S460N va S420N normallashtirilgan, EN 10025-3 standartiga mos keladigan, yuqori{2}}mustahkam, past{3}}qotishma konstruktiv po'lat plitalar bo'lib, ular asosan oquvchanlik kuchida farqlanadi (S460N uchun 460 MPa va S420N uchun mos va og'irligi uchun {{7}0 MPa) ko'priklar, kranlar va kemalar kabi tuzilmalar, S460N talab qilinadigan yuklar uchun ko'proq quvvatni taklif qiladi va S420N mo''tadil iqlim uchun biroz pastroq quvvatli, yaxshi payvandlanish imkoniyatini taklif qiladi.
S42 ning kimyoviy tarkibi0N po'lat plitalar
|
Element |
Choynak tahlili (maksimal %) |
Mahsulot tahlili (maksimal %) |
|---|---|---|
|
Uglerod (C) |
0.20 |
0.23 |
|
Kremniy (Si) |
0.60 |
0.70 |
|
Marganets (Mn) |
1.00-1.70 |
1.10-1.80 |
|
Fosfor (P) |
0.025 |
0.035 |
|
Oltingugurt (S) |
0.015 |
0.025 |
|
Azot (N) |
0.025 |
0.030 |
|
Alyuminiy (Al) |
0,020 (daq, jami) |
0,020 (daq, jami) |
|
Niobiy (Nb) |
0.05 |
0.06 |
|
Vanadiy (V) |
0.10 |
0.12 |
|
Titan (Ti) |
0.05 |
0.07 |
|
Xrom (Cr) |
0.30 |
0.35 |
|
Nikel (Ni) |
0.80 |
0.85 |
|
Molibden (Mo) |
0.10 |
0.12 |
S460N po'lat plitasining kimyoviy tarkibi
|
Element |
Choynak tahlili (maksimal %) |
Mahsulot tahlili (maksimal %) |
|---|---|---|
|
Uglerod (C) |
0.20 |
0.23 |
|
Kremniy (Si) |
0.60 |
0.70 |
|
Marganets (Mn) |
1.70 |
1.80 |
|
Fosfor (P) |
0.025 |
0.035 |
|
Oltingugurt (S) |
0.015 |
0.025 |
|
Azot (N) |
0.025 |
0.030 |
|
Alyuminiy (Al) |
0,020 (daq, jami) |
0,020 (daq, jami) |
|
Niobiy (Nb) |
0.05 |
0.06 |
|
Vanadiy (V) |
0.12 |
0.15 |
|
Titan (Ti) |
0.05 |
0.07 |
S420N po'lat plitalarining mexanik xususiyatlari
|
Qalinligi (mm) |
Hosildorlik kuchi (min, MPa) |
Kuchlanish kuchi (MPa) |
Uzayish (min,%) |
Ta'sir energiyasi (min, J @ -20 daraja) |
|---|---|---|---|---|
|
16 dan kam yoki teng |
420 |
520-680 |
19 |
27 |
|
16<> |
400 |
520-680 |
19 |
27 |
|
40<> |
390 |
520-680 |
19 |
27 |
|
63<> |
340 |
520-680 |
19 |
27 |
|
80<> |
290 |
520-680 |
19 |
27 |
|
100<> |
260 |
520-680 |
20 |
27 |
|
150<> |
220 |
500-650 |
20 |
27 |
S460N po'lat plitalarining mexanik xususiyatlari
|
Qalinligi (mm) |
Hosildorlik kuchi (min, MPa) |
Kuchlanish kuchi (MPa) |
Uzayish (min,%) |
Ta'sir energiyasi (min, J @ -20 daraja) |
|---|---|---|---|---|
|
16 dan kam yoki teng |
460 |
540-720 |
17 |
27 |
|
16<> |
460 |
540-720 |
17 |
27 |
|
40<> |
440 |
570-720 |
17 |
27 |
|
63<> |
400 |
570-720 |
17 |
27 |
|
80<> |
380 |
570-720 |
17 |
27 |
|
100<> |
340 |
540-720 |
18 |
27 |
Asosiy xususiyatlar
Standart: ikkalasi ham yaxshi payvandlanishi va zarbaga chidamliligini ta'minlaydigan normallashtirilgan nozik konstruktiv po'latlar uchun EN 10025-3 standartiga to'g'ri keladi.
Kuchliligi: S460N minimal oqish quvvati 460 MPa, S420N esa 420 MPa ga ega, bu esa S460Nni ogʻir{5}}ilovalar uchun kuchliroq qiladi.
Ilovalar: Katta payvandlangan tuzilmalarda, jumladan, ko'priklar, kranlar, elektr stantsiyalari uskunalari, qozonxonalar va tog'-kon mashinalarida qo'llaniladi.
Payvandlash imkoniyati: Ikkalasi ham yaxshi payvandlanish qobiliyatini ta'minlaydi, ko'pincha oldindan qizdirishni va mos sarf materiallarini (masalan, ER70S-6) talab qiladi, ishlab chiqarishga yordam beradigan past uglerod ekvivalentlari (CEV).
Past-Temp chidamlilik: “N” normallashtirilgan yetkazib berishni bildiradi, yaxshi qattiqlikni taʼminlaydi, “NL” darajalari sovuqroq iqlimlar uchun past haroratlarda (masalan, -50 daraja va S460N -20 daraja) yanada yaxshi ishlashni taklif qiladi.