GB/T713 past qotishma bosimli idish plitasi

GB/T713 past qotishma bosimli idish plitasi

Mahsulot: GB/T713 past qotishma bosimli idish plitasi
Turi: Chelik plitalar
Standart: GB/T
Tolerantlik: ± 1%
So'rov yuborish
Hozir chat
Ta'rif
Texnik parametrlar

GB/T713 past qotishma bosimli idish plitasi


GB / T 713 - bosimli idishlar uchun po'lat plitalar uchun Xitoy milliy standarti. Ushbu standart qozon va bosimli idishlar uchun po'lat plitalar tartibining mazmunini, sinflarning ifodasi, o'lchamlari, shakli, vazni va ruxsat etilgan og'ishlari, texnik talablar, sinov usullari, tekshirish qoidalari, qadoqlash, markalash va sifat sertifikatlari va boshqalarni belgilaydi.

 

 
GB standarti uchun biz taqdim eta oladigan baholar

 

GB

GB713Q245R, Q345R, Q370R, 18MnMoNbR, 13MnNiMoR,

15CrMoR, 14Cr1MoR, 12Cr2Mo1R, 12Cr1MoVR

GB3531 16MnDR,15MnNiDR,09MnNiDR va boshqalar

 

 
q245R idish plitasining kimyoviy tarkibi

 

C Si Mn P S Al
0,20 maksimal 0,35 maks. 0.50-1.00 0,025 maksimal 0,015 maks. 0,020 min.

 

 
Q345R qozon plitasining kimyoviy tarkibi

 

Baho

C%

SI%

million%

cr%

Ni%

Mo%

Nb%

V%

P%

S%

Alt%

Q345R

O.20 dan kam yoki teng

0,55 dan kam yoki unga teng

1.20-1.60

 

 

 

 

0,025 dan kam yoki unga teng

0,015 dan kam yoki unga teng

0,020 dan katta yoki unga teng

 

 
Q370R qozon po'lat plastinka kimyoviy tarkibi

 

Baho C% SI% million% cr% Ni% Mo% Nb% V% P% S% Alt%
Q370R O.18 dan kam yoki teng 0,55 dan kam yoki unga teng 1.20-1.60     0.015-0.050 0,025 dan kam yoki unga teng 0,015 dan kam yoki unga teng  

 

 
18MnMoNbR po'lat qozon plitasining kimyoviy tarkibi

 

Baho C% SI% million% cr% Ni% Mo% Nb% V% P% S% Alt%
18MnMoNbR O.22 dan kam yoki teng 0.15-0.50 1.20-1.60   0.45-0.65 0.025-0.050 0,020 dan kam yoki unga teng 0,010 dan kam yoki unga teng  

 

 
13MnNiMoR qozon plitasi Chelik kimyoviy tarkibi

 

C Si Mn Cr Ni Mo Nb P S
0,15 dan kam yoki unga teng 0.15-0.50 1.20-1.60 0.20-0.40 0.60-1.00 0.20-0.40 0.005-0.020 0,020 dan kam yoki unga teng 0,010 dan kam yoki unga teng

 

 
15CrMoR bosimli idish plastinka kimyoviy tarkibi

 

C

Si

Mn

P

S

Cr

Mo

0.12-0.18

0.15-0.40

0.40-0.70

0,025 dan kam yoki unga teng

0,010 dan kam yoki unga teng

0.80-1.20

0.3-0.60

 

 
14Cr1MoR bosimli idish po'lat plastinka kimyoviy tarkibi

 

C

Si

Mn

P

Cr

Mo

Ni

0.05%-0.17%

0.50%-0.80%

0.40%-0.65%

0.010%-0.012%

1%-1.5%

0.45%-0.65%

0.20%-0.25%

 

 
12Cr2Mo1R bosimli idish plastinka materialining kimyoviy tarkibi

 

C Si Mn P S Cr Mo
0.08-0.15 0.50 0.30-0.60 0.020 0.010 2.00-2.50 0.90-1.10

 

 
12Cr1MoVR idish po'lat plastinka kimyoviy tarkibi

 

Baho C Si Mn Cu Ni Cr Mo Nb V Ti Alt P S
12Cr1MoVR 0.08-0.15 0.15-0.40 0.40-0.70 0,30 dan kam yoki unga teng 0,30 dan kam yoki unga teng 0.90-1.20 0.25-0.35 - 0.15-0.30 - - 0,025 dan kam yoki unga teng 0,010 dan kam yoki unga teng

 

 
Nega bizni tanlaysiz?

 

1. Bepul namuna.
2. Rich bozor prognozi maslahati.
3. O'z vaqtida javob.
4. Xarajatlarni tejashga yordam beradigan narxni qulflang, Savdo kafolati.
5. Ilg'or ishlab chiqarish liniyalari, Kuchli ishlab chiqarish qobiliyati.
6. Professional buyurtma tizimi, To'liq ishlash.

 

 
GB / T713 bosimli idish sifatli po'lat plitalar Mahsulotlar tasviri

 

China pressure vessel steel plate Suppliers

 

 
GNEE guruhi jamoasi fotosurati

 

China carbon steel pressure vessel Suppliers

 

 
GNEE guruhi mijozlariga tashrif

 

China pressure vessel quality steel Manufacturers

 

 
GNEE Group xorijiy po'lat ko'rgazmalarida ishtirok etadi

 

China boiler quality plates Distributors

Buyurtmalaringizga batafsil javob berish uchun professional xodimlarimiz bor. GB / T713 past qotishma bosimli idish plitasi haqida savollaringiz bo'lsa, iltimos, men bilan bog'laning.

 

Issiq teglar: gb / t713 past qotishma bosimli idish plitasi, Xitoy gb / t713 past qotishma bosimli idish plitasi ishlab chiqaruvchilari, etkazib beruvchilari, zavodi