Bosimli idish va qozon po'lat P355ML1,P355ML1 po'lat plitalar,P355ML1 po'lat plitalari termomexanik prokat ostida issiqlik bilan ishlov berishdan o'tishi kerak. Bu ishlov berish P355ML1 po'lat plitasining material xususiyatlariga salbiy ta'sir ko'rsatmasdan yaxshi sovuq shakllanish va issiq shakllanish xususiyatlarini taklif qiladi.
P355ML2 po'lat plitalar, low harorat ta'sir sinov minus 40 darajada amalga oshirilishi lozim .Bosim idishi va qozon po'lat plitalar P355ML2 prokat paytida termomexanik haddelenmiş ostida issiqlik bilan ishlov berish amalga oshiriladi. Bu ishlov berish material xususiyatlariga salbiy ta'sir qilmasdan yaxshi sovuq shakllanish va issiq shakllanish xususiyatlarini taklif qiladi. Shunday qilib, bu po'lat P355ML2, shuning uchun ham sovutish uchun mos{8}} sovuq-flanj, shuningdek, sovuq-egilish va sovuq{11}}katlama uchun.
EN10028-5 P355ML1 ML2 bosimli idish va qozon po'lat plitalari Kimyoviy tarkibi va mexanik xususiyatlari
|
EN10028-5 P355ML1Kimyoviy tarkibi |
|||||||
|
Baho |
Maksimal element (%) |
||||||
|
C |
Si |
Mn |
P |
S |
Al |
N |
|
|
P355ML1 |
0,14 |
0,50 |
1,60 |
0,020 |
0,015 |
0,020 |
0,015 |
|
Nb |
V |
Ti |
Ni |
Mo |
|
|
|
|
0,05 |
0,10 |
0,05 |
0,50 |
0,20 |
|
|
|
|
Baho |
P355ML1 Mexanik xususiyat |
|||
|
Qalinligi |
Yo'l bering |
Kuchlanish |
Cho'zilish |
|
|
P355ML1 |
mm |
Min Mpa |
Mpa |
Min % |
|
6-16 |
355 |
450-610 |
22% |
|
|
16-40 |
355 |
450-610 |
22% |
|
|
40-63 |
345 |
450-610 |
22% |
|
|
EN10028-5 P355ML2Kimyoviy tarkibi |
|||||||
|
Baho |
Maksimal element (%) |
||||||
|
C |
Si |
Mn |
P |
S |
Al |
N |
|
|
P355ML2 |
0,14 |
0,50 |
1,60 |
0,020 |
0,015 |
0,020 |
0,015 |
|
Nb |
V |
Ti |
Ni |
Mo |
|
|
|
|
0,05 |
0,10 |
0,05 |
0,50 |
0,20 |
|
|
|
|
Baho |
P355ML2 Mexanik xususiyat |
|||
|
Qalinligi |
Yo'l bering |
Kuchlanish |
Cho'zilish |
|
|
P355ML2 |
mm |
Min Mpa |
Mpa |
Min % |
|
6-16 |
355 |
450-610 |
22% |
|
|
16-40 |
355 |
450-610 |
22% |
|
|
40-63 |
345 |
450-610 |
22% |
|
P355ML1 / ML2 po'lat plitalar uchun texnik talablar va qo'shimcha xizmatlar
♦ Yuqori kuchlanish sinovi
♦ Past haroratga ta'sir qilish testi
♦ Payvandlangan issiqlik bilan ishlov berishning simulyatsiyasi-(PWHT)
♦ EN 10160, ASTM A435, A577, A578 bo'yicha ultratovush tekshiruvi
♦ EN 10204 FORMAT 3.1/3.2 bo'yicha original tegirmon sinov sertifikati berilgan
♦ Yakuniy foydalanuvchining talabiga binoan portlatish va bo'yash, kesish va payvandlash
EN10028-5 P355ML1 ML2 Bosimli idish va qozon uchun po'lat plitalar ilovasi
EN10028-5 P355ML1 / ML2 bosimli idish va qozon po'lat plitasi neft, gaz loyihasida bosimli idish, qozon, saqlash tanklari va issiqlik almashtirgichda qo'llaniladi.
EN10028-5 P355ML1 ML2 Bosimli idish va qozon po'lat plitalari Boshqa nom
EN10028-5 P355ML1 ML2 Qozon po'lat plitasi, EN10028-5 P355ML1 ML2 Bosimli idish po'lat plastinka, EN10028-5 P355ML1 ML2 saqlash tanklari Chelik plastinka. EN10028-5 P355ML1 ML2 issiqlik almashinuvchisi po'lat plitalar.
Qo'shimcha shart
UT (Ultratovush tekshiruvi), AR (Faqat issiq haddelenmiş holda), TMCP (Termal mexanik nazoratni qayta ishlash), N (Normallashtirilgan), Q+T (O'chirilgan va Temperlangan), Z yo'nalishi testi (Z15, Z25, Z35), Charpy V-Notch ta'siri testi, Uchinchi tomon SG testi va sinovlari (shu kabilar),
Agar siz GNEE mahsulotlari haqida ko'proq bilmoqchi bo'lsangiz, elektron pochta manziliga xat yuborishingiz mumkinalloy@gneesteelgroup.com. Biz sizga yordam berishdan xursandmiz.



