EN10028-6 P690QL1bosimli uskunalar va qozonlarda ishlatiladigan yuqori-kuchli, so‘ndirilgan va qattiqlashtirilgan, payvandlanadigan nozik taneli po‘lat plastinka. "P690" 690 ga teng bo'lgan minimal rentabellikni bildiradiMPa, "QL1" esa uning belgilangan qattiqligiga ega ekanligini bildiradi27J past haroratda−40daraja. U asosan neft-kimyo, kimyoviy qayta ishlash va elektr energiyasini ishlab chiqarish kabi yuqori quvvat va chidamlilik talab qilinadigan sohalarda qo'llaniladi, deya qayd etadi GNEE Steel.
Qalinligi: 6MM dan 300MM gacha,
Kengligi: 1500 mm dan 4050 mm gacha,
Uzunligi: 3000 mm dan 15000 mm gacha
EN10028-6 P690QL1 bosimli idish va qozon po'lat plitalari kimyoviy tarkibi va mexanik xususiyatlari
|
P690QL1 Kimyoviy tarkibi |
|||||||
|
Baho |
Maksimal element (%) |
||||||
|
C |
Si |
Mn |
P |
S |
N |
B |
|
|
P690QL1 |
0.20 |
0.80 |
1.70 |
0.020 |
0.010 |
0.015 |
0.005 |
|
Mo |
Cu |
Nb |
Ni |
Ti |
V |
Cr |
|
|
0.70 |
0.3 |
0.06 |
2.50 |
0.05 |
0.12 |
1.50 |
|
|
Baho |
P690QL1 Mexanik xususiyat |
|||
|
Qalinligi |
Yo'l bering |
Kuchlanish |
Cho'zilish |
|
|
P690QL1 |
mm |
Min Mpa |
Mpa |
Min % |
|
6-50 |
690 |
770-940 |
14% |
|
|
50-100 |
670 |
770-940 |
14% |
|
|
100-150 |
630 |
720-900 |
14% |
|
EN10028-6 P690QL1 bosimli idish va qozon uchun po'lat plitalar ilovasi
Kimyoviy reaktsiya idishlari
EN10028-6 P690QL1 qozon va bosimli idish po'lat plitasi sintez reaktsiyalarida (masalan, o'g'it zavodlarida ammiak sintez minoralari va kimyoviy zavodlarda polimerizatsiya reaktorlari) ishlatiladi. U yuqori harorat va bosimlarga (masalan, ammiak sintezi minorasi 30MPa bosim va 450 daraja haroratda ishlaydi) va o'rta korroziyaga (masalan, vodorod va kislota gazlari) qarshilik ko'rsatishi kerak, buning natijasida hech qanday oqish yoki struktura buzilishi sodir bo'lmaydi.
Neft-kimyo saqlash tanklari va minoralari
EN10028-6 P690QL1 Past haroratli bosimli idish po'lat plitasi xom neft, suyultirilgan gaz (LNG) va suyultirilgan neft gazini (LPG) saqlash tanklarida, shuningdek, neftni qayta ishlashda rektifikatsion minoralar va assimilyatsiya minoralarida (neftni qayta ishlash tanklari: normal harorat va bosim kabi) ishlatiladi; past -haroratli saqlash idishlari (masalan, -162 daraja past haroratli LNG saqlash tanklari) past haroratlarda po‘latning mo‘rt sinishiga yo‘l qo‘ymaslik uchun past haroratda mukammal mustahkamlikka ega po‘lat plitalarni talab qiladi; yuqori bosimli gidrogenatsiya minoralari (neft-kimyoni gidrotozalash jarayoni).
Issiqlik almashinuvi idishlari
EN10028-6 P690QL1 Yuqori-sifatli qozon po'lat plitasi o'rta issiqlik almashinuvi uchun uskunalarda (masalan, qobiqli va quvurli issiqlik almashtirgichlar va plastinka issiqlik almashinuvchilari) ishlatiladi. Ularning chig'anoqlari va quvurlari varaqlari o'zgaruvchan issiq va sovuq zarbalarga bardosh berishi, charchoqqa chidamliligini ta'minlashi va tez-tez harorat o'zgarishi natijasida payvand choki yorilishiga yo'l qo'ymaslik kerak.
Metallurgiya sanoati
Po'lat zavodlarida (0,5-1,5 MPa bosim va 1200 daraja haroratda) yuqori haroratli issiq havoni saqlaydigan "domna pechkasi" yuqori haroratga chidamli EN10028-6 P690QL1 plitasi; rangli metallarni eritishda "avtoklav" (masalan, gidrometallurgik mis eritishda yuvish avtoklav) kislotali korroziyaga chidamli bo'lishi kerak va EN10028-6 P690QL1 bosimli idish po'lat plitasi odatda qo'llaniladi.
EN10028-6 P690QL1 bosimli idish va qozon po'lat plitasi Boshqa nom
EN10028-6 P690QL1 Qozon po'lat plitasi|EN10028-6 P690QL1 Bosimli idish po'lat plita |EN10028-6 P690QL1 Saqlash tanklari Chelik plastinka|EN10028-6 P690QL1 Issiqlik almashtirgich po'lat plitalar.
