SA 387 Gr 12 plastinka nima?
TheSA 387 12-darajali plastinka kimyoviy tarkibi tufayli yuqori haroratli xizmatlarda foydalanish uchun mo'ljallangan. Bu payvandlanadigan bosimli idishlarda keng qo'llaniladigan xrom{1}}molli uglerodli qotishma po'latdir. ning yaxshi ishlashiSA 387 Gr 12 plastinkayuqori haroratda ularni sanoat qozonlari uchun mukammal qiladi. Kimyoviy tarkibidagi xrom korroziyaga va oksidlanishga chidamliligini oshirishga yordam beradi. Ushbu xususiyatlarning barchasi tufayli material sanoatning keng doiralarida nordon xizmat ko'rsatish uchun idealdir.

Sa 387 Gr 12 ning ekvivalent materiallari nima?
Sa 387 Gr 12 ning ekvivalent materiallari BS 620B, UNS K11757, A387 / SA 387, DIN 13 CRMO 44 va EN 3 CRMO 45 hisoblanadi.
SA 387 Gr 12 Plitaning Materiallar spetsifikatsiyasi
Darajasi:ASME SA 387 12-darajali qotishma po'lat plitalar
Ta'sir sinovi:-52 daraja
Jarayon:Issiq-Qayta (HR)
Kengligi:1000 dan 4500 mm gacha
Qalinligi:5 dan 150 mm gacha
Uzunlik:3000 dan 18000 mm gacha
ASTM SA387 12-darajali plastinkaning kimyoviy xossalari
| Baho | Cr | Mn | C | S | P | Si | Mo |
| SA 387 Gr.12 | 0.50-0.80 | 0.55-0.80 | 0.05-0.17 | 0.025 | 0.025 | 0.15-0.40 | 0.45-0.60 |
ASME SA387 12-sinf plastinkasining mexanik xususiyatlari
| Sinf | Uzoq. (50 mm) | Hosildorlik (MPa) | Uzoq. (200 mm) | Kuchlanish (MPa) | Hududning qisqarishi* |
| 2-sinf | 22% min | 275 min | 19% min | 450 - 585 | - |
| 1-sinf | 22% min | 230 min | 18% min | 380 - 550 | - |
Nima uchun SA 387 Gr 12 va ekvivalentlari uchun GNEE Steelni tanlaysiz
Professional bosimli idish po'lat plitalar yetkazib beruvchi sifatida,GNEE po'lattaklif qiladi:
SA 387 Gr 12 va unga tenglashtirilgan navlar (13CrMo4-5, 12CrMo)
Plitalar qalinligi diapazoni:6 mm - 150 mm
Normallashtirilgan va temperli ta'minot holati
EN 10204 3.1 / 3.2 Mill sinov sertifikatlari
Uchinchi tomon tekshiruvi-(SGS, BV, TUV)
Ekvivalentlik va material tanlash uchun texnik yordam
Xulosa
SA 387 12-sinfyuqori haroratli bosimli idishlar uchun koʻp qirrali va ishonchli Cr-Mo qotishma poʻlatdir. Uning eng taniqli ekvivalentlari o'z ichiga oladiEN 13CrMo4-5 (1.7335)vaGB 12CrMo, turli standartlar ostida o'xshash tarkib va ishlashni taklif qiladi.
📩 Bugun GNEE Steel bilan bog'laningekspert maslahati, raqobatbardosh narxlar va global loyihalaringiz uchun SA 387 Gr 12 va shunga o'xshash bosimli idish po'lat plitalarini ishonchli yetkazib berish uchun.
SA 387 GR 12 qanday material?
SA387 GR 12 SINF 2
Yuqori haroratli xizmatda foydalanish uchun ishlab chiqilgan ASME SA387 12-sinf axrom-molibden karbonli qotishma po'latpayvandlanadigan bosimli idishlar va sanoat qozonlarda foydalanish uchun.
ASTM A387 Grade 22 nimaga teng?
ASTM A387 22-darajali ekvivalent po'lat navlari orasida,SA387 22-sinf, 10CrMo9-10boshqa ekvivalentlarga qaraganda mashhurroq. SA387 22-darajali po'lat ASME SA387/SA387M standarti ostida. SA387 22-darajali po'latning kimyoviy ko'rsatkichlari va texnik talablari ASTM A387 22-darajali po'lat bilan deyarli bir xil.
SA 387 11-sinf 2-sinf nimaga teng?
Sa 387 Gr 11 Ekvivalent material hisoblanadiASME SA387AQSh bozorlarida Yevropa Ittifoqi bilan 13CrMoSi5-5 sinfidagi modullarga ega. Sa 387 Gr 11 Cl 2 ekvivalent materiali ASME va ASTM standartining SA387-11-2 hisoblanadi.
Mahsulotlarni ko'rsatish



