JIS G3192-2008 standarti issiq haddelenmiş po'lat qismlarning keng ko'lamli modellarini o'z ichiga oladi, shu jumladan kanallar po'latlari, burchaklar, H-nurlar va boshqalar. JIS G3192-2008 standarti issiq haddelenmiş po'lat qismlarning keng ko'lamli modellarini qamrab oladi. Ular orasida kanal po'latining modellari SS400, SS490, SS540 va boshqalarni o'z ichiga oladi.
SS540 metall kanali yuqori rentabellik va kuchlanish kuchiga ega. Uning rentabelligi odatda 390MPa va 540MPa orasida va kuchlanish kuchi 540MPa va 700MPa orasida. Bundan tashqari, u yaxshi cho'zilish va zarba chidamliligiga ega, bu uni sovuq va issiq ish uchun mos qiladi.
SS540 po'lat metall kanalining kimyoviy tarkibi
| Baho | C dan kichik yoki teng | Si | Mn dan kichik yoki teng | P dan kichik yoki teng | S dan kichik yoki teng |
| SS540 | 0.30 | 0.40 | 1.60 | 0.040 | 0.040 |
SS540 kanal nurining mexanik xususiyati
| rade | Siqish sinovi (ko'ndalang) | ||||||
| Yuqori rentabellik darajasi MPa | Kuchlanish kuchi MPa | Uzayish% | 180 daraja Burilish testi b Ichki diametri 35 mm dan katta yoki unga teng | ||||
| Nominal qalinligi mm | L=50 b=25 | L=200 b=40 | |||||
| Nominal qalinligi mm | |||||||
| 16 dan kichik yoki teng | >16 | 5 dan kichik yoki teng | >5~16 | >16 | |||
| SS540 | 400 dan katta yoki teng | 390 dan katta yoki unga teng | 540 dan katta yoki unga teng | 16 dan katta yoki teng | 13 dan katta yoki teng | 17 dan katta yoki teng | 4a |
SS540 parallel gardish kanali mavjud o'lchamlar
| Hajmi | Chuqurlik | Kengligi | Qalinligi | Uzunlik | Og'irligi (lbs/ft) |
| 3/4" x 3/8" x 1/8" | 0.75" | 0.375" | 1/8" | 240.00" | 0.560 |
| 1" x 1/2" x 1/8" | 1" | 0.5" | 1/8" | 240.00" | 0.840 |
| 1-1/4" x 1/2" x 1/8" | 1.25" | 0.5" | 1/8" | 240.00" | 0.990 |
| 1-1/2" x 1/2" x 1/8" | 1.5" | 0.5" | 1/8" | 240.00" | 1.119 |
| 1-1/2" x 9/16" x 3/16" | 1.5" | 0.563" | 3/16" | 240.00" | 1.440 |
| 1-1/2" x 3/4" x 1/8" | 1.5" | 0.75" | 1/8" | 240.00" | 1.170 |
| 2" x 1/2" x 1/8" | 2" | 0.5" | 1/8" | 240.00" | 1.430 |
| 2" x 9/16" x 3/16" | 2" | 0.563" | 3/16" | 240.00" | 1.860 |
| 2" x 5/8" x 1/4" | 2" | 0.625" | 1/4" | 240.00" | 2.280 |
| 2" x 1" x 1/8" | 2" | 1" | 1/8" | 240.00" | 1.590 |
| 2" x 1" x 3/16" | 2" | 1" | 3/16" | 240.00" | 2.319 |
| 2-1/2" x 5/8" x 3/16" | 2.5" | 0.625" | 3/16" | 240.00" | 2.270 |
SS540 tizimli kanal mahsulot tasviri

GNEE guruhi jamoasi fotosurati

GNEE guruhi mijozlariga tashrif

GNEE Group xorijiy po'lat ko'rgazmalarida ishtirok etadi

Bizda professional onlayn xizmat xodimlari mavjud. Agar sizda SS540 Carbon Steel Channel haqida savollaringiz bo'lsa, iltimos, bizga so'rov yuboring va biz sizga bir ish kuni ichida javob beramiz.
Issiq teglar: ss540 karbonli po'lat kanal, Xitoy ss540 karbonli po'lat kanal ishlab chiqaruvchilar, etkazib beruvchilar, zavod