A572 po'lat va A588 po'lat o'rtasidagi farq nima?

Sep 16, 2025 Xabar QOLDIRISH

A572 va A588 konstruktiv po'lat plitalarikkalasi ham konstruktiv ilovalarda qoʻllaniladigan yuqori-mustahkam, past qotishma (HSLA) poʻlat navlaridir, lekin ular oʻziga xos kompozitsiyalari va maqsadlarida farqlanadi:

 

A572 Issiq-prokatlangan konstruktiv po'lat plitalar

 

  • A572 karbonli po'latning kimyoviy tarkibi

Kimyoviy Foiz

Temir

98%

Uglerod

0.21%–0.23%

Marganets

1.35%–1.65%

Silikon

0.15%–0.40%

Oltingugurt

0.03%

Fosfor

0.03%

 

  • A572 uglerod po'latining rentabellik / tortishish kuchi
 

Metrik

Imperator

Kuchlanish kuchi, yakuniy

450 MPa

65,300 psi

Chidamlilik, hosildorlik

345 MPa

50,000 psi

Tanaffusdagi cho'zilish

(200 mm da)

18.0%

18.0%

Tanaffusdagi cho'zilish

(50 mm ichida)

21.0%

21.0%

Brinell qattiqligi

135

135

Rokvellning qattiqligi

74

74

Elastiklik moduli

200 GPa

29 ksi

Kesish moduli

80 GPa

11,6 ksi

 

Darslar: Har xilA572 konstruktiv po'lat plitalar spetsifikatsiyasi doirasidagi navlar (masalan, A572 50 daraja, A572 60 daraja) maxsus dastur talablariga mos keladigan turli darajadagi kuch va boshqa mexanik xususiyatlarni taklif qiladi.

 

A588 HSLA issiq{1}}prokatlangan po'lat plitalar

 

Kimyoviy tarkibi A588 %
Chelik darajasi C Mn P S Si Cu Ni Cr V Mo Nb
A588 A darajasi 0,19 dan kam yoki unga teng 0.80-1.25 0,04 dan kam yoki unga teng 0,05 dan kam yoki unga teng 0.3-0.65 0.25-0.40 0,40 dan kam yoki unga teng 0.4-0.65 0.02-0.10 - -
A588 B darajasi 0,20 dan kam yoki unga teng 0.75-1.35 0,04 dan kam yoki unga teng 0,05 dan kam yoki unga teng 0.15-0.50 0.20-0.40 0,50 dan kam yoki unga teng 0.4-0.70 0.01-0.10 - -
A588 C darajasi 0,15 dan kam yoki unga teng 0.8-1.35 0,04 dan kam yoki unga teng 0,05 dan kam yoki unga teng 0.15-0.40 0.20-0.50 0.25-0.50 0.3-0.50 0.01-0.10 - -
A588 K sinf 0,17 dan kam yoki unga teng 0.5-1.20 0,04 dan kam yoki unga teng 0,05 dan kam yoki unga teng 0.25-0.50 0.30-0.50 0,40 dan kam yoki unga teng 0.4-0.70 - 0,10 dan kam yoki unga teng 0.005-0.50

 

ASTM A588 Chelik plitalar va barlar Boshqa shakllar
<100 mm 100-125 mm dan katta yoki unga teng >125-200  
Kuchlanish kuchi min MPa 485 460 435 485
Oqim kuchi min MPa 345 315 290 345
Uzayish min 21 21 21 21

 

Ilovalar: A588 konstruktiv po'lat plitasi odatda me'moriy xususiyatlar, ko'priklar, uzatish minoralari, yuk vagonlari va korroziyaga chidamlilikni talab qiluvchi boshqa tizimli ilovalarda qo'llaniladi.

 

Farqlar

 

Korroziyaga qarshilik:

A572 super qalin po'lat plitalar A588 ning atmosfera korroziyaga chidamliligini ta'minlaydigan qo'shimcha elementlar tufayli A588 HSLA issiq{2}}prokatli po'lat bilan bir xil darajada korroziyaga chidamliligiga ega emas.

 

Foydalanish maqsadi:

A572 asosan yuqori quvvat talab qiladigan konstruktiv ilovalar uchun ishlatiladi, A588 esa atmosfera korroziyasiga duchor bo'lgan tashqi tuzilmalar uchun maxsus mo'ljallangan.

