SA662GrC - o'rta va past haroratli bosimli idishlar uchun Amerika standarti uglerodli marganets kremniyli po'lat plitalar. U asosan past haroratli payvandlangan bosimli idishlar ishlab chiqarish uchun ishlatiladi. Payvandlangan bosimli idishlar uchun uglerod marganets silikon po'lat plitalari past haroratli tirqishning mustahkamligi uchun yuqori talablarga ega. -40 darajada foydalanish uchun past haroratli payvandlangan bosimli idishlar ishlab chiqarish uchun ishlatiladi.
SA662 po'lat kimyoviy tarkibi:
|
Tarkibi |
SA662 A darajasi |
SA662 B darajasi |
SA662 C darajasi |
SA662 C darajasi |
SA662 C darajasi |
|
|
Issiqlik |
Mahsulot |
Issiqlik |
Mahsulot |
Issiqlik |
Mahsulot |
|
|
C dan kichik yoki teng |
0.14 |
0.17 |
0.19 |
0.22 |
0.20 |
0.24 |
|
Mn |
0.90~1.35 |
0.84~1.46 |
0.85~1.50 |
0.79~1.62 |
1.00~1.60 |
0.92~1.72 |
|
P dan kichik yoki teng |
0.035 |
0.035 |
0.035 |
0.035 |
0.035 |
0.035 |
|
S dan kichik yoki teng |
0.035 |
0.035 |
0.035 |
0.035 |
0.035 |
0.035 |
|
Si |
0.15~0.40 |
0.13~0.45 |
0.15~0.40 |
0.13~0.45 |
0.15~0.50 |
0.13~0.55 |