Q345HD po'lat plitasi

Aug 26, 2025 Xabar QOLDIRISH

Q345HD "Q" Yadro elektr po'lat po'latida, "345" po'lat plastinkaga tegishli, bu esa "atom quvvat" so'zining boshida eng kichik kapitalning hosilini anglatadi. Q345HD ikki sinfga ega: Q345HD1 va Q345HD2.

Q345HD po'lat plastinka eritish moslamalari tahlili:
C: 0.24 dan kam yoki unga teng: 0,15-0,4, mN: 0.015, S: 0,4-0,6 ga teng: 0.45-0,6 ga teng: 0.45-0,6 ga teng: 0,4-0,6 ga teng: 0,4-0,6 ga teng: 0,4-0,6 ga teng: 0,4-0,6 ga teng: 0,4-0,6 ga teng: 0,02, v) dan kam yoki unga teng 0.05, Ti: 0.03 dan kam yoki unga teng yoki unga teng: 0.02-0.04, b: 0,001, 0,04 dan kam yoki unga teng

Q345HD yadro po'latosi plastinka mexanik xususiyatlari (6-38mm):
RP0.2 (MPA): 345 ga qaraganda ko'proq yoki teng
RM (MPA): 550-690
A (%): 18 ga teng yoki teng

Q345hd po'lat plitasining ijro etuvchi standarti: GB / T 30814-2014; Boshqa materiallar: Q205HD, Q230HD, Q250HD, Q250HD, Q245HD, Q345HD1, Q420HD.

Q345HD issiq rollash holatida issiqlik, issiq rulonli plyaji, normalizatsiya, normallashtirish, normallashtirishni normallashtirish.

Q345HD po'lat plitasining asosiy xususiyatlari: atom elektr stansiyasi yaxshi tarkibiy barqarorlik, payvandlash, sovuqqonlik va issiqlik va issiqlik kuchiga ega va reaktsiyani nurlantirish bo'yicha yadroviy charchoq kuchiga ega va reaktsiyani nurlantirish davrida yaxshi qarshilik ko'rsatadi.

 

wechat2025-07-16094237523

4. Q345HD po'lat plitasi etkazib berish holati
Temir plastinka qonli + tempered + tempered yoki qonli holatda etkazib beriladi. Etkazib berish holati texnik talablarga muvofiq ham belgilanishi mumkin.

5. Q3455hd po'lat plitasi -
Z15, Z25, Z35.

6. Q345HD po'lat plastinka ultratovush tekshiruvi talablari
UT sinfi 1, UT sinfi 2, UT 3-sinf.

7. Q345HD po'lat plitasi zichligi
7.85 g / sm³.

8. Q3455HD po'lat plastinka nazariy vazni formulasi
Qalinlik*Kenglik*Uzunligi*Zichlik.

9. Q345HD po'lat plitasi an'anaviy o'lchamlari
8mm-150mm *1600 mm - 2500 mm*3000-12000mm

 

wechat2025-07-16094137182

Q345HD po'lat plitalar ishlab chiqarish va kesish jarayoni oqimi

Ishlab chiqarish jarayoni:
Birlamchi SMeling → LF ni qayta ishlash → VD Castinging) → Tozalash, isitish → Ultrasonik sinov → Ultrasonik sinov → Chiqish va namuna olish → Ishlash testi → Saqlash.

Kesish jarayoni:
After the performance indicators of the Q345HD steel plate meet the requirements in the factory inspection, cutting processing is carried out according to the cutting technology. It can be cut and processed based on drawings. Generally, when the steel plate thickness is ≤20 mm, CNC plasma cutting or CNC laser cutting is preferred. If the steel plate thickness is >30 mm, CNC Flane kemasi odatda kesish aniqligi va vaqtini boshqarish uchun tanlanadi.

Q345HD-ning buyurtma jarayoni bilan tanishish

Muayyan o'lchamlar, texnik xususiyatlar va miqdori.

Minimal partiyaviy buyurtma 60 tonna.

Till etkazib berish tsiklini va blok narxini tasdiqlaydi.

Yetkazib beruvchi bilan aloqa va moslash.

Tsikl va narx bo'yicha shartnoma tuzish.

MILLIY METALATAL MA'LUMOT KODI.

Etkazib berishni kutish.