EN10025-5 Evropa standarti bo'yicha S235J2W, S235J2W po'lat plitalar, S235J2W ob-havoga chidamli korroziyaga qarshi po'lat plitalar asosan korroziyaga qarshilik ko'rsatish uchun o'z mulkiga ega bo'lgan qattiq ob-havo sharoitida qo'llaniladi. Minimal oqish quvvati bilan 235 Mpa va qalinligi uchun valentlik kuchi 1500 mm dan 1016 mm gacha bo'lishi kerak.
Kimyoviy tarkibi % S235J2W navi mahsulot tahlili
|
C |
Si |
Mn |
Cu |
P |
S |
Cr |
N |
|
0.16 |
0.45 |
0.15-0.70 |
0.20-0.60 |
0.040 |
0.035 |
0.35-0.85 |
0.010 |
S235J2W sinfining mexanik xususiyatlari
|
Harorat |
-20 |
-10 |
0 |
20 |
|
Teshik ta'siri testi. Min. yutilgan energiya J |
27 |
|
Nominal qalinligi (mm) |
16 gacha |
16 - 40 |
40 - 63 |
63 - 80 |
80 - 100 |
100 - 150 |
|
ReH - Minimal oqish quvvati (MPa) |
235 |
225 |
215 |
215 |
215 |
195 |
|
Nominal qalinligi (mm) |
3 ga |
3 - 100 |
100-150 |
|
Rm -Kuchlanish kuchi (MPa) |
360-510 |
360-510 |
350-500 |
|
Nominal qalinligi (mm) |
1,5<2 dan katta yoki unga teng |
2﹤2,5 dan katta yoki unga teng |
2,5<3 dan katta yoki unga teng |
3<40 dan katta yoki unga teng |
40﹤63 dan katta yoki unga teng |
6﹤100 dan katta yoki unga teng |
100﹤150 dan katta yoki unga teng |
|
A - Minimal cho'zilish Lo=5,65 √ Shunday qilib (%) Uzunlamasına |
19 |
20 |
21 |
26 |
25 |
24 |
22 |