Qo'shimcha shart
UT (Ultratovush tekshiruvi), AR (Faqat issiq haddelenmiş holda), TMCP (Termal mexanik nazoratni qayta ishlash), N (Normallashtirilgan), Q+T (O'chirilgan va Temperlangan), Z yo'nalishi testi (Z15, Z25, Z35), Charpy V-Notch ta'siri testi, Uchinchi tomon SG testi va sinovlari (shu kabilar),
Bepul namuna olish uchun bosing
Agar siz GNEE mahsulotlari haqida ko'proq bilmoqchi bo'lsangiz, elektron pochta manziliga xat yuborishingiz mumkinalloy@gneesteelgroup.com.Biz sizga yordam berishdan xursandmiz.
| GNEE tomonidan ta'minlangan bosimli idish plitalarining darajalari | |||||
| ASTM | ASTM A202/A202M | ASTM A202 A darajasi | ASTM A202 B darajasi | ||
| ASTM A203/A203M | ASTM A203 A darajasi | ASTM A203 B darajasi | ASTM A203 D darajasi | ASTM A203 E darajasi | |
| ASTM A203 F darajasi | |||||
| ASTM A204/A204M | ASTM A204 A darajasi | ASTM A204 B darajasi | ASTM A204 C darajasi | ||
| ASTM A285/A285M | ASTM A285 A darajasi | ASTM A285 B darajasi | ASTM A285 C darajasi | ||
| ASTM A299/A299M | ASTM A299 A darajasi | ASTM A299 B darajasi | |||
| ASTM A302/A302M | ASTM A302 A darajasi | ASTM A302 B darajasi | ASTM A302 C darajasi | ASTM A302 D darajasi | |
| ASTM A387/A387M | ASTM A387 5-sinf 1-sinf | ASTM A387 5-sinf 2-sinf | ASTM A387 11-sinf 1-sinf | ASTM A387 11-sinf 2-sinf | |
| ASTM A387 12-sinf 1-sinf | ASTM A387 12-sinf 2-sinf | ASTM A387 22-sinf 1-sinf | ASTM A387 22-sinf 2-sinf | ||
| ASTM A515/A515M | ASTM A515 60-sinf | ASTM A515 65-sinf | ASTM A515 70-sinf | ||
| ASTM A516/A516M | ASTM A516 55-sinf | ASTM A516 60-sinf | ASTM A516 65-sinf | ASTM A516 70-sinf | |
| ASTM A517/A517M | ASTM A517 A darajasi | ASTM A517 B darajasi | ASTM A517 E darajasi | ASTM A517 F darajasi | |
| ASTM A517 P darajasi | ASTM A517 J darajasi | ||||
| ASTM A533/A533M | ASTM A533 A sinfi 1 | ASTM A533 B sinfi 1 | ASTM A533 C sinf 1 | ASTM A533 D sinfi 1 | |
| ASTM A533 A sinfi 2 | ASTM A533 B sinfi 2 | ASTM A533 C sinfi 2 | ASTM A533 D sinfi 2 | ||
| ASTM A533 A sinfi 3 | ASTM A533 B sinfi 3 | ASTM A533 C sinfi 3 | ASTM A533 D sinfi 3 | ||
| ASTM A537/A537M | ASTM A537 1-sinf | ASTM A537 2-sinf | ASTM A537 sinf 3 | ||
| ASTM A612/A612M | ASTM A612 | ||||
| ASTM A662/A662M | ASTM A662 A darajasi | ASTM A662 B darajasi | ASTM A662 C darajasi | ||
| UZ | EN10028-2 | EN10028-2 P235GH | EN10028-2 P265GH | EN10028-2 P295GH | EN10028-2 P355GH |
| UZ10028-2 16MO3 | |||||
| EN10028-3 | EN10028-3 P275N | EN10028-3 P275NH | EN10028-3 P275NL1 | EN10028-3 P275NL2 | |
| EN10028-3 P355N | EN10028-3 P355NH | EN10028-3 P355NL1 | EN10028-3 P355NL2 | ||
| EN10028-3 P460N | EN10028-3 P460NH | EN10028-3 P460NL1 | EN10028-3 P460NL2 | ||
| EN10028-5 | EN10028-5 P355M | EN10028-5 P355ML1 | EN10028-5 P355ML2 | EN10028-5 P420M | |
| EN10028-5 P420ML1 | EN10028-5 P420ML2 | EN10028-5 P460M | EN10028-5 P460ML1 | ||
| EN10028-5 P460ML2 | |||||
| EN10028-6 | EN10028-6 P355Q | EN10028-6 P460Q | EN10028-6 P500Q | EN10028-6 P690Q | |
| EN10028-6 P355QH | EN10028-6 P460QH | EN10028-6 P500QH | EN10028-6 P690QH | ||
| EN10028-6 P355QL1 | EN10028-6 P460QL1 | EN10028-6 P500QL1 | EN10028-6 P690QL1 | ||
| EN10028-6 P355QL2 | EN10028-6 P460QL2 | EN10028-6 P500QL2 | EN10028-6 P690QL2 | ||
| JIS | JIS G3115 | JIS G3115 SPV235 | JIS G3115 SPV315 | JIS G3115 SPV355 | JIS G3115 SPV410 |
| JIS G3115 SPV450 | JIS G3115 SPV490 | ||||
| JIS G3103 | JIS G3103 SB410 | JIS G3103 SB450 | JIS G3103 SB480 | JIS G3103 SB450M | |
| JIS G3103 SB480M | |||||
| GB | GB713 | GB713 Q245R | GB713 Q345R | GB713 Q370R | GB713 12Cr1MoVR |
| GB713 12Cr2Mo1R | GB713 13MnNiMoR | GB713 14Cr1MoR | GB713 15CrMoR | ||
| GB713 18MnMoNbR | |||||
| GB3531 | GB3531 09MnNiDR | GB3531 15MnNiDR | GB3531 16MnDR | ||
| DIN | DIN 17155 | DIN 17155 HI | DIN 17155 HII | DIN 17155 10CrMo910 | DIN 17155 13CrMo44 |
| DIN 17155 15Mo3 | DIN 17155 17Mn4 | DIN 17155 19Mn6 | |||