“Kichik{1}}to‘plamdagi sinov buyurtmasidan 50 tonna po‘lat plitalar a’lo darajada bajarildi-endi biz yana 300 tonna po‘lat plitalar qo‘shmoqdamiz.A285 C darajasi!" Yaqinda Birlashgan Arab Amirliklarining (BAA) neft-kimyo korxonasi GNEE STEEL kompaniyasiga qo'shimcha buyurtma yubordi, bu uch oy oldingi birinchi hamkorlikdan keyin ikkinchi xaridni amalga oshirdi.
Dastlabki hamkorlikka nazar tashlaydigan bo‘lsak, mijoz yangi xom neft saqlash tanki loyihasi uchun past{0}}uglerodli bosimli idish po‘lat plitalarini sotib olishi kerak edi va xalqaro platforma orqali GNEE bilan bog‘landi. Mijozning mahsulot barqarorligi haqidagi xavotirlarini inobatga olgan holda, GNEE savdo guruhi proaktiv ravishda A285 C darajali po'lat plitalari uchun batafsil texnik ma'lumotlarni taqdim etdi (ASTM A285 standartiga muvofiq, oquvchanlik kuchi 170MPa dan katta yoki unga teng, valentlik kuchi 380-7}515 megapiksel yoki yetkazib berilganda uchun mos past haroratli bosimli idishlar) va laboratoriya uchun namunalarni mexanik xususiyatni tekshirish uchun yuborish uchun tashkil etilgan.
Buyurtmachining laboratoriyasi shunday javob berdi: "Namunalar ta'sir qilish energiyasi (-20 darajada 27J dan katta yoki unga teng) va payvandlash ko'rsatkichlari saqlash tanklarini ishlab chiqarish talablariga to'liq javob beradi va GNEE texnik jamoasi butun jarayon davomida payvandlash jarayonlari haqidagi savollarga favqulodda mas'uliyat bilan javob berdi." Keyinchalik, 50 tonnalik sinov buyurtmasi (xususiyatlar: 8-16 mm × 1800-2500 mm × 8000 mm) SGS sinovidan o'tgandan so'ng yetkazib berildi. Xaridor po'lat plitalarning o'lchov aniqligini (og'ish ± 0,5 mm dan kam yoki unga teng) va sirt sifatini yuqori darajada tan oldi.
300 tonna qo'shimcha buyurtma saqlash tanklarining asosiy konstruktsiyasini ishlab chiqarish uchun ishlatiladi. Hozirda ishlab chiqarish yakunlandi va mahsulotlar Dubay portiga jo'natildi. "Professional xizmatlar + barqaror sifat" ga tayangan holda, GNEE Yaqin Sharqdagi neft-kimyo materiallari bozorini muvaffaqiyatli ochdi.
Bepul namuna olish uchun bosing
Agar siz GNEE mahsulotlari haqida ko'proq bilmoqchi bo'lsangiz, elektron pochta manziliga xat yuborishingiz mumkinalloy@gneesteelgroup.com. Biz sizga yordam berishdan xursandmiz.
A285 Grade C ekvivalenti nima?
Astm A285 C darajasining ekvivalenti
ASTM ekvivalenti yuqori{0}}bosimli po'latdirEvropa darajasi - P235GH, Britaniya standarti 161 Gr. 360/164 Gr. 360 bahoga ega.
SA 285 C materiali nima?
SA 285 Gr C bosimli idish plitalari apast va o'rta kuchga ega bo'lgan karbonli po'lat plitalar, u yaxshi payvandlanish va shakllanuvchanlikka ega. A285 darajali C plitalari korroziyaga mukammal qarshilikka ega va yaxshi pishiqligi va egiluvchanligi tufayli keng ko'lamli ilovalar uchun javob beradi.
ASTM A285 Grade C ning harorati qanday?
A285 C toifali ASTM po'lat plitalari past haroratli ilovalar uchun maxsus ishlab chiqilmagan. Bu asosan oʻrtacha va past bosimli idishlar uchun-qoʻllaniladigan uglerodli poʻlat plastinka. A285 C po'lat plitalar uchun odatiy ish harorati oralig'iatrof-muhit harorati taxminan 200 daraja (390 daraja F).
A285 nima?
ASTM A285 spetsifikatsiyasiBosimli idish plitalari, uglerodli po'lat, past- va o'rta-kuchlanishga chidamliligi-birlashtiruvchi bosimli idishlar uchun standart spetsifikatsiya. Turli xil quvvat darajalariga ega bo'lgan uchta nav, shu jumladan, 2" gacha qalinlikda mavjud.
A285 va A36 o'rtasidagi farq nima?
A285 C darajasi past va o'rta kuchlanish kuchi 380 dan 515 MPa gacha, A36 materialining kuchlanish kuchi 400 dan 500 Mpa gacha.. Bu ularning kimyoviy tarkibidagi o'zgaruvchanlik bilan bog'liq.
ASTM A285 C darajasining ekvivalenti nima?
