12MnNiVR qozonli po'lat plitalar

Mar 26, 2024 Xabar QOLDIRISH

12MnNiVR - bosimli idishlar uchun po'lat plastinka. JIS G3115 yapon standartidagi SPV490Q yoriq sezuvchanlik koeffitsienti Pcm bilan solishtirganda, u pastroq va po'lat plitalar payvandlash uchun qulayroqdir. Ta'sir sinovining namuna olish yo'nalishi bo'ylamadan ko'ndalangga o'zgartiriladi va zarba harorati -10 darajadan - 15 darajaga yoki undan pastroqqa o'zgartiriladi va zarba kuchi yaxshilanadi. 12MnNiVR yirik neft saqlash tanklarini ishlab chiqarishda qo'llaniladi.

 

12MnNiVR bosimli idish po'lat plastinka Kimyoviy tarkibi:

C Si Mn P S Ni Cr Mo V PCmMaks
0 dan kichik yoki unga teng.15 0.15~0.4 1.2~1.6 0 dan kichik yoki unga teng.025 0.010 dan kichik yoki unga teng 0.15~0.4 0 dan kichik yoki unga teng.3 0 dan kichik yoki unga teng.3 0.02~0.06 0 dan kichik yoki unga teng.26

 