Aug 20, 2025 Xabar QOLDIRISH

S690Q VS S690QL: "L" balandlikdagi "L" - quvvatli po'lat

(690 MPA ramzi|en 10025-6 standart)

 

Asosiy farq: past - Harorat qattiqligi

info-256-257

S690Q: Minimal ta'sir kuchayishi -20 darajali (o'rtacha 30j). → Odatda foydalanish: Tegishli iqlimlarning, karchilik uskunalari.

S690QL:-40 daraja va undan yuqori darajadagi (40j gacha katta yoki unga teng). → tanqidiy foydalanish: Arktika quvurlari, offshor platformalari, Sibirda tog'-kon avtomobillari.

 

Noto'g'ri ta'minlanganlik uchun xavf: S690Q -20 darajali xavfni kamaytirish (masalan, Kanada burg'ulash joyi) 2020 yilda qulashi mumkin.

 

Kimyoviy va ishlov berish farqlari

 

Parametrlar690qlmmax oltingugurt (s) 0,010% 0,010% 0.47 ga teng (CARBON ekvivalenti) 1. {Carbon ekvivalenti (Carbonati ekvivalenti) (MN + MO) / 10 + (CR + Cu) /20 + Ni / 40

 

Nima uchun "L" real loyihalarda

 

Offshor shamol turbinalari: S690QL-yoğuralarda -30 darajadagi dengizlarda ishlatiladi (masalan, HornSea 2, Buyuk Britaniya). Moddiy muvaffaqiyatsizlik darajasi: S690Q uchun 0,2% vs 5%.

Narxlarning ta'siri: S690QL narxi 15% ga ko'p turadi, ammo 6-12 yilga, korroziy muhitda xizmat ko'rsatadi.

Payvandlash: S690QL vodorodni oldini olish uchun qat'iy qiziydi (150-250 daraja) ni talab qiladi.

 

Global standartlar va ekvivalentlar

 

Evropa (en 10025-6): S690Q===s690ql

China (GB/T 16270): S690Q ≈ Q690D / S690QL ≈ Q690E (stricter low-temp requirements)

AQSh (ASTM): A514 sinfiga teng (lekin majburiy -40 daraja sinovi yo'q).

 

Qaror nazorat ro'yxati

info-244-165

Agar S690Q ni tanlang:

  • Operatsion templar> -20 darajasi
  • Byudjet sezgirligi mavjud
  • Qalinligi <40 mm (yo'q z {{{{{{{{{{{{{{{{{{{{{{{{{{- stressda)

 

S690QL-ga o'ting:

  • Atrof atrofidagi yoki -40 darajadan kam yoki unga teng yoki teng bo'lgan
  • Qalin plitalar (40 mm ga teng) derazani kechiktirish
  • Vodorod ta'sir qilish (quvurlar, hg)

 

Har qanday savol yoki har qanday savollar uchun iltimos, men bilan bemalol bog'laning.

Elektron pochta:alloy@gneesteelgroup.com
Whatsapp (wovapp): +86-15824687445

 

Boshqa po'lat plastinka
Ism Material Shikastlanish (mm) Tonna Izoh
Past qotishma Q34aa, Q345B, Q345D, Q345D, Q360C, Q460C, ST52-3, S355J {{10} S355J, S275NGC, S275NG, S275NG, 35cro 6 - 350 5788.56 Normallashtirish, temperli, boshqariladigan ruling, issiqlik, issiqlik, issiqlik, issiqlik, 1-chi tekshirish, 2-chi tekshirish, 3-chi tekshirish
Bosimli bosim Q245R, Q345R, Q370R, 16MNDR, 09mnidr, 15cr16Gr60, SA516Gr60, SA516Gr405, SA187Gr11, SA387GR12, SA387GR12, SA387GR12, P265,P295,P355GH,Q245R(R-HIC),Q345R(R-HIC) 3 - 300 8650 Normallashtirish, temperli, boshqariladigan ruling, issiqlik, issiqlik, issiqlik, issiqlik, 1-chi tekshirish, 2-chi tekshirish, 3-chi tekshirish
Yuqori - kuchi Wh785d / E, Q890D / E, WH60d / E, Q550D, Q550D, Q690D, Q690D, Q690D, Q690D, Q690D, Q690D, Q690D, Q690D, Q690D, Q690D, Q690D, Q690D, Q690D, Q690D, Q690D, Q690D, Q690D, Q690D, Q690D, Q690D, Q690D, Q690D, Q690D, Q690D, Q690D, Q690D, Q690D, Q690D, Q690D, Q690D / E 8 - 120 3086.352 Qoniqdi va tebrandi
- chidamli plitalar NM360, NM400, NM450, NM500 6 - 150 3866.297 Qoniqdi va tebrandi
Ko'prik plitasi Q2355QC, Q345QC, Q320QC, Q345QDNH, Q3709 - 50, a 709 - 50 t - 2 8 - 200 2853.621 Issiq rulon, normallashtirilgan, issiq rulonli boshqariladigan rulon, qon to'kilgan va tebranishi