ASTM A537 1-sinfIssiqlik {{0} {{1 {1} {{2} {{3} - Silogenes {{2} - payvandlangan bosimli bosim va inshootlar uchun silika plastinka uchun ishlatiladi. Bu uning neft, gaz va neft-kimyo sanoatida bosimli xizmatlarga mos keltirish va ko'pincha qozonxonalarda qo'llaniladi va ko'pincha qozonlarda ishlatiladi.
ASTM A537 Class 1 Uglerod po'lat plitasi
Material - issiqlik bilan davolangan oqim va natijada yuqorida va keskinlik kuchini ASTM A516 baholaridan ko'ra ko'proq hosil va keskinlik kuchini ko'rsatadi. Po'lat bolani va bosimli kemalarda, ham qozonlarda, ikkalangizda ham, dunyodagi etakchi ruhoniylarga, shuningdek, dunyodagi etakchi ruhoniylarga etkazib berish uchun juda mos keladi.
Qo'shimcha ma'lumot olish uchun quyidagi texnik xususiyatlarga qarang.
ASTM A537 CLASS 1 Carbon po'lat plitasi
ASTM A537 Class 1 Carbon temir po'lat plitasi quyidagi jadvalda umumlashtirilgan.
| Baho | C | Si | Mn | P | S | Kri | Mor | Ni | Ku | |
|---|---|---|---|---|---|---|---|---|---|---|
| 40 mm dan kam yoki unga teng | >40 mm | |||||||||
| A537 1-sinf | 0.24 | 0.15/0.50 | 0.70/1.35 | 1.00/1.60 | 0.035 | 0.035 | 0.025 | 0.080 | 0.25 | 0.35 |
ASTM A537 Class 1 Uglerod po'lat plitasining mexanik xususiyatlari
ASTM A537-sinflar 1 uglerod po'lat plitasining mexanik xususiyatlari quyidagi jadvalda umumlashtiriladi.
| Baho | Hosildorlik (MPA) | Zinarli (MPA) | Cho'zish | Qalinlik | |
|---|---|---|---|---|---|
| A05mm | A200mm | ||||
| A537 1-sinf | 345 | 485/620 | 22% | 18% | 65 dan kam yoki teng |
| 310 | 450/585 | 22% | 18% | >65 dan kam yoki 100 ga teng | |
Issiqlikni davolash
ASTM A537 sinf 1 plitalar kerakli mexanik xususiyatlarga erishish uchun davolangan holat (qonli va uni sindirilgan) bilan ta'minlaydi.
Ekvivalent navlar
En 10028-3: P275H
Jis G3115: SPV355
GB 713: Q345R
ASTM A537 Class 1 bosimli idish va qozon po'lat plitasi Boshqa ismi
ASTM A537 CLASS 1 (A537CLCL1) qozon po'lat plitasi, ASTM A537 1 (A537CLCL1) 1 (A537CLCL1) 1 (A537CLC1) Saqlash idishlari po'lat plastinkasi. ASTM A537 sinf 1 (A537CLCL1) issiqlik almashtirgich po'lat plitasi.
Qo'shimcha shart
UT (ultratovik tekshiruv), Ar (faqat issiqlik), n (normallangan), q + t (z35, z35, z35), uchinchi tomon sinovi (SGS testi), qoplangan yoki bo'yash kabi rasm.
Agar siz GNEE mahsulotlari haqida ko'proq ma'lumot olishni istasangiz, elektron pochta xabarini yuborishingiz mumkinalloy@gneesteelgroup.com. Biz sizga yordam berishdan ko'proq xursandmiz.
ARTM A537 sinf 1 ta material nima?
ASTM A537 1-sinfUglerod po'lat va uglerodli po'lat plitalar va uglerod po'lat plitalariMahsulotni bosim o'tkazishda qo'llaniladigan muhandislar. Material - bu normallangan po'lat va issiqlik bilan davolash qilingan qotishma va natijada yordam va keskinlik kuchini ASTM A516 sinflaridan ko'proq hosil va keskinlik kuchini ko'rsatadi.
ASTM A537 sinfi va 2-sinf o'rtasidagi farq nima?
ASTM A537 / ASME SA537 plastinka materiallari - muomalada, uglerod {{3} {{3} {- Manbone kremniy po'lat.A537 sinf 1 plastinkasi normallashtirilgan va 2 ta plastinka qon quyiladi va tebranadi. A537 uglerod po'lat plitasi A516 ga qaraganda ko'proq keskinlik kuchini taklif etadi. A537 plitasi odatda neft va gaz va neft-kimyo sanoatida qo'llaniladi.
A537-sinf 1-sinfining kuchliligi nima?
345 MPa
ASTM A537 1-sinf - bu past - uglerod, yuqori - uchun ishlatiladigan qotishma plitasi. Ushbu material yuqori - yuqori muhit uchun juda kuch va kuchni taklif qiladi. U kuchuk kuchga ega345 MPaVa yuqori - balandlikdagi asbob-uskunalarda foydalanish uchun ideal qiladigan 485 mpa 485 MPAning keskinlik kuchi.
537 Cl 1 ga teng?
ASTM A537 sinf 1 Uglerod po'lat plitalarining ekvivalent navlariDIN 19 million va SPV36 standartlari.



