CCS DH36 yuqori - yuqori - yuqori {{}} yuqori {{}} yuqori {{}} yuqori {{}} yuqori {{}} yuqori - Quvvatli plastinka navi, juda yaxshi plastinka navi, a'lo platforma va kemalarning korpuslari, shu jumladan katta tashuvchilar singari tasniflash. U minimal kuchlanish kuchi 355 MPa va 490-620 MPAning keskinlik oralig'i.
CCS / DH36 Tempering va qon ketishida yuqori quvvatli kimyoviy tarkib
|
Element |
CCS DH36 Max% |
Element |
CCS DH36 Max% |
|
C |
0.18 |
Ni |
0.40 |
|
Mn |
0.90-1.60 |
Mor |
0.08 |
|
Si |
0.50 |
Aldamoq |
0.015 min |
|
S |
0.035 |
Nb |
0.20-0.05 |
|
P |
0.035 |
V |
0.05-0.10 |
|
Ku |
0.35 |
Ti |
0.02 |
|
Kri |
0.20 |
N |
|
CCS / DH36 Tempering va qon ketishidagi yuqori kuch
|
Baho |
Qalinlik |
Kuch berish kuchi |
Mustahkamlik chegarasi |
Cho'zish |
Ta'sir energiyasi |
|
(mm) |
MPa (min) |
Mpa |
% (min) |
(K kv) (min) |
|
|
|
|
|
|
-20 daraja |
|
|
CCS DH36 |
8-240 |
355 |
490-620 |
21 |
34J |
|
CCS / DH36 ga tengli po'lat navi |
|||||||
|
Dnv |
Yalqov |
Xiyonat |
Bv |
Abs |
Nk |
Kr |
Rina |
|
Nv d36 |
Gl - d36 |
LR / DH36 |
BV / DH36 |
ABS / D36 |
K D36 |
R D36 |
RI / D36 |
|
CCS po'lat plitasi navi |
||||
|
Umumiy kuch |
CCS / a |
Ccs / b |
Ccs / d |
Ccs / e |
|
Yuqori kuch |
CCS / A32 |
CCS / D32 |
CCS / E32 |
CCS / F32 |
|
CCS / A36 |
CCS / D36 |
CCS / E36 |
CCS / F36 |
|
|
CCS / A40 |
CCS / D40 |
CCS / E40 |
CCS / F40 |
|
|
Qo'shimcha kuch |
CCS / A420 |
CCS / D420 |
CCS / E420 |
CCS / F420 |
|
CCS / A460 |
CCS / D460 |
CCS / E460 |
CCS / F460 |
|
|
CCS / A500 |
CCS / D500 |
CCS / E500 |
CCS / F500 |
|
|
CCS / A550 |
CCS / D550 |
CCS / E550 |
CCS / F550 |
|
|
CCS / A620 |
CCS / D620 |
CCS / E620 |
CCS / F620 |
|
|
CCS / A690 |
CCS / D690 |
CCS / E690 |
CCS / F690 |
|