GNEE po'latdan issiq sotish EN 10149-2 S700MC po'lat zahiralari Xitoyda, Xitoyda po'lat yetkazib beruvchi sifatida, eng yaxshi narx va yuqori sifat. EN 10149-2S700MC po'latavtomobil nurlari uchun nur qismlari uchun mos bo'lgan yuqori quvvat va yaxshi bükme ko'rsatkichlariga ega.
S700MC - EN10149: Part2 spetsifikatsiyasi bo'yicha etkazib beriladigan yuqori rentabellikdagi strukturaviy po'latdir. Materiallarning yuqori rentabelligi (700Mpa min.) tufayli u turli xil yuk ko'taruvchi ilovalarda ishlatilishi mumkin.
Ommabop ravishda, po'lat sovuq shakllangan komponentlar, shu jumladan sovuq presslangan qismlar va qismlar uchun ishlatiladi. Odatda qo'llanilishi po'lat ramkalar, yuk ko'taruvchi nurlar va quvurlarni o'z ichiga oladi.
S700MC mukammal bükme va katlama xususiyatlarini taklif qiladi, ammo po'lat ish uchun to'g'ri spetsifikatsiyaga ega bo'lishini ta'minlash uchun alohida e'tibor berilishi kerak.
EN 10149-2 S700MC po'lat Kimyoviy tarkibi %
| Baho | C | Si | Mn | p | S | Al | Nb | V | Ti | Mo |
| S700MC | 0,10 dan kam yoki unga teng | 0..50 dan kam yoki unga teng | 2.10 dan kam yoki unga teng | 0,025 dan kam yoki unga teng | 0,010 dan kam yoki unga teng | 0.015 | 0,09 dan kam yoki unga teng | 0,20 dan kam yoki unga teng | 0,15 dan kam yoki unga teng | 0,50 dan kam yoki unga teng |
EN 10149-2 S700MC po'lat Mexanik xususiyatlari
| Baho | Hosildorlik kuchi (MPa) |
Mustahkamlik chegarasi (MPa) |
Uzayish (%) | 180 daraja sovuq egilish, diametri | |
| Qalinligi ~ 3 mm Past=80mm, b=20mm |
Qalinligi 3 mm L0=5.65 √ S0 |
||||
| S700MC | 750 | 800-950 | 10 | 12 | 2.0a |
EN 10149-2 S700MC po'lat ekvivalent darajasi
EN 10149-2 S700MC po'lat plitalar / varaq EN 10149-2 standartida, material raqami 1,8969. Xuddi shu standart ostidagi po'lat navlariS315MC, S355MC, S420MC, S460MC, S500MC, S550MC, S600MC, S650MC. S700MC po'latining ekvivalent navlari SEW092 QStE 690TM, NFA36-231 E690D, ASTM A514, BS1449 75F70.
S700mc Chelik Ekvivalenti Astm
| Germaniya DIN, WNr |
EI UZ |
Angliya BS |
AQSh - |
Fransiya AFNOR |
|||||
|
S700MC |
|
|
|
EN 10149-2 Raqam: 1.8974 S700MC |
baholar Taqqoslash | |
| ASTM | A514 | |
| NFA36-231 | E690D | |
| SEW092 | QStE 690TM | |
| UNI8890 | - | |
| BS1449 | 75F70 | |
GNEE po'lati Sizga yuqori{0}}sifatli mahsulotlar va sotuvdan keyingi-xizmatni eng past narx bilan qaytaradi. GNEE po'lati sifat, narx va yetkazib berish bo'yicha mijozlar kutganidan oshib ketishga intiladi. GNEE po'lati siz bilan o'zaro manfaat, o'zaro manfaatlilik va umumiy rivojlanish asosida-uzoq muddatli hamkorlik munosabatlarini o'rnatishga chin dildan umid qiladi. Agar sizda EN 10149-2 S700MC po'lat zaxirasiga oid savollaringiz bo'lsa, iltimos, GNEE po'latiga murojaat qiling yoki ko'proq GNEE po'lati uchun asosiy EN 10149-2 S700MC po'latdan tayyorlangan mahsulotlar sahifamizga tashrif buyuring.
Agar siz GNEE mahsulotlari haqida ko'proq bilmoqchi bo'lsangiz, elektron pochta manziliga xat yuborishingiz mumkinalloy@gneesteelgroup.com. Biz sizga yordam berishdan xursandmiz.
S700mc po'lat navi nima?
S700mc astandart yuqori rentabellikdagi strukturaviy sinf. S700mc kimyoviy tarkibi 0,12% uglerod, 0,60% kremniy, 2,10% marganets, 0,15% molibden, 0,025% fosfor, 0,015% oltingugurt va alyuminiydan iborat. Shuningdek, u 0,09% niobiy, 0,20% vanadiy, 0,225% titan va 0,005% borning kichik konsentratsiyasiga ega.
S700mc po'latining ekvivalenti nima?