| Gnee tomonidan ta'minlangan bosimli bosimli plitalar | |||||
| Askm | ASTM a202 / A202M | ASTM a202 sinf a | ASTM a202 dori b | ||
| ASTM a203 / A203M | ASTM AE203 sinfi a | Asti a203 sinf b | Asti a203 dyuym d d | ASTM A203 sinf | |
| Astm A203 dona f | |||||
| ASTM a204 / A204M | ASTM AE204 SAZI A | ASTM a204 sinf b | ASTM AK | ||
| ASTM A285 / A285M | ASTM A285 SLE A | ASTM A285 sinfi b | ASTM A285 sinf c | ||
| ASTM A299 / A299M | ASTM A299 sinfi a | ASTM A299 sinfi b | |||
| ASTM A302 / A302M | Ashm A302 | ASTM A302 sinf b | ASTM A302 sinf c | ASTM A302 dyali D | |
| ASTM A387 / A387M | ASTM A387-sinflar11 | ASTM A387-sinflar22 | ASTM A387 11-sinf11 | ASTM A387 SLOY2 | |
| ASTM A387-sinf 12 sinf11 | ASTM A387-sinf 12 sinf2 | ASTM A387-sinflar11 | ASTM A387-sinf 22-sinf2 | ||
| ASTM A515 / A515M | ASTM A515 60 | ASTM A515-sinf 65 | ASTM A515 70 | ||
| ASTM A516 / A516M | ASTM A516-sinf 55 | ASTM A516 60 | ASTM A516-sinf 65 | ASTM A516 70 | |
| ASTM A517 / A517M | ASTM A517 SAYTI A | ASTM A517 sinf b | ASTM A517 sinf E | ASTM A517 SAF F | |
| Asti a517 sinf | ASTM A517 SLEH J | ||||
| ASTM A533 / A533M | ASTM A533 sinfi1 | ASTM A533 sinf B sinf11 | ASTM A533 sinf c clact1 | ASTM A533 sinf d clas11 | |
| ASTM A533 sinfi2 | ASTM A533 sinf B sinf2 | ASTM A533 sinf c clac2 | ASTM A533 sinf d clas22 | ||
| ASTM A533 sinfi | ASTM A533 sinf b sinflari3 | ASTM A533 sinf c clact3 | ASTM A533 sinf d clas3 | ||
| ASTM A537 / A537M | ASTM A537 sinf11 | ASTM A537 Clas22 | ASTM A537 Classi3 | ||
| ASTM A612 / A612M | ASTM A612 | ||||
| ASTM A662 / A662M | ASTM A662 sinf a | ASTM A662 sinf b | ASTM A662 sinf c | ||
| Ro'mol | En10028--- | En10028-2 p235g | En10028-2 p265g | En10028-2 p295g | En10028-2 p355gh |
| En 10028-2 16 Mo3 | |||||
| En10028-3 | En10028-3 p275n | En10028-3 p275nh | En10028-3 p275n1 | En10028-3 p275n22 | |
| En10028-3 p355n | En10028-3 p355nh | En10028-3 p355n1 | En10028-3 p355n22 | ||
| En10028-3 p460n | En10028-3 p460nh | En10028-3 p460nl1 | En10028-3 p460n22 | ||
| En10028-5 | En10028-5 p355m | En10028-5 p355l1 | En10028-5 p355l2 | En10028-5 p420M | |
| En10028-5 p420l1 | En10028-5 p420l22 | En10028-5 p460m | En10028-5 p460l1 | ||
| En10028-5 p460l2 | |||||
| En10028-6 | En10028-6 p355q | En10028-6 p460q | En10028-6 p500q | En10028-6 p690q | |
| En10028-6 p355qh | En10028-6 p460Qh | En10028-6 p500qh | En10028-6 p690Qh | ||
| En10028-6 p355ql1 | En10028-6 p460ql1 | En10028-6 p500ql1 | En10028-6 p690ql1 | ||
| En10028-6 p355ql22 | En10028-6 p460ql22 | En10028-6 p500ql22 | En10028-6 p690ql22 | ||
| Jis | Jis g3115 | Jis g3115 SPV235 | Jis g3115 SPV315 | Jis g3115 SPV355 | Jis g3115 SPV410 |
| Jis g3115 SPV450 | Jis g3115 SPV490 | ||||
| Jis g3103 | Jis g3103 sb410 | Jis g3103 sb450 | Jis g3103 sb480 | Jis g3103 sb450m | |
| Jis g3103 sb480m | |||||
| Gb | Gb713 | Gb713 Q245R | Gb713 Q345R | Gb713 Q370R | GB 713 12 CR1MOVR |
| GB 713 12 CR2MO1R | GB 713 13 mnnimor | GB 713 14 cr1or | GB 713 15 crmor | ||
| GB 713 18 mnmonbr | |||||
| Gb3531 | GB 3531 09 mnniidr | GB 3531 15 mnniidr | GB 3531 16 mndrd | ||
| Did | Din 17155 | Din 17155 salom | Din 17155 hii | Din 17155 10 CRMO910 | Din 17155 13 CRMO44 |
| Din 17155 15 MO3 | DIN 17155 17 mn4 | DIN 17155 19 mn6 | |||