 

Ob-havo xususiyatlari:

A588 atrof-muhitga ta'sir qilganda vaqt o'tishi bilan himoya patina hosil qiladi va uning atmosfera korroziyasiga chidamliligini oshiradi.

 

A572 va A588 o'rtasida tanlov o'tkazayotganda, qo'llash uchun eng mos materialni aniqlash uchun loyihaning joylashuvi, atmosfera sharoitlariga ta'sir qilish, kerakli mexanik xususiyatlar va korroziyaga chidamlilik zarurati kabi omillarni hisobga oling.

Bepul namuna olish uchun bosing

 

Email:alloy@gneesteelgroup.com
Whatsapp (WeChat): +86 15824687445

 

Boshqa uglerodli va past{0}}qotishma yuqori-po'lat
ASTM/ASME ASTM A36/A36M ASTM A36      
ASTM A283/A283M ASTM A283 A darajasi ASTM A283 B darajasi ASTM A283 C darajasi ASTM A283 D darajasi
ASTM A514/A514M ASTM A514 A darajasi ASTM A514 B darajasi ASTM A514 C darajasi ASTM A514 E darajasi
ASTM A514 F darajasi ASTM A514 H darajasi ASTM A514 J darajasi ASTM A514 K darajasi
ASTM A514 M darajasi ASTM A514 P darajasi ASTM A514 Q darajasi ASTM A514 R darajasi
ASTM A514 S darajasi ASTM A514 T darajasi    
ASTM A572/A572M ASTM A572 42-sinf ASTM A572 50-darajali ASTM A572 55-sinf ASTM A572 60-sinf
ASTM A572 65-sinf      
ASTM A573/A573M ASTM A573 58-sinf ASTM A573 65-sinf ASTM A573 70-sinf  
ASTM A588/A588M ASTM A588 A darajasi ASTM A588 B darajasi ASTM A588 C darajasi ASTM A588 K darajasi
ASTM A633/A633M ASTM A633 A darajasi ASTM A633 C darajasi ASTM A633 D darajasi ASTM A633 E darajasi
ASTM A656/A656M ASTM A656 50-darajali ASTM A656 60-sinf ASTM A656 70-sinf ASTM A656 80-sinf
ASTM A709/A709M ASTM A709 36-sinf ASTM A709 50-darajali ASTM A709 50S darajasi ASTM A709 darajasi 50 Vt
ASTM A709 darajasi HPS 50W ASTM A709 darajasi HPS 70W ASTM A709 100-darajali ASTM A709 darajasi 100 Vt
ASTM A709 darajasi HPS 100W      
ASME SA36/SA36M ASME SA36      
ASME SA283/SA283M ASME SA283 A darajasi ASME SA283 B darajasi ASME SA283 C darajasi ASME SA283 D darajasi
ASME SA514/SA514M ASME SA514 A darajasi ASME SA514 B darajasi ASME SA514 C darajasi ASME SA514 E darajasi
ASME SA514 F darajasi ASME SA514 H darajasi ASME SA514 J darajasi ASME SA514 K darajasi
ASME SA514 M darajasi ASME SA514 P darajasi ASME SA514 Q darajasi ASME SA514 R darajasi
ASME SA514 S darajasi ASME SA514 T darajasi    
ASME SA572/SA572M ASME SA572 42-sinf ASME SA572 50-sinf ASME SA572 55-sinf ASME SA572 60-sinf
ASME SA572 65-sinf      
ASME SA573/SA573M ASME SA573 58-sinf ASME SA573 65-sinf ASME SA573 70-sinf  
ASME SA588/SA588M ASME SA588 A darajasi ASME SA588 B darajasi ASME SA588 C darajasi ASME SA588 K darajasi
ASME SA633/SA633M ASME SA633 A darajasi ASME SA633 C darajasi ASME SA633 D darajasi ASME SA633 E darajasi
ASME SA656/SA656M ASME SA656 50-sinf ASME SA656 60-sinf ASME SA656 70-sinf ASME SA656 80-sinf
ASME SA709/SA709M ASME SA709 36-sinf ASME SA709 50-sinf ASME SA709 50S darajasi ASME SA709 darajasi 50W
