S235 Evropa standartidagi oddiy uglerodli strukturaviy po'latdir, standartni amalga oshirish Evropa standarti EN10025 standarti, mos ravishda S235JR, S235J0 va S235J2 uchta sinfdir.
S235JR, S235J0 va S235J2 uch darajali ta'sir harorati o'rtasidagi farq, JR xona haroratining ta'sirini, 0 daraja ta'siri nomidan J0, -20 daraja ta'siri nomidan J2, har xil haroratning ta'siridan tashqari, farq yo'q.
S235JR po'lat Evropaga tegishli standart oddiy uglerodli konstruktiv po'latdir, S235R H{2}}po'lat po'latdan asosan temir yo'l, ko'prik, barcha turdagi qurilish loyihalari, statik yuklarni ko'taradigan turli metall qismlar va issiqlik bilan ishlov berish va umumiy payvandlashni talab qilmaydigan muhim bo'lmagan mexanik qismlarni ishlab chiqarish uchun ishlatiladi.
S235J0 - bu Evropa standartidagi qotishma bo'lmagan strukturaviy po'latdir, Q235C milliy standartiga teng, S235J0 - uglerodli po'latdir. Taxminan 0,05% dan 0,70% gacha bo'lgan uglerod miqdori, individual 0,90% gacha bo'lishi mumkin. Oddiy uglerodli strukturaviy po'lat va yuqori sifatli uglerodli strukturaviy po'latning ikkita toifasiga bo'linishi mumkin.
S235JR metall h nurining kimyoviy tarkibi
| C | Mn | P | S | N | Cu | CEV |
| maksimal 0,2 | maksimal 1,4 | maksimal 0,04 | maksimal 0,04 | maksimal 0,012 | maksimal 0,55 | maksimal 0,38 |
S235J0 h shaklidagi po'lat kimyoviy tarkibi
| C | Mn | P | S | N | Cu | CEV |
| maksimal 0,17 | maksimal 1,4 | maksimal 0,035 | maksimal 0,035 | maksimal 0,012 | maksimal 0,55 | maksimal 0,38 |
konstruktiv po'lat h nurlarining o'lchamlari
|
H tipidagi po'lat hajmi va nazariy og'irligi |
|||||
| Hajmi (mm) |
Nazariy vazn (kg/m) |
Hajmi (mm) |
Nazariy vazn (kg/m) |
Hajmi (mm) |
Nazariy vazn (kg/m) |
| 100*50*5*7 | 9.3 | 250*125*6*9 | 29 | 446*199*8*12 | 65.1 |
| 100*100*6*8 | 16.9 | 250*250*9*14 | 71.8 | 450*200*9*14 | 74.9 |
| 125*60*6*8 | 13.1 | 294*200*8*12 | 55.8 | 482*300*11*15 | 110.8 |
| 125*125*6.5*9 | 23.6 | 298*149*5.5*8 | 32 | 488*300*11*18 | 124.9 |
| 148*100*6*9 | 31.1 | 340*250*9*14 | 36.7 | 496*199*9*14 | 77.9 |
| 150*75*5*7 | 14 | 300*150*6.5*9 | 93 | 500*200*10*16 | 88.1 |
| 150*150*7*10 | 20.7 | 300*300*10*15 | 78.1 | 582*300*12*17 | 132.8 |
| 175*90*5*8 | 18 | 346*174*6*9 | 41.2 | 588*300*12*20 | 147 |
| 175*175*7.5*11 | 40.4 | 350*175*7*11 | 49.4 | 596*199*10*15 | 92.4 |
| 194*150*6*9 | 29.9 | 350*350*12*19 | 134.9 | 600*200*11*17 | 103.4 |
| 198*99*4.5*7 | 17.8 | 390*300*10*16 | 104.6 | 700*300*13*24 | 181.8 |
| 200*100*5.5*8 | 20.9 | 396*199*7*11 | 56.1 | 800*300*14*26 | 206.8 |
| 200*200*8*12 | 49.9 | 400*200*8*13 | 65.4 | 900*300*16*28 | 240.1 |
| 244*175*7*11 | 43.6 | 400*400*13*21 | 171.7 | ||
| 248*124*5*8 | 25.1 | 440*300*11*18 | 120.8 | ||
|
Uzunligi=6------12metr |
|||||
h metall nurli mahsulot tasviri

GNEE guruhi jamoasi fotosurati

GNEE guruhi mijozlariga tashrif


Bizda 15 yildan ortiq ishlab chiqarish va eksport tajribamiz bor. Agar sizda S235JR S235J0 H Section Steel yoki boshqa profilli po'lat uchun moslashtirilgan ehtiyojlaringiz bo'lsa, iltimos, men bilan bog'laning.
Issiq teglar: s235jr s235j0 h po'lat po'lat, Xitoy s235jr s235j0 h po'lat po'lat ishlab chiqaruvchilar, etkazib beruvchilar, zavod