JIS G3125 darajasi SPA-C korten po'lat plitalar xususiyatlari
JIS G3125 SPA-C po'lat plitasi - bu ob-havoga chidamli po'lat plitalar. Tegishli standart JIS G3125. JIS G3125 SPA-C po'lat plitalarining ekvivalent materiallari GB / T Q345GNHL po'lat va AS WR350/2 po'latdir.
JIS G3125 SPA-C nurash po'latining ishlashi
| Baho |
Elastik modul |
190 - 210 GPa 20 daraja |
|
JIS G3125 SPA-C darajasi |
Uzayish A5 |
20 daraja haroratda 26% |
|
Puasson nisbati |
0.3 [-] 20 daraja |
|
|
Mustahkamlik chegarasi |
20 daraja haroratda 450 MPa |
|
|
Hosildorlik kuchi |
20 daraja haroratda 315 MPa |