P355 N va P355 NH po'latlari o'rtasidagi farq nima?

Oct 20, 2025 Xabar QOLDIRISH

EN 10028-3 P355N / P355NH po'latdan ishlov berish kimyoviy tarkibi

 

Chelik darajasi

Kimyoviy tarkibi

Chelik nomi

Chelik raqami

C maks

Si maks

Mn

P maks

S maks

Al(jami) min

N maks

Cr maks

Cu maks

Mo maks

Nb maks

Ni maks

Ti maks

V maks

Nb+Ti+V maks

P355N

1.0562

0.18

0.50

1.10-1.70

0.025

0.015

0.020

0.012

0.30

0.30

0.08

0.05

0.50

0.03

0.10

0.12

P355NH

1.0565

 

EN 10028-3 P355N / P355NH po'lat konstruktsiyasining mexanik xususiyatlari

 

Chelik darajasi

Umumiy etkazib berish shartlari

po'lat qalinligi
t
mm

hosil kuchi
ReH
MPa
min

Mustahkamlik chegarasi
MPa

Singandan keyin
Cho'zilish
A,% min

Chelik
nomi

Chelik raqami

P355N
P355NH

 

1.0562
1.0565

 

Normallashtirish

16 dan kichik yoki teng

355

490~630

22

16<>

345

40<>

335

60<>

315

470~610

21

100<>

305

460~600

150<>

295

450~590

 

P355N / P355NH po'lat konstruktsiyasi Issiqlik bilan ishlov berish

 

Yuvish, so'ndirish, qaynatish

P355N / P355NH po'lat konstruktsiyasi Chelik xizmatlari:

Kesish, burg'ulash, bukish, qirqish, payvandlash

Professional global po'latdan ishlov beruvchi yetkazib beruvchi sifatida biz sizga malakali P355N / P355NH po'latdan ishlov berish qismlarini raqobatbardosh narxda va tez yetkazib berish vaqtida taklif qilishimizga va'da beramiz. Biz mijozning chizmalariga muvofiq ishlab chiqarishimiz mumkin. Biz omborimizda ko'plab P355N / P355NH po'lat plitalar zaxirasini saqlaymiz. Shunday qilib, siz bizga qo'shilishingiz mumkinligiga chin dildan umid qilamiz. Keling, sizni mahalliy po'lat bozorida etakchi bo'lish uchun birlashaylik.

 

P355NH nima?

Bosimli idishlar uchun nozik taneli strukturaviy po'lat. P355NH po'lati yaxshi payvandlanishi va mo'rt yorilishga yuqori qarshilik bilan ajralib turadi.

 

P355N materiali nima?

P355N sinfi xrom va molibdenli qotishma po'latdir. EN 10216-3 P355N choksiz quvurlarning odatiy kimyosi maksimal 0,08% molibdenga qo'shimcha ravishda maksimal 0,30% xrom bilan ishlab chiqariladi, bu bir nechta xususiyatlarni yaxshilaydi.

 

P355N va P355NH o'rtasidagi farq nima?

P355 N va P355 Nh ikkalasi ham bosimli idish po'latlaridir, ammo ular haroratga qarab mo'ljallangan ilovalarida farqlanadi. P355 N xona haroratida xizmat ko'rsatish uchun mo'ljallangan, P355 Nh esa yuqori haroratli ilovalar uchun mo'ljallangan, ya'ni u yuqori haroratlarda o'z kuchini va xususiyatlarini saqlab qoladi.

 

P355NL1 va P355NL2 o'rtasidagi farq nima?

P355NL1 -40 daraja haroratda sinovdan o'tgan, bu uni oddiy sovuq muhitlar uchun mos qiladi. P355NL2 -50 daraja ko'ndalang zarba sinovlaridan o'tgan, juda past haroratli operatsiyalar uchun ideal bo'lgan yuqori chidamlilikni taklif etadi.

 

p355 ASTM materialiga nima ekvivalent?

P355GH bosimli idish po'lati ASTM A516 Grade 70 va ASME SA516 Grade 70 ga ekvivalentdir. Butun neft-kimyo sanoatida keng qo'llaniladigan P355GH bosimli idish po'lat navi bo'lib, Evro Norm standarti (EN10028) bo'yicha belgilangan bo'lib, Britaniya standarti va D standartlarini o'zgartirgan.

 

Bizga murojaat qiling

 

Agar siz GNEE mahsulotlari haqida ko'proq bilmoqchi bo'lsangiz, elektron pochta manziliga xat yuborishingiz mumkinalloy@gneesteelgroup.com. Biz sizga yordam berishdan xursandmiz.

