EN10028-6 P355Qbosimli idishlar va qozonlar uchun cho'ktiriladigan va qattiqlashtirilgan-payvandlanadigan, nozik po'latdir. U yuqori bosim va haroratga bardosh berishga mo'ljallangan bo'lib, uni neft, gaz, saqlash tanklari va issiqlik almashtirgichlarda qo'llash uchun mos keladi.
P355Q po'lat plitalari uchun mexanik xususiyat
| Qalinligi (mm) | |||
| P355Q | 50 dan kam yoki teng | >50 100 dan kam yoki teng | > 100 |
| Oqim kuchi (Mpa dan katta yoki unga teng) | 355 | 335 | 315 |
| 100 dan kam yoki teng | > 100 | ||
| Kuchlanish kuchi (Mpa) | 490-630 | 450-590 | |
P355Q po'lat plitalarining kimyoviy tarkibi (issiqlik tahlili maksimal%)
| P355Q po'lat plitasining asosiy kimyoviy elementlari tarkibi | |||||||
| C | Si | Mn | P | S | B | N | Cr |
| 0.16 | 0.40 | 1.50 | 0.025 | 0.015 | 0.005 | 0.015 | 0.30 |
| Cu | Mo | Nb | Ni | Ti | V | Zr | |
| 0.30 | 0.25 | 0.05 | 0.50 | 0.03 | 0.06 | 0.05 | |
EN10028-6 P355Q bosimli idish va qozon uchun po'lat plitalar ilovasi

Kimyoviy reaktsiya idishlari
EN10028-6 P355Q qozon va bosimli idish po'lat plitasi sintez reaktsiyalarida (masalan, o'g'it zavodlarida ammiak sintez minoralari va kimyoviy zavodlarda polimerizatsiya reaktorlari) ishlatiladi. U yuqori harorat va bosimlarga (masalan, ammiak sintezi minorasi 30MPa bosim va 450 daraja haroratda ishlaydi) va o'rta korroziyaga (masalan, vodorod va kislota gazlari) qarshilik ko'rsatishi kerak, buning natijasida hech qanday oqish yoki struktura buzilishi sodir bo'lmaydi.
Neft-kimyo saqlash tanklari va minoralari
EN10028-6 P355Q past haroratli bosimli idish po'lat plitasi xom neft, suyultirilgan gaz (LNG) va suyultirilgan neft gazi (LPG) saqlash tanklarida, shuningdek, neftni qayta ishlashda rektifikatsion minoralar va assimilyatsiya minoralarida (normal harorat va bosimli tanklar kabi) ishlatiladi. past-haroratli saqlash idishlari (masalan, -162 darajagacha past haroratli LNG saqlash tanklari) past haroratlarda po‘latning mo‘rt sinishiga yo‘l qo‘ymaslik uchun past haroratda mukammal mustahkamlikka ega po‘lat plitalarni talab qiladi; yuqori bosimli gidrogenatsiya minoralari (neft-kimyoni gidrotozalash jarayoni).
Issiqlik almashinuvi idishlari
EN10028-6 P355Q yuqori-sifatli qozon po'lat plitasi o'rtacha issiqlik almashinuvi uchun uskunalarda (masalan, qobiqli va quvurli issiqlik almashtirgichlar va plastinka issiqlik almashinuvchilari) ishlatiladi. Ularning chig'anoqlari va quvurlari varaqlari o'zgaruvchan issiq va sovuq zarbalarga bardosh berishi, charchoqqa chidamliligini ta'minlashi va tez-tez harorat o'zgarishi natijasida payvand choki yorilishiga yo'l qo'ymaslik kerak.
Metallurgiya sanoati
Po'lat zavodlarida (0,5-1,5MPa bosim va 1200 daraja haroratda yuqori{0}}haroratli issiq havoni saqlaydigan yuqori o'choqli issiq do'mna pechi) yuqori haroratga chidamli EN10028-6 P355Q plitasi; rangli metallarni eritishda "avtoklav" (masalan, gidrometallurgik mis eritishda yuvish avtoklav) kislotali korroziyaga chidamli bo'lishi kerak va EN10028-6 P355Q bosimli idish po'lat plitasi odatda qo'llaniladi.
EN10028-6 P355Q bosimli idish va qozon po'lat plitasi Boshqa nom
EN10028-6 P355Q qozon po'lat plitasi, EN10028-6 P355Q bosimli idish po'lat plitasi, EN10028-6 P355Q saqlash tanklari po'lat plastinka. EN10028-6 P355Q issiqlik almashinuvchisi po'lat plitalar.
Qo'shimcha shart
UT (Ultratovush tekshiruvi), AR (Faqat issiq haddelenmiş holda), TMCP (Termal mexanik nazoratni qayta ishlash), N (Normallashtirilgan), Q+T (O'chirilgan va Temperlangan), Z yo'nalishi testi (Z15, Z25, Z35), Charpy V-Notch ta'siri testi, Uchinchi tomon SG testi va sinovlari (shu kabilar),
Agar siz GNEE mahsulotlari haqida ko'proq bilmoqchi bo'lsangiz, elektron pochta manziliga xat yuborishingiz mumkinalloy@gneesteelgroup.com.Biz sizga yordam berishdan xursandmiz.