S700MC po'latining ekvivalent navlari SEW092 QStE 690TM, NFA36-231 E690D, ASTM A514, BS{6}}F70. BBN po'lat Sizni yuqori-sifatli mahsulotlar va eng past narxda to'liq sotuvdan keyingi xizmat bilan qaytaradi.
S700mc va S690ql o'rtasidagi farq nima?
S700MC Steel asosan yuqori rentabellikni talab qiladigan ilovalar uchun ishlab chiqilgan strukturaviy po'lat plitalardir. Ular bir nechta yuk ko'taruvchi ilovalar uchun ishlatiladi. S690ql past qotishma konstruktiv po'latdir, u yuqori quvvatga ega va yaxshi payvandlanishi mumkin.
| GNEE tomonidan ta'minlangan uglerod va past{0}}qotishma yuqori-po'latlar navlari | |||||
| ASTM/ASME | ASTM A36/A36M | ASTM A36 | |||
| ASTM A283/A283M | ASTM A283 A darajasi | ASTM A283 B darajasi | ASTM A283 C darajasi | ASTM A283 D darajasi | |
| ASTM A514/A514M | ASTM A514 A darajasi | ASTM A514 B darajasi | ASTM A514 C darajasi | ASTM A514 E darajasi | |
| ASTM A514 F darajasi | ASTM A514 H darajasi | ASTM A514 J darajasi | ASTM A514 K darajasi | ||
| ASTM A514 M darajasi | ASTM A514 P darajasi | ASTM A514 Q darajasi | ASTM A514 R darajasi | ||
| ASTM A514 S darajasi | ASTM A514 T darajasi | ||||
| ASTM A572/A572M | ASTM A572 42-sinf | ASTM A572 50-darajali | ASTM A572 55-sinf | ASTM A572 60-sinf | |
| ASTM A572 65-sinf | |||||
| ASTM A573/A573M | ASTM A573 58-sinf | ASTM A573 65-sinf | ASTM A573 70-sinf | ||
| ASTM A588/A588M | ASTM A588 A darajasi | ASTM A588 B darajasi | ASTM A588 C darajasi | ASTM A588 K darajasi | |
| ASTM A633/A633M | ASTM A633 A darajasi | ASTM A633 C darajasi | ASTM A633 D darajasi | ASTM A633 E darajasi | |
| ASTM A656/A656M | ASTM A656 50-darajali | ASTM A656 60-sinf | ASTM A656 70-sinf | ASTM A656 80-sinf | |
| ASTM A709/A709M | ASTM A709 36-sinf | ASTM A709 50-darajali | ASTM A709 50S darajasi | ASTM A709 darajasi 50 Vt | |
| ASTM A709 darajasi HPS 50W | ASTM A709 darajasi HPS 70W | ASTM A709 100-darajali | ASTM A709 darajasi 100 Vt | ||
| ASTM A709 darajasi HPS 100W | |||||
| ASME SA36/SA36M | ASME SA36 | ||||
| ASME SA283/SA283M | ASME SA283 A darajasi | ASME SA283 B darajasi | ASME SA283 C darajasi | ASME SA283 D darajasi | |
| ASME SA514/SA514M | ASME SA514 A darajasi | ASME SA514 B darajasi | ASME SA514 C darajasi | ASME SA514 E darajasi | |
| ASME SA514 F darajasi | ASME SA514 H darajasi | ASME SA514 J darajasi | ASME SA514 K darajasi | ||
| ASME SA514 M darajasi | ASME SA514 P darajasi | ASME SA514 Q darajasi | ASME SA514 R darajasi | ||
| ASME SA514 S darajasi | ASME SA514 T darajasi | ||||
| ASME SA572/SA572M | ASME SA572 42-sinf | ASME SA572 50-sinf | ASME SA572 55-sinf | ASME SA572 60-sinf | |
| ASME SA572 65-sinf | |||||
| ASME SA573/SA573M | ASME SA573 58-sinf | ASME SA573 65-sinf | ASME SA573 70-sinf | ||
| ASME SA588/SA588M | ASME SA588 A darajasi | ASME SA588 B darajasi | ASME SA588 C darajasi | ASME SA588 K darajasi | |
| ASME SA633/SA633M | ASME SA633 A darajasi | ASME SA633 C darajasi | ASME SA633 D darajasi | ASME SA633 E darajasi | |
| ASME SA656/SA656M | ASME SA656 50-sinf | ASME SA656 60-sinf | ASME SA656 70-sinf | ASME SA656 80-sinf | |
