S355G10+N steel plate introduction: S355G10+N is a kind of European standard steel plate, belongs to the fixed coastal structure with weldable structural steel, its delivery status for normalized or normalized rolled, the impact of the impact of the -40 degrees impact test, G after the 10 indicates the steel characteristics of the relevant figures, as for the back of the +N means normalized or normalized rolled, just standard inside the naming of the steel number of a method.
S355G10+N steel plate implementation standard: implementation of EN10225-2009 standard.
S355G10+N steel plate delivery status: steel plate should be normalized or normalized rolled delivery
S355G10+N steel plate performance analysis: marine engineering steel is suitable for a variety of complex working conditions and harsh natural environment, and the service cycle is 50% higher than the ordinary ship steel, so the requirements of marine engineering steel not only has high strength and high plasticity, good welding performance and resistance to seawater erosion, should also have a good toughness to ensure that the steel and equipment to adapt to a variety of loads and low-temperature environment.
S355G10+N steel plate application scope: S355G10+N belongs to the high strength structural steel series products, with good comprehensive mechanical properties, welding performance, process performance. It is suitable for the manufacture of structural parts such as oil extraction platforms and terminal equipment in ocean and offshore.