A285 Gr.C plitalarining ekvivalent po'lat navlari:
| Britaniya standarti | Evropa normasi | ASTM/ASME |
|---|---|---|
| 161 Gr.360/164 Gr.360 | P235GH | A/SA285 - C darajasi |
| GNEE tomonidan ta'minlangan bosimli idish plitalarining darajalari | |||||
| ASTM | ASTM A202/A202M | ASTM A202 A darajasi | ASTM A202 B darajasi | ||
| ASTM A203/A203M | ASTM A203 A darajasi | ASTM A203 B darajasi | ASTM A203 D darajasi | ASTM A203 E darajasi | |
| ASTM A203 F darajasi | |||||
| ASTM A204/A204M | ASTM A204 A darajasi | ASTM A204 B darajasi | ASTM A204 C darajasi | ||
| ASTM A285/A285M | ASTM A285 A darajasi | ASTM A285 B darajasi | ASTM A285 C darajasi | ||
| ASTM A299/A299M | ASTM A299 A darajasi | ASTM A299 B darajasi | |||
| ASTM A302/A302M | ASTM A302 A darajasi | ASTM A302 B darajasi | ASTM A302 C darajasi | ASTM A302 D darajasi | |
| ASTM A387/A387M | ASTM A387 5-sinf 1-sinf | ASTM A387 5-sinf 2-sinf | ASTM A387 11-sinf 1-sinf | ASTM A387 11-sinf 2-sinf | |
| ASTM A387 12-sinf 1-sinf | ASTM A387 12-sinf 2-sinf | ASTM A387 22-sinf 1-sinf | ASTM A387 22-sinf 2-sinf | ||
| ASTM A515/A515M | ASTM A515 60-sinf | ASTM A515 65-sinf | ASTM A515 70-sinf | ||
| ASTM A516/A516M | ASTM A516 55-sinf | ASTM A516 60-sinf | ASTM A516 65-sinf | ASTM A516 70-sinf | |
| ASTM A517/A517M | ASTM A517 A darajasi | ASTM A517 B darajasi | ASTM A517 E darajasi | ASTM A517 F darajasi | |
| ASTM A517 P darajasi | ASTM A517 J darajasi | ||||
| ASTM A533/A533M | ASTM A533 A sinfi 1 | ASTM A533 B sinfi 1 | ASTM A533 C sinfi 1 | ASTM A533 D sinfi 1 | |
| ASTM A533 A sinfi 2 | ASTM A533 B sinfi 2 | ASTM A533 C sinfi 2 | ASTM A533 D sinfi 2 | ||
| ASTM A533 A sinfi 3 | ASTM A533 B sinfi 3 | ASTM A533 C sinfi 3 | ASTM A533 D sinfi 3 | ||
| ASTM A537/A537M | ASTM A537 1-sinf | ASTM A537 2-sinf | ASTM A537 sinf 3 | ||
| ASTM A612/A612M | ASTM A612 | ||||
| ASTM A662/A662M | ASTM A662 A darajasi | ASTM A662 B darajasi | ASTM A662 C darajasi | ||
| UZ | EN10028-2 | EN10028-2 P235GH | EN10028-2 P265GH | EN10028-2 P295GH | EN10028-2 P355GH |
| UZ10028-2 16MO3 | |||||
| EN10028-3 | EN10028-3 P275N | EN10028-3 P275NH | EN10028-3 P275NL1 | EN10028-3 P275NL2 | |
| EN10028-3 P355N | EN10028-3 P355NH | EN10028-3 P355NL1 | EN10028-3 P355NL2 | ||
| EN10028-3 P460N | EN10028-3 P460NH | EN10028-3 P460NL1 | EN10028-3 P460NL2 | ||
| EN10028-5 | EN10028-5 P355M | EN10028-5 P355ML1 | EN10028-5 P355ML2 | EN10028-5 P420M | |
| EN10028-5 P420ML1 | EN10028-5 P420ML2 | EN10028-5 P460M | EN10028-5 P460ML1 | ||
| EN10028-5 P460ML2 | |||||
| EN10028-6 | EN10028-6 P355Q | EN10028-6 P460Q | EN10028-6 P500Q | EN10028-6 P690Q | |
| EN10028-6 P355QH | EN10028-6 P460QH | EN10028-6 P500QH | EN10028-6 P690QH | ||
| EN10028-6 P355QL1 | EN10028-6 P460QL1 | EN10028-6 P500QL1 | EN10028-6 P690QL1 | ||
| EN10028-6 P355QL2 | EN10028-6 P460QL2 | EN10028-6 P500QL2 | EN10028-6 P690QL2 | ||
| JIS | JIS G3115 | JIS G3115 SPV235 | JIS G3115 SPV315 | JIS G3115 SPV355 | JIS G3115 SPV410 |
| JIS G3115 SPV450 | JIS G3115 SPV490 | ||||
| JIS G3103 | JIS G3103 SB410 | JIS G3103 SB450 | JIS G3103 SB480 | JIS G3103 SB450M | |
| JIS G3103 SB480M | |||||
| GB | GB713 | GB713 Q245R | GB713 Q345R | GB713 Q370R | GB713 12Cr1MoVR |
| GB713 12Cr2Mo1R | GB713 13MnNiMoR | GB713 14Cr1MoR | GB713 15CrMoR | ||
| GB713 18MnMoNbR | |||||
| GB3531 | GB3531 09MnNiDR | GB3531 15MnNiDR | GB3531 16MnDR | ||
| DIN | DIN 17155 | DIN 17155 HI | DIN 17155 HII | DIN 17155 10CrMo910 | DIN 17155 13CrMo44 |
| DIN 17155 15Mo3 | DIN 17155 17Mn4 | DIN 17155 19Mn6 | |||