Asosiy farq shundaki, P275NH po'latining minimal oquvchanligi 275 N / mm², P355NH po'lati esa 355 N / mm² ga teng. Ikkalasi ham bosimli idishlar uchun EN 10028-3 standarti bo'yicha normallashtirilgan nozik taneli po'latdir, lekin P355NH kuchliroqdir.

|
P355NH Kimyoviy tarkibi |
|||||||
|
Baho |
Maksimal element (%) |
||||||
|
C |
Si |
Mn |
P |
S |
Al(min) |
N |
|
|
P355NH |
0.20 |
0.50 |
0.9-1.70 |
0.03 |
0.025 |
|
0.02 |
|
Cr |
Cu |
Mo |
Nb |
Ni |
Ti |
V |
|
|
0.30 |
0.30 |
0.08 |
0.005 |
0.50 |
0.03 |
0.10 |
|
Uglerod ekvivalenti: Ceq=【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
|
P275NH Kimyoviy tarkibi |
|||||||
|
Baho |
Maksimal element (%) |
||||||
|
C |
Si |
Mn |
P |
S |
Al(min) |
N |
|
|
P275NH |
0.16 |
0.40 |
0.5-1.40 |
0.030 |
0.020 |
|
0.02 |
|
Cr |
Cu |
Mo |
Nb |
Ni |
Ti |
V |
|
|
0.30 |
0.30 |
0.08 |
0.005 |
0.50 |
0.03 |
0.05 |
|
Uglerod ekvivalenti: Ceq=【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
|
Baho |
|
P355NHMexanik xususiyat |
|||||
|
Qalinligi |
Yo'l bering |
Tensilmie |
Cho'zilish |
Ta'sir energiyasi (KV J) min |
|||
|
P355NH |
mm |
Min Mpa |
Mpa |
Min % |
-20 daraja |
0 daraja |
+20 daraja |
|
16 dan kam yoki teng |
355 |
490-630 |
22 |
47 |
55 |
63 |
|
|
16>35 dan kam yoki teng |
355 |
490-630 |
22 |
47 |
55 |
63 |
|
|
35>50 dan kam yoki unga teng |
345 |
490-630 |
22 |
47 |
55 |
63 |
|
|
50>70 dan kam yoki unga teng |
325 |
490-630 |
22 |
47 |
55 |
63 |
|
|
70>100 dan kam yoki unga teng |
315 |
470-610 |
21 |
47 |
55 |
63 |
|
|
100>150 dan kam yoki unga teng |
295 |
450-590 |
21 |
47 |
55 |
63 |
|
|
Baho |
|
P275NHMexanik xususiyat |
|||||
|
Qalinligi |
Yo'l bering |
Tensilmie |
Cho'zilish |
Ta'sir energiyasi (KV J) min |
|||
|
P275NH |
mm |
Min Mpa |
Mpa |
Min % |
-20 daraja |
0 daraja |
+20 daraja |
|
16 dan kam yoki teng |
275 |
390-510 |
24 |
47 |
55 |
63 |
|
|
16>35 dan kam yoki teng |
275 |
390-510 |
24 |
47 |
55 |
63 |
|
|
35>50 dan kam yoki unga teng |
265 |
390-510 |
24 |
47 |
55 |
63 |
|
|
50>70 dan kam yoki unga teng |
255 |
390-510 |
24 |
47 |
55 |
63 |
|
|
70>100 dan kam yoki unga teng |
235 |
370-490 |
23 |
47 |
55 |
63 |
|
|
100>150 dan kam yoki unga teng |
235 |
350-470 |
23 |
47 |
55 |
63 |
|