ASTM A612 spetsifikatsiyasi o'rtacha va past haroratli xizmat ko'rsatish uchun bosimli idish plitalari, uglerodli po'lat, yuqori quvvat uchun standart spetsifikatsiyadir.

ASTM A612 o'rtacha va past haroratli xizmat ko'rsatish uchun payvandlangan bosimli idishlarda foydalanish uchun mo'ljallangan uglerod-marganets-silikon po'lat plitalarini o'z ichiga oladi.

 

ASTM A612M kimyoviy tarkibi qanday?

MATERIAL C Mn Si P dan kichik yoki teng S dan kichik yoki teng
ASTM A612M 0.29 0.13-0.55 0.92-1.72 0.035 0.035

 

ASTM A612M ning kuchlanishi nima?

MATERIAL Kuchlanish kuchi (MPa) Oqim kuchi (MPa) MIN % cho‘zilish MIN
ASTM A612M 560-725 345 16

 

ASTM A612 po'lati nimaga teng?

ASTM A612 ASME SA-516 Gr.70‌,‌EN 10028-3 P355N‌, Q345R ga ekvivalentdir