ASTM A302 materiali nimaga teng?

May 19, 2025 Xabar QOLDIRISH

ASTM A302/A302M-17(2022) PDF

 

ASTM A302 nima?

Bu spetsifikatsiya, ayniqsa, payvandlangan qozonlar va boshqa bosimli idishlar uchun moʻljallangan marganets{0}}molibden va marganets-molibden-nikel qotishma poʻlat plitalarini qamrab oladi.

ASTM A302

ASTM A302 Kimyoviy tarkibi:

ASTM A302 Kimyoviy tarkibi
Chelik darajasi Maksimal element (%)
C Si Mn P S Mo Ni
A302 A darajasi 0.20-0.25 0.13–0.45 0.87–1.41 0,035 0,035 0.41–0.64  
A302 B darajasi 0.20-0.25 0.13-0.45 1.07-1.62 0.035 0.035 0.41-0.64  
A302 C darajasi 0.20-0.25 0.13-0.45 1.07-1.62 0.035 0.035 0.41-0.64 0.37-0.73
A302 D darajasi 0.20-0.25 0.13-0.45 1.07-1.62 0.035 0.035 0.41-0.64 0.67-1.03

 

ASTM A302 mexanik xususiyatlari:

Chelik darajasi   ASTM A302 Mexanik xususiyat
Qalinligi Yo'l bering Kuchlanish Cho'zilish
A302 A darajasi mm Min Mpa Mpa Min %
6-50 310 515-655 19%
50-200 310 515-655 15%
A302 B darajasi 6-50 345 Mpa 550-690 Mpa 18%
50-200 345 Mpa 550-690 Mpa 15%
A302 C darajasi 6-50 50 [345] 80-100kis [550-690]Mpa 17%
50-200 20%

ASTM A302 materiali nimaga teng?

ASTM A302 Ekvivalent po'lat darajasi:
Chelik darajasi Yevropa Germaniya Fransiya Italiya U.K.
ASTM A302 Gr. A, B 14Cr Mo 45 13 Cr Mo 44 15 CD 4.05 14 Cr Mo 46 620 Gr.27,31

 

ASTM A302 qotishma po'lat va EN 1.4310 zanglamaydigan po'lat
ASTM A302 qotishma po'lat va EN 1.4310 zanglamaydigan po'lat ham temir qotishmalari hisoblanadi. Har ikkala material uchun qiymatlarga ega 31 ta moddiy xususiyat mavjud.

 

ASTM A302 qotishma po'lat, B darajasi
Qotishma po'lat, B daraja, Mn-Mo-Qozon va boshqa bosimli idishlar uchun Ni qotishma po'lat plitalar.