Qadoqlash va jo'natish


Ko'rgazmalar va mijozlar tashriflari

GNEE Steel shuningdek, A204 sinfi B, A515 sinf 70, A537 sinf 1, SA387 sinf 11 sinf, P265GH, S537 sinf 2, P355Q, P275N, P395Q va boshqalar kabi turli xil qozon va bosimli idish po'lat plitalarini etkazib beradi. po‘lat plitalarning boshqa turlari haqida ko‘proq ma’lumot olish uchun +8615824687445 bo‘yicha maslahat telefoniga qo‘ng‘iroq qilishingiz yoki alloy@gneesteelgroup.com manziliga xat yuborishingiz mumkin. Biz bilan maslahatlashishga xush kelibsiz va biz sizning savollaringizga javob berishga tayyormiz.
| GNEE tomonidan ta'minlangan bosimli idish plitalarining darajalari | |||||
| ASTM | ASTM A202/A202M | ASTM A202 A darajasi | ASTM A202 B darajasi | ||
| ASTM A203/A203M | ASTM A203 A darajasi | ASTM A203 B darajasi | ASTM A203 D darajasi | ASTM A203 E darajasi | |
| ASTM A203 F darajasi | |||||
| ASTM A204/A204M | ASTM A204 A darajasi | ASTM A204 B darajasi | ASTM A204 C darajasi | ||
| ASTM A285/A285M | ASTM A285 A darajasi | ASTM A285 B darajasi | ASTM A285 C darajasi | ||
| ASTM A299/A299M | ASTM A299 A darajasi | ASTM A299 B darajasi | |||
| ASTM A302/A302M | ASTM A302 A darajasi | ASTM A302 B darajasi | ASTM A302 C darajasi | ASTM A302 D darajasi | |
| ASTM A387/A387M | ASTM A387 5-sinf 1-sinf | ASTM A387 5-sinf 2-sinf | ASTM A387 11-sinf 1-sinf | ASTM A387 11-sinf 2-sinf | |
| ASTM A387 12-sinf 1-sinf | ASTM A387 12-sinf 2-sinf | ASTM A387 22-sinf 1-sinf | ASTM A387 22-sinf 2-sinf | ||
| ASTM A515/A515M | ASTM A515 60-sinf | ASTM A515 65-sinf | ASTM A515 70-sinf | ||
| ASTM A516/A516M | ASTM A516 55-sinf | ASTM A516 60-sinf | ASTM A516 65-sinf | ASTM A516 70-sinf | |
| ASTM A517/A517M | ASTM A517 A darajasi | ASTM A517 B darajasi | ASTM A517 E darajasi | ASTM A517 F darajasi | |
| ASTM A517 P darajasi | ASTM A517 J darajasi | ||||
| ASTM A533/A533M | ASTM A533 A sinfi 1 | ASTM A533 B sinfi 1 | ASTM A533 C sinfi 1 | ASTM A533 D sinfi 1 | |
| ASTM A533 A sinfi 2 | ASTM A533 B sinfi 2 | ASTM A533 C sinfi 2 | ASTM A533 D sinfi 2 | ||
| ASTM A533 A sinfi 3 | ASTM A533 B sinfi 3 | ASTM A533 C sinfi 3 | ASTM A533 D sinfi 3 | ||
| ASTM A537/A537M | ASTM A537 1-sinf | ASTM A537 2-sinf | ASTM A537 sinf 3 | ||
| ASTM A612/A612M | ASTM A612 | ||||
| ASTM A662/A662M | ASTM A662 A darajasi | ASTM A662 B darajasi | ASTM A662 C darajasi | ||
| UZ | EN10028-2 | EN10028-2 P235GH | EN10028-2 P265GH | EN10028-2 P295GH | EN10028-2 P355GH |
| UZ10028-2 16MO3 | |||||
| EN10028-3 | EN10028-3 P275N | EN10028-3 P275NH | EN10028-3 P275NL1 | EN10028-3 P275NL2 | |
| EN10028-3 P355N | EN10028-3 P355NH | EN10028-3 P355NL1 | EN10028-3 P355NL2 | ||
| EN10028-3 P460N | EN10028-3 P460NH | EN10028-3 P460NL1 | EN10028-3 P460NL2 | ||
| EN10028-5 | EN10028-5 P355M | EN10028-5 P355ML1 | EN10028-5 P355ML2 | EN10028-5 P420M | |
| EN10028-5 P420ML1 | EN10028-5 P420ML2 | EN10028-5 P460M | EN10028-5 P460ML1 | ||
| EN10028-5 P460ML2 | |||||
| EN10028-6 | EN10028-6 P355Q | EN10028-6 P460Q | EN10028-6 P500Q | EN10028-6 P690Q | |
| EN10028-6 P355QH | EN10028-6 P460QH | EN10028-6 P500QH | EN10028-6 P690QH | ||
| EN10028-6 P355QL1 | EN10028-6 P460QL1 | EN10028-6 P500QL1 | EN10028-6 P690QL1 | ||
| EN10028-6 P355QL2 | EN10028-6 P460QL2 | EN10028-6 P500QL2 | EN10028-6 P690QL2 | ||
| JIS | JIS G3115 | JIS G3115 SPV235 | JIS G3115 SPV315 | JIS G3115 SPV355 | JIS G3115 SPV410 |
| JIS G3115 SPV450 | JIS G3115 SPV490 | ||||
| JIS G3103 | JIS G3103 SB410 | JIS G3103 SB450 | JIS G3103 SB480 | JIS G3103 SB450M | |
| JIS G3103 SB480M | |||||
| GB | GB713 | GB713 Q245R | GB713 Q345R | GB713 Q370R | GB713 12Cr1MoVR |
| GB713 12Cr2Mo1R | GB713 13MnNiMoR | GB713 14Cr1MoR | GB713 15CrMoR | ||
| GB713 18MnMoNbR | |||||
| GB3531 | GB3531 09MnNiDR | GB3531 15MnNiDR | GB3531 16MnDR | ||
| DIN | DIN 17155 | DIN 17155 HI | DIN 17155 HII | DIN 17155 10CrMo910 | DIN 17155 13CrMo44 |
| DIN 17155 15Mo3 | DIN 17155 17Mn4 | DIN 17155 19Mn6 | |||