Introduction To N08800 Nickel-based High Temperature Alloy

Mar 07, 2024 Xabar QOLDIRISH

N08800 is a nickel-based alloy material, also known as Incoloy 800 or UNS N08800. Mainly composed of nickel, iron and chromium, it is a high-temperature and corrosion-resistant alloy commonly used in industrial applications in high-temperature and highly corrosive environments.


In the chemical composition of N08800 alloy, the nickel content is usually between 32-38%, the iron content is between 43-50%, and the chromium content is between 17-21%. In addition, it also contains small amounts of carbon, manganese, silicon, aluminum, titanium and other elements. The addition of these elements can further improve the performance and stability of the alloy.

 

N08800 alloy has excellent corrosion resistance and can resist corrosion from a variety of acid, alkali and salt solutions. Especially in high temperature and high pressure environments, its corrosion resistance is more outstanding. In addition, the alloy also has good high-temperature strength and toughness, can withstand mechanical stress and thermal stress at high temperatures, and is not easily deformed or damaged.


Due to these excellent properties of N08800 alloy, it is widely used in various industrial fields with high temperatures and strong corrosion environments, such as petrochemical industry, chemical industry, nuclear industry, aerospace, etc. In these fields, N08800 alloy is often used to manufacture key equipment such as reactors, heat exchangers, furnace tubes, pipes, valves, etc. to ensure the long-term stable operation and safety and reliability of the equipment.

China steel round bar Distributors

China round steel Manufacturers

China round bar Suppliers