245R | Gb713 Q345R | Gb713 Q370R | GB 713 12 CR1MOVR |
| GB 713 12 CR2MO1R | GB 713 13 mnnimor | GB 713 14 cr1or | GB 713 15 crmor | ||
| GB 713 18 mnmonbr | |||||
| Gb3531 | GB 3531 09 mnniidr | GB 3531 15 mnniidr | GB 3531 16 mndrd | ||
| Did | Din 17155 | Din 17155 salom | Din 17155 hii | Din 17155 10 CRMO910 | Din 17155 13 CRMO44 |
| Din 17155 15 MO3 | DIN 17155 17 mn4 | DIN 17155 19 mn6 | |||