A203 F darajali bosimli idish plitasi

Apr 10, 2024 Xabar QOLDIRISH

ASTM A203 F darajasi - ASTM A203 po'latining bir turi. Ko'rsatilgan xususiyatlar normallashtirilgan holatga mos keladi. ASTM A203 po'latining boshqa variantlari bilan solishtirganda eng yuqori quvvat va eng past egiluvchanlikka ega.
 

Kimyoviy tarkibi (%):

Darajasi / Material

Element

Tarkibi( Maks-A, min-I)

A203 darajasi F/ A203 GrF

C

A:0.20

Mn

A:0.70

Si

0.15-0.40

P

0.035

S

0.035

 

Mexanik xususiyatlar (Mpa):

Darajasi / Material

Kuchlanish sinovi

Ksi/MPa

A203 darajasi F/ A203 GrF

Mustahkamlik chegarasi

80-100/550-690

Hosildorlik kuchi

I:55/380

Cho'zilish

I:20%

Ta'sir sinovi (agar mavjud bo'lsa)

 

 

China boiler quality plates Distributors

China pressure vessel quality steel Manufacturers

China pressure vessel steel plate Manufacturers