 

P355N and P355NH

P355N and P355NH

P355N and P355NH

GNEE tomonidan ta'minlangan bosimli idish plitalarining darajalari
ASTM ASTM A202/A202M ASTM A202 A darajasi ASTM A202 B darajasi    
ASTM A203/A203M ASTM A203 A darajasi ASTM A203 B darajasi ASTM A203 D darajasi ASTM A203 E darajasi
ASTM A203 F darajasi      
ASTM A204/A204M ASTM A204 A darajasi ASTM A204 B darajasi ASTM A204 C darajasi  
ASTM A285/A285M ASTM A285 A darajasi ASTM A285 B darajasi ASTM A285 C darajasi  
ASTM A299/A299M ASTM A299 A darajasi ASTM A299 B darajasi    
ASTM A302/A302M ASTM A302 A darajasi ASTM A302 B darajasi ASTM A302 C darajasi ASTM A302 D darajasi
ASTM A387/A387M ASTM A387 5-sinf 1-sinf ASTM A387 5-sinf 2-sinf ASTM A387 11-sinf 1-sinf ASTM A387 11-sinf 2-sinf
ASTM A387 12-sinf 1-sinf ASTM A387 12-sinf 2-sinf ASTM A387 22-sinf 1-sinf ASTM A387 22-sinf 2-sinf
ASTM A515/A515M ASTM A515 60-sinf ASTM A515 65-sinf ASTM A515 70-sinf  
ASTM A516/A516M ASTM A516 55-sinf ASTM A516 60-sinf ASTM A516 65-sinf ASTM A516 70-sinf
ASTM A517/A517M ASTM A517 A darajasi ASTM A517 B darajasi ASTM A517 E darajasi ASTM A517 F darajasi
ASTM A517 P darajasi ASTM A517 J darajasi    
ASTM A533/A533M ASTM A533 A sinfi 1 ASTM A533 B sinfi 1 ASTM A533 C sinfi 1 ASTM A533 D sinfi 1
ASTM A533 A sinfi 2 ASTM A533 B sinfi 2 ASTM A533 C sinfi 2 ASTM A533 D sinfi 2
ASTM A533 A sinfi 3 ASTM A533 B sinfi 3 ASTM A533 C sinfi 3 ASTM A533 D sinfi 3
ASTM A537/A537M ASTM A537 1-sinf ASTM A537 2-sinf ASTM A537 sinf 3  
ASTM A612/A612M ASTM A612      
ASTM A662/A662M ASTM A662 A darajasi ASTM A662 B darajasi ASTM A662 C darajasi  
UZ EN10028-2 EN10028-2 P235GH EN10028-2 P265GH EN10028-2 P295GH EN10028-2 P355GH
UZ10028-2 16MO3      
EN10028-3 EN10028-3 P275N EN10028-3 P275NH EN10028-3 P275NL1 EN10028-3 P275NL2
EN10028-3 P355N EN10028-3 P355NH EN10028-3 P355NL1 EN10028-3 P355NL2
EN10028-3 P460N EN10028-3 P460NH EN10028-3 P460NL1 EN10028-3 P460NL2
EN10028-5 EN10028-5 P355M EN10028-5 P355ML1 EN10028-5 P355ML2 EN10028-5 P420M
EN10028-5 P420ML1 EN10028-5 P420ML2 EN10028-5 P460M EN10028-5 P460ML1
EN10028-5 P460ML2      
EN10028-6 EN10028-6 P355Q EN10028-6 P460Q EN10028-6 P500Q EN10028-6 P690Q
EN10028-6 P355QH EN10028-6 P460QH EN10028-6 P500QH EN10028-6 P690QH
EN10028-6 P355QL1 EN10028-6 P460QL1 EN10028-6 P500QL1 EN10028-6 P690QL1
EN10028-6 P355QL2 EN10028-6 P460QL2 EN10028-6 P500QL2 EN10028-6 P690QL2
JIS JIS G3115 JIS G3115 SPV235 JIS G3115 SPV315 JIS G3115 SPV355 JIS G3115 SPV410
JIS G3115 SPV450 JIS G3115 SPV490    
JIS G3103 JIS G3103 SB410 JIS G3103 SB450 JIS G3103 SB480 JIS G3103 SB450M
JIS G3103 SB480M      
GB GB713 GB713 Q245R GB713 Q345R GB713 Q370R GB713 12Cr1MoVR
GB713 12Cr2Mo1R GB713 13MnNiMoR GB713 14Cr1MoR GB713 15CrMoR
GB713 18MnMoNbR      
GB3531 GB3531 09MnNiDR GB3531 15MnNiDR GB3531 16MnDR  
DIN DIN 17155 DIN 17155 HI DIN 17155 HII DIN 17155 10CrMo910 DIN 17155 13CrMo44
DIN 17155 15Mo3 DIN 17155 17Mn4 DIN 17155 19Mn6