A516 engil po'latdan yasalgan bosimli idishning kimyoviy tarkibi
| Kimyoviy tarkibi | Qalinligi t (mm) uchun maksimal C % | Mn % uchun qalinligi t (mm) |
Si % | P % maks |
S % maks |
||||
|---|---|---|---|---|---|---|---|---|---|
| 6-12,5 mm | 12,5-25 mm | 25-50 mm | >50 mm | 12,5 mm dan kam yoki unga teng | >12,5 mm | ||||
| A516 Gr55 | 0.18 | 0.20 | 0.22 | 0.25 | 0.55-0.98 | 0.60-1.30 | 0.13-0.45 | 0.035 | 0.035 |
| A516 Gr60 | 0.21 | 0.23 | 0.23 | 0.25 | 0.6-0.9 | 0.80-1.20 | 0.13-0.45 | 0.035 | 0.035 |
| A516 Gr65 | 0.24 | 0.26 | 0.26 | 0.28 | 0.85-1.20 | 0.85-1.20 | 0.13-0.45 | 0.035 | 0.035 |
| A516 Gr70 | 0.27 | 0.28 | 0.28 | 0.30 | 0.85-1.20 | 0.85-1.20 | 0.13-0.45 | 0.035 | 0.035 |
A516 Karbonli po'latdan yasalgan bosimli idishning mexanik xususiyati
| Mexanik xususiyat | Kuchlanish kuch (MPa) |
Minimal Yo'l bering kuch (MPa) |
Minimal cho'zilish (%) o'lchagich uzunligi | |
|---|---|---|---|---|
| 50 mm | 200 mm | |||
| A516 Gr55 | 380-515 | 205 | 27 | 23 |
| A516 Gr 60 | 415 - 550 | 220 | 25 | 21 |
| A516 Gr65 | 450 - 585 | 240 | 23 | 19 |
| A516 Gr70 | 485 - 620 | 260 | 21 | 17 |
A516 bosimli idishning po'lat qobig'i plitasining zaxira o'lchamlari
| BAJA | O'LCHAN (Dyuym) | WIDTH (Dyuym) | UZUNLIK (Dyuym) |
|---|---|---|---|
| A516 / SA516 | 0.1875 | 96 | 240/480 |
| A516 / SA516 | 0.2500 | 96/120 | 240/480 |
| A516 / SA516 | 0.3125 | 96/120 | 240/480 |
| A516 / SA516 | 0.3750 | 96/120 | 240/480 |
| A516 / SA516 | 0.5000 | 96/120 | 240/480 |
| A516 / SA516 | 0.6250 | 96/120 | 240/480 |
| A516 / SA516 | 0.7500 | 96/120 | 240/480 |
| A516 / SA516 | 0.8750 | 96/120 | 240/480 |
| A516 / SA516 | 1.0000 | 96/120 | 240/480 |
| A516 / SA516 | 1.1250 | 96/120 | 240/480 |
| A516 / SA516 | 1.2500 | 96/120 | 240/480 |
| A516 / SA516 | 1.5000 | 96/120 | 240/480 |
| A516 / SA516 | 1.7500 | 96/120 | 240/480 |
| A516 / SA516 | 2.0000 | 96/120 | 240/480 |
| A516 / SA516 | 2.2500 | 96/120 | 240/480 |
| A516 / SA516 | 2.5000 | 96/120 | 240/480 |
| A516 / SA516 | 2.7500 | 96/120 | 240/480 |
| A516 / SA516 | 3.0000 | 96/120 | 240/480 |
| A516 / SA516 | 3.2500 | 96/120 | 240 |
| A516 / SA516 | 3.5000 | 96/120 | 240 |
| A516 / SA516 | 3.7500 | 96/120 | 240 |
| A516 / SA516 | 4.0000 | 96/120 | 240 |
| A516 / SA516 | 5.0000 | 96 | 240 |
| A516 / SA516 | 6.0000 | 96 | 240 |
Issiq haddelenmiş qozonli po'lat plitalar Mahsulotlar tasviri



GNEE guruhi jamoasi fotosurati

GNEE guruhi mijozlariga tashrif buyurish






GNEE Group po'lat ko'rgazmasi






Bizda etarli inventar mavjud va eng qisqa vaqt ichida qadoqlashimiz va jo'natishimiz mumkin. Agar sizda A516 bosimli idish uglerod po'lat plitalari yoki boshqa issiq haddelenmiş po'lat mahsulotlariga ehtiyojingiz bo'lsa, men bilan bog'laning.
Issiq teglar: A516 bosimli idish karbonli po'lat plitalar, Xitoy A516 bosimli idish karbonli po'lat plitalar ishlab chiqaruvchilar, etkazib beruvchilar, zavod