LR DH62 Kema qurish po'lat plitasi

Nov 14, 2025 Xabar QOLDIRISH

LR Grade DH62 Shipbuilding po'lat plitasi asosan kema qurish loyihasi va Okean offshore strukturaviy loyiha uchun ishlatiladi.

LR darajasi DH62 kema qurish po'lat plitalar Boshqa nomi

LR darajali DH62 kema qurish po'lat plitasi, LR darajali DH62 kema po'lat plitasi, LR darajali DH62 dengiz po'lat plitasi, LR darajali DH62 po'lat plitalar.

Qo'shimcha shart

UT (Ultratovush tekshiruvi), AR (Faqat issiq haddelenmiş holda), TMCP (Termal mexanik nazoratni qayta ishlash), N (Normallashtirilgan), Q+T (O'chirilgan va Temperlangan), Z yo'nalishi testi (Z15, Z25, Z35), Charpy V-Notch ta'siri testi, Uchinchi tomon SG testi va sinovlari (shu kabilar),

 

LR DH62 qo'shimcha yuqori kuchli kimyoviy tarkibi

Baho

Maksimal element (%)

C

Si

Mn

P

S

Al

N

LR DH62

0.20

0.55

1.70

0.030

0.030

0.015

0.020

Nb

V

Ti

Cu

Cr

Ni

Mo

0.02-0.05

0.03-0.10

0.02

 

 

 

 

Yoriq sezgirligi: pcm=(C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Uglerod ekvivalenti: Ceq=【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%

 

 

LR DH62 qo'shimcha yuqori quvvat xususiyati

Baho

 

Mexanik xususiyat

Charpy V ta'sir sinovi

Qalinligi

Yo'l bering

Kuchlanish

Cho'zilish

Daraja

Energiya 1

Energiya 2

LR DH62

mm

Min Mpa

Mpa

Min %

-20

J

J

t 50 dan kam yoki teng

620

720-890

17%

41

62

50<t 70 dan kam yoki teng

620

720-890

17%

41

62

70<t 100 dan kam yoki teng

620

720-890

17%

41

62

Eslatma: Energiya 1 - ko'ndalang zarba sinovi, Energiya 2 - uzunlamasına