| GNEE tomonidan ta'minlangan bosimli idish plitalarining darajalari | |||||
| ASTM | ASTM A202/A202M | ASTM A202 A darajasi | ASTM A202 B darajasi | ||
| ASTM A203/A203M | ASTM A203 A darajasi | ASTM A203 B darajasi | ASTM A203 D darajasi | ASTM A203 E darajasi | |
| ASTM A203 F darajasi | |||||
| ASTM A204/A204M | ASTM A204 A darajasi | ASTM A204 B darajasi | ASTM A204 C darajasi | ||
| ASTM A285/A285M | ASTM A285 A darajasi | ASTM A285 B darajasi | ASTM A285 C darajasi | ||
| ASTM A299/A299M | ASTM A299 A darajasi | ASTM A299 B darajasi | |||
| ASTM A302/A302M | ASTM A302 A darajasi | ASTM A302 B darajasi | ASTM A302 C darajasi | ASTM A302 D darajasi | |
| ASTM A387/A387M | ASTM A387 5-sinf 1-sinf | ASTM A387 5-sinf 2-sinf | ASTM A387 11-sinf 1-sinf | ASTM A387 11-sinf 2-sinf | |
| ASTM A387 12-sinf 1-sinf | ASTM A387 12-sinf 2-sinf | ASTM A387 22-sinf 1-sinf | ASTM A387 22-sinf 2-sinf | ||
| ASTM A515/A515M | ASTM A515 60-sinf | ASTM A515 65-sinf | ASTM A515 70-sinf | ||
| ASTM A516/A516M | ASTM A516 55-sinf | ASTM A516 60-sinf | ASTM A516 65-sinf | ASTM A516 70-sinf | |
| ASTM A517/A517M | ASTM A517 A darajasi | ASTM A517 B darajasi | ASTM A517 E darajasi | ASTM A517 F darajasi | |
| ASTM A517 P darajasi | ASTM A517 J darajasi | ||||
| ASTM A533/A533M | ASTM A533 A sinfi 1 | ASTM A533 B sinfi 1 | ASTM A533 C sinfi 1 | ASTM A533 D sinfi 1 | |
| ASTM A533 A sinfi 2 | ASTM A533 B sinfi 2 | ASTM A533 C sinfi 2 | ASTM A533 D sinfi 2 | ||
| ASTM A533 A sinfi 3 | ASTM A533 B sinfi 3 | ASTM A533 C sinfi 3 | ASTM A533 D sinfi 3 | ||
| ASTM A537/A537M | ASTM A537 1-sinf | ASTM A537 2-sinf | ASTM A537 sinf 3 | ||
| ASTM A612/A612M | ASTM A612 | ||||
| ASTM A662/A662M | ASTM A662 A darajasi | ASTM A662 B darajasi | ASTM A662 C darajasi | ||
| UZ | EN10028-2 | EN10028-2 P235GH | EN10028-2 P265GH | EN10028-2 P295GH | EN10028-2 P355GH |
| UZ10028-2 16MO3 | |||||
| EN10028-3 | EN10028-3 P275N | EN10028-3 P275NH | EN10028-3 P275NL1 | EN10028-3 P275NL2 | |
| EN10028-3 P355N | EN10028-3 P355NH | EN10028-3 P355NL1 | EN10028-3 P355NL2 | ||
| EN10028-3 P460N | EN10028-3 P460NH | EN10028-3 P460NL1 | EN10028-3 P460NL2 | ||
| EN10028-5 | EN10028-5 P355M | EN10028-5 P355ML1 | EN10028-5 P355ML2 | EN10028-5 P420M | |
| EN10028-5 P420ML1 | EN10028-5 P420ML2 | EN10028-5 P460M | EN10028-5 P460ML1 | ||
| EN10028-5 P460ML2 | |||||
| EN10028-6 | EN10028-6 P355Q | EN10028-6 P460Q | EN10028-6 P500Q | EN10028-6 P690Q | |
| EN10028-6 P355QH | EN10028-6 P460QH | EN10028-6 P500QH | EN10028-6 P690QH | ||
| EN10028-6 P355QL1 | EN10028-6 P460QL1 | EN10028-6 P500QL1 | EN10028-6 P690QL1 | ||
| EN10028-6 P355QL2 | EN10028-6 P460QL2 | EN10028-6 P500QL2 | EN10028-6 P690QL2 | ||
| JIS | JIS G3115 | JIS G3115 SPV235 | JIS G3115 SPV315 | JIS G3115 SPV355 | JIS G3115 SPV410 |
| JIS G3115 SPV450 | JIS G3115 SPV490 | ||||
| JIS G3103 | JIS G3103 SB410 | JIS G3103 SB450 | JIS G3103 SB480 | JIS G3103 SB450M | |
| JIS G3103 SB480M | |||||
| GB | GB713 | GB713 Q245R | GB713 Q345R | GB713 Q370R | GB713 12Cr1MoVR |
| GB713 12Cr2Mo1R | GB713 13MnNiMoR | GB713 14Cr1MoR | GB713 15CrMoR | ||
| GB713 18MnMoNbR | |||||
| GB3531 | GB3531 09MnNiDR | GB3531 15MnNiDR | GB3531 16MnDR | ||
| DIN | DIN 17155 | DIN 17155 HI | DIN 17155 HII | DIN 17155 10CrMo910 | DIN 17155 13CrMo44 |
| DIN 17155 15Mo3 | DIN 17155 17Mn4 | DIN 17155 19Mn6 | |||