| ASME SA709/SA709M | ASME SA709 36-sinf | ASME SA709 50-sinf | ASME SA709 50S darajasi | ASME SA709 darajasi 50W | |
| ASME SA709 darajasi HPS 50W | ASME SA709 darajasi HPS 70W | ASME SA709 100-sinf | ASME SA709 darajasi 100 Vt | ||
| ASME SA709 darajasi HPS 100W | |||||
| EN10025 | EN10025-2 | EN10025-2 S235J0 | EN10025-2 S275J0 | EN10025-2 S355J0 | EN10025-2 S355K2 |
| EN10025-2 S235JR | EN10025-2 S275JR | EN10025-2 S355JR | EN10025-2 S420J0 | ||
| EN10025-2 S235J2 | EN10025-2 S275J2 | EN10025-2 S355J2 | |||
| EN10025-3 | EN10025-3 S275N | EN10025-3 S355N | EN10025-3 S420N | EN10025-3 S460N | |
| EN10025-3 S275NL | EN10025-3 S355NL | EN10025-3 S420NL | EN10025-3 S460NL | ||
| EN10025-4 | EN10025-4 S275M | EN10025-4 S355M | EN10025-4 S420M | EN10025-4 S460M | |
| EN10025-4 S275ML | EN10025-4 S355ML | EN10025-4 S420ML | EN10025-4 S460ML | ||
| EN10025-6 | EN10025-6 S460Q | EN10025-6 S460QL | EN10025-6 S460QL1 | EN10025-6 S500Q | |
| EN10025-6 S500QL | EN10025-6 S500QL1 | EN10025-6 S550Q | EN10025-6 S550QL | ||
| EN10025-6 S550QL1 | EN10025-6 S620Q | EN10025-6 S620QL | EN10025-6 S620QL1 | ||
| EN10025-6 S690Q | EN10025-6 S690QL | EN10025-6 S690Q1 | EN10025-6 S890Q | ||
| EN10025-6 S890QL | EN10025-6 S890QL1 | EN10025-6 S960Q | EN10025-6 S960QL | ||
| JIS | JIS G3101 | JIS G3101 SS330 | JIS G3101 SS400 | JIS G3101 SS490 | JIS G3101 SS540 |
| JIS G3106 | JIS G3106 SM400A | JIS G3106 SM400B | JIS G3106 SM400C | JIS G3106 SM490A | |
| JIS G3106 SM490YA | JIS G3106 SM490B | JIS G3106 SM490YB | JIS G3106 SM490C | ||
| JIS G3106 SM520B | JIS G3106 SM520C | JIS G3106 SM570 | |||
| DIN | DIN 17100 | DIN17100 St52-3 | DIN17100 St37-2 | DIN17100 St37-3 | DIN17100 RSt37-2 |
| DIN17100 USt37-2 | |||||
| DIN 17102 | DIN17102 StE315 | DIN17102 ESTE315 | DIN17102 TStE315 | DIN17102 WStE315 | |
| DIN17102 StE355 | DIN17102 ESTE355 | DIN17102 TStE355 | DIN17102 WStE355 | ||
| DIN17102 StE380 | DIN17102 ESTE380 | DIN17102 TStE380 | DIN17102 WStE380 | ||
| DIN17102 StE420 | DIN17102 ESTE420 | DIN17102 TStE420 | DIN17102 WStE420 | ||
| DIN17102 StE460 | DIN17102 ESTE460 | DIN17102 TStE460 | DIN17102 WStE460 | ||
| DIN17102 StE500 | DIN17102 ESTE500 | DIN17102 TStE500 | DIN17102 WStE500 | ||
| DIN17102 ESTE285 | |||||
| GB | GB/T700 | GB/T700 Q235A | GB/T700 Q235B | GB/T700 Q235C | GB/T700 Q235D |
| GB/T700 Q275 | |||||
| GB/T1591 | GB/T1591 Q345A | GB/T1591 Q390A | GB/T1591 Q420A | GB/T1591 Q420E | |
| GB/T1591 Q345B | GB/T1591 Q390B | GB/T1591 Q420B | GB/T1591 Q460C | ||
| GB/T1591 Q345C | GB/T1591 Q390C | GB/T1591 Q420C | GB/T1591 Q460D | ||
| GB/T1591 Q345D | GB/T1591 Q390D | GB/T1591 Q420D | GB/T1591 Q460E | ||
| GB/T1591 Q345E | GB/T1591 Q390E | ||||
| GB/T16270 | GB/T16270 Q550C | GB/T16270 Q550D | GB/T16270 Q550E | GB/T16270 Q550F | |
| GB/T16270 Q620C | GB/T16270 Q620D | GB/T16270 Q620E | GB/T16270 Q620F | ||
| GB/T16270 Q690C | GB/T16270 Q690D | GB/T16270 Q690E | GB/T16270 Q690F | ||
| GB/T16270 Q800C | GB/T16270 Q800D | GB/T16270 Q800E | GB/T16270 Q800F | ||
| GB/T16270 Q890C | GB/T16270 Q890D | GB/T16270 Q890E | GB/T16270 Q890F | ||
| GB/T16270 Q960C | GB/T16270 Q960D | GB/T16270 Q960E | GB/T16270 Q960F | ||
| GB/T16270 Q500 | |||||