Kema qurish uchun lampochka tekis po'lat
Egiluvchan yassi po'lat, asosan, kemasozlik va ko'prik qurilishi sohasida qo'llaniladigan o'rta-o'lchamdagi ko'ndalang- materialdir, kema qurish uchun egiluvchan yassi po'lat esa kema qurish uchun yordamchi-o'rta o'lchamdagi-kesimli materialdir.
Kema qurish sferik yassi po'latdan foydalanish:
Katta va oddiy kemalarni loyihalashda asosiy korpus asosan skelet (shuningdek qovurg'a yoki keel deb ataladi) bilan bog'langan kema qurish po'lat plitalari bilan bir xil qalinlikdagi va sinfdagi kema qurish sferoidli yassi po'latdan yasalgan.
Kema qurish lampochkasi tekis po'lat o'lchami
| Model | hajmi (mm) | CSA (sm2) | vazn (kg/m) | ||||
| b | t | h | r1 | r | |||
| HP80x5 | 80 | 5 | 19 | 4 | 1,5 dan kam yoki teng | 5.41 | 4.25 |
| HP80x6 | 6 | 20 | 2 dan kichik yoki teng | 6.21 | 4.88 | ||
| HP100x7 | 100 | 7 | 22.5 | 4.5 | 2 dan kichik yoki teng | 8.74 | 6.86 |
| HP100x8 | 8 | 23.5 | 9.74 | 7.65 | |||
| HP120x6 | 120 | 6 | 23 | 5 | 2 dan kichik yoki teng | 9.32 | 7.32 |
| HP120x7 | 7 | 24 | 10.52 | 8.26 | |||
| HP120x8 | 8 | 25 | 11.72 | 9.2 | |||
| HP140x7 | 140 | 7 | 26 | 5.5 | 2 dan kichik yoki teng | 12.43 | 9.75 |
| HP140x8 | 8 | 27 | 13.83 | 10.85 | |||
| HP140x10 | 10 | 29 | 3 dan kichik yoki teng | 16.63 | 13.05 | ||
| HP160x7 | 160 | 7 | 29 | 6 | 2 dan kichik yoki teng | 14.6 | 11.46 |
| HP160x8 | 8 | 30 | 16.2 | 12.72 | |||
| HP160x9 | 9 | 31 | 17.8 | 13.97 | |||
| HP160x11 | 11 | 33 | 3 dan kichik yoki teng | 21 | 16.49 | ||
| HP180x8 | 180 | 8 | 33 | 7 | 2 dan kichik yoki teng | 18.86