ASME SA709 darajasi HPS 50W ASME SA709 darajasi HPS 70W ASME SA709 100-sinf ASME SA709 darajasi 100 Vt
ASME SA709 darajasi HPS 100W      
EN10025 EN10025-2 EN10025-2 S235J0 EN10025-2 S275J0 EN10025-2 S355J0 EN10025-2 S355K2
EN10025-2 S235JR EN10025-2 S275JR EN10025-2 S355JR EN10025-2 S420J0
EN10025-2 S235J2 EN10025-2 S275J2 EN10025-2 S355J2  
EN10025-3 EN10025-3 S275N EN10025-3 S355N EN10025-3 S420N EN10025-3 S460N
EN10025-3 S275NL EN10025-3 S355NL EN10025-3 S420NL EN10025-3 S460NL
EN10025-4 EN10025-4 S275M EN10025-4 S355M EN10025-4 S420M EN10025-4 S460M
EN10025-4 S275ML EN10025-4 S355ML EN10025-4 S420ML EN10025-4 S460ML
EN10025-6 EN10025-6 S460Q EN10025-6 S460QL EN10025-6 S460QL1 EN10025-6 S500Q
EN10025-6 S500QL EN10025-6 S500QL1 EN10025-6 S550Q EN10025-6 S550QL
EN10025-6 S550QL1 EN10025-6 S620Q EN10025-6 S620QL EN10025-6 S620QL1
EN10025-6 S690Q EN10025-6 S690QL EN10025-6 S690Q1 EN10025-6 S890Q
EN10025-6 S890QL EN10025-6 S890QL1 EN10025-6 S960Q EN10025-6 S960QL
JIS JIS G3101 JIS G3101 SS330 JIS G3101 SS400 JIS G3101 SS490 JIS G3101 SS540
JIS G3106 JIS G3106 SM400A JIS G3106 SM400B JIS G3106 SM400C JIS G3106 SM490A
JIS G3106 SM490YA JIS G3106 SM490B JIS G3106 SM490YB JIS G3106 SM490C
JIS G3106 SM520B JIS G3106 SM520C JIS G3106 SM570  
DIN DIN 17100 DIN17100 St52-3 DIN17100 St37-2 DIN17100 St37-3 DIN17100 RSt37-2
DIN17100 USt37-2      
DIN 17102 DIN17102 StE315 DIN17102 ESTE315 DIN17102 TStE315 DIN17102 WStE315
DIN17102 StE355 DIN17102 ESTE355 DIN17102 TStE355 DIN17102 WStE355
DIN17102 StE380 DIN17102 ESTE380 DIN17102 TStE380 DIN17102 WStE380
DIN17102 StE420 DIN17102 ESTE420 DIN17102 TStE420 DIN17102 WStE420
DIN17102 StE460 DIN17102 ESTE460 DIN17102 TStE460 DIN17102 WStE460
DIN17102 StE500 DIN17102 ESTE500 DIN17102 TStE500 DIN17102 WStE500
DIN17102 ESTE285      
GB GB/T700 GB/T700 Q235A GB/T700 Q235B GB/T700 Q235C GB/T700 Q235D
GB/T700 Q275      
GB/T1591 GB/T1591 Q345A GB/T1591 Q390A GB/T1591 Q420A GB/T1591 Q420E
GB/T1591 Q345B GB/T1591 Q390B GB/T1591 Q420B GB/T1591 Q460C
GB/T1591 Q345C GB/T1591 Q390C GB/T1591 Q420C GB/T1591 Q460D
GB/T1591 Q345D GB/T1591 Q390D GB/T1591 Q420D GB/T1591 Q460E
GB/T1591 Q345E GB/T1591 Q390E    
GB/T16270 GB/T16270 Q550C GB/T16270 Q550D GB/T16270 Q550E GB/T16270 Q550F
GB/T16270 Q620C GB/T16270 Q620D GB/T16270 Q620E GB/T16270 Q620F
GB/T16270 Q690C GB/T16270 Q690D GB/T16270 Q690E GB/T16270 Q690F
GB/T16270 Q800C GB/T16270 Q800D GB/T16270 Q800E GB/T16270 Q800F
GB/T16270 Q890C GB/T16270 Q890D GB/T16270 Q890E GB/T16270 Q890F
GB/T16270 Q960C GB/T16270 Q960D GB/T16270 Q960E GB/T16270 Q960F
GB/T16270 Q500      

 

A572 and A588 alloy steel plate

A572 and A588 alloy steel plate

A572 and A588 alloy steel plate

A572 and A588 alloy steel plate

A572 and A588 alloy steel plate