a516gr70 ning xususiyatlari qanday?

Mar 14, 2024 Xabar QOLDIRISH

ASTM A516 70-darajali (A516GR70) xususiyatlari:

kimyoviy tarkibi:

Uglerod (C): 0.27-0,31%
Marganets (Mn): 0.79-1,3%
Fosfor (P): 0.035% maksimal
Oltingugurt (S): 0.035% maksimal
Kremniy (Si): 0.13-0,45%

China pressure vessel steel manufacturer

Mexanik xatti-harakatlar:

Kuchlanish kuchi: 485-620 MPa (70-90 ksi)
Hosildorlik kuchi: Minimal 260 MPa (38 ksi)
Uzayish: 8 dyuym uchun minimal 17%, 2 dyuym uchun minimal 21%
Zichlik: 7,85 g/sm3 (0,284 lb/kub dyuym)

Elastiklik moduli: 200 GPa (29,000 ksi)

Issiqlik o'tkazuvchanligi: 100 gradusda 52,6 Vt / m · K

Maxsus issiqlik quvvati: 470 J/kg·K

Qarshilik: 0.0000159Ō·m

China boiler plate Distributors

Qattiqlik: Odatda taxminan 187 Brinell (HB) yoki ekvivalent Rokvell qattiqligi.

 

Payvandlash qobiliyati: to'g'ri isitish va payvandlashdan keyingi issiqlik bilan ishlov berish amaliyotlari bilan yaxshi payvandlanish.

 

Korroziyaga chidamlilik: turli atmosfera sharoitida korroziyaga chidamli; muayyan muhitda mahalliy korroziyaga moyil.

 

Ta'sirga chidamlilik: xona haroratida va past haroratlarda yaxshi zarba qarshiligi.

 

Ilovalar: Odatda o'rtacha va past haroratli xizmat ko'rsatish sharoitlari mavjud bo'lgan bosimli idish va qozon ilovalarida qo'llaniladi.

 

Issiqlik bilan ishlov berish: Payvandlashdan keyin normallashtirish yoki stressni bartaraf etish ko'pincha materialning xususiyatlarini yaxshilash va qoldiq stresslarni olib tashlash uchun ishlatiladi.

China vessel plate Manufacturers