| GNEE tomonidan ta'minlangan bosimli idish plitalarining darajalari | |||||
| ASTM | ASTM A202/A202M | ASTM A202 A darajasi | ASTM A202 B darajasi | ||
| ASTM A203/A203M | ASTM A203 A darajasi | ASTM A203 B darajasi | ASTM A203 D darajasi | ASTM A203 E darajasi | |
| ASTM A203 F darajasi | |||||
| ASTM A204/A204M | ASTM A204 A darajasi | ASTM A204 B darajasi | ASTM A204 C darajasi | ||
| ASTM A285/A285M | ASTM A285 A darajasi | ASTM A285 B darajasi | ASTM A285 C darajasi | ||
| ASTM A299/A299M | ASTM A299 A darajasi | ASTM A299 B darajasi | |||
| ASTM A302/A302M | ASTM A302 A darajasi | ASTM A302 B darajasi | ASTM A302 C darajasi | ASTM A302 D darajasi | |
| ASTM A387/A387M | ASTM A387 5-sinf 1-sinf | ASTM A387 5-sinf 2-sinf | ASTM A387 11-sinf 1-sinf | ASTM A387 11-sinf 2-sinf | |
| ASTM A387 12-sinf 1-sinf | ASTM A387 12-sinf 2-sinf | ASTM A387 22-sinf 1-sinf | ASTM A387 22-sinf 2-sinf | ||
| ASTM A515/A515M | ASTM A515 60-sinf | ASTM A515 65-sinf | ASTM A515 70-sinf | ||
| ASTM A516/A516M | ASTM A516 55-sinf | ASTM A516 60-sinf | ASTM A516 65-sinf | ASTM A516 70-sinf | |
| ASTM A517/A517M | ASTM A517 A darajasi | ASTM A517 B darajasi | ASTM A517 E darajasi | ASTM A517 F darajasi | |
| ASTM A517 P darajasi | ASTM A517 J darajasi | ||||
| ASTM A533/A533M | ASTM A533 A sinfi 1 | ASTM A533 B sinfi 1 | ASTM A533 C sinf 1 | ASTM A533 D sinfi 1 | |
| ASTM A533 A sinfi 2 | ASTM A533 B sinfi 2 | ASTM A533 C sinfi 2 | ASTM A533 D sinfi 2 | ||
| ASTM A533 A sinfi 3 | ASTM A533 B sinfi 3 | ASTM A533 C sinfi 3 | ASTM A533 D sinfi 3 | ||
| ASTM A537/A537M | ASTM A537 1-sinf | ASTM A537 2-sinf | ASTM A537 sinf 3 | ||
| ASTM A612/A612M | ASTM A612 | ||||
| ASTM A662/A662M | ASTM A662 A darajasi | ASTM A662 B darajasi | ASTM A662 C darajasi | ||
| UZ | EN10028-2 | EN10028-2 P235GH | EN10028-2 P265GH | EN10028-2 P295GH | EN10028-2 P355GH |
| UZ10028-2 16MO3 | |||||
| EN10028-3 | EN10028-3 P275N | EN10028-3 P275NH | EN10028-3 P275NL1 | EN10028-3 P275NL2 | |
| EN10028-3 P355N | EN10028-3 P355NH | EN10028-3 P355NL1 | EN10028-3 P355NL2 | ||
| EN10028-3 P460N | EN10028-3 P460NH | EN10028-3 P460NL1 | EN10028-3 P460NL2 | ||
| EN10028-5 | EN10028-5 P355M | EN10028-5 P355ML1 | EN10028-5 P355ML2 | EN10028-5 P420M | |
| EN10028-5 P420ML1 | EN10028-5 P420ML2 | EN10028-5 P460M | EN10028-5 P460ML1 | ||
| EN10028-5 P460ML2 | |||||
| EN10028-6 | EN10028-6 P355Q | EN10028-6 P460Q | EN10028-6 P500Q | EN10028-6 P690Q | |
| EN10028-6 P355QH | EN10028-6 P460QH | EN10028-6 P500QH | EN10028-6 P690QH | ||
| EN10028-6 P355QL1 | EN10028-6 P460QL1 | EN10028-6 P500QL1 | EN10028-6 P690QL1 | ||
| EN10028-6 P355QL2 | EN10028-6 P460QL2 | EN10028-6 P500QL2 | EN10028-6 P690QL2 | ||
| JIS | JIS G3115 | JIS G3115 SPV235 | JIS G3115 SPV315 | JIS G3115 SPV355 | JIS G3115 SPV410 |
| JIS G3115 SPV450 | JIS G3115 SPV490 | ||||
| JIS G3103 | JIS G3103 SB410 | JIS G3103 SB450 | JIS G3103 SB480 | JIS G3103 SB450M | |
| JIS G3103 SB480M | |||||
| GB | GB713 | GB713 Q245R | GB713 Q345R | GB713 Q370R | GB713 12Cr1MoVR |
| GB713 12Cr2Mo1R | GB713 13MnNiMoR | GB713 14Cr1MoR | GB713 15CrMoR | ||
| GB713 18MnMoNbR | |||||
| GB3531 | GB3531 09MnNiDR | GB3531 15MnNiDR | GB3531 16MnDR | ||
| DIN | DIN 17155 | DIN 17155 HI | DIN 17155 HII | DIN 17155 10CrMo910 | DIN 17155 13CrMo44 |
| DIN 17155 15Mo3 | DIN 17155 17Mn4 | DIN 17155 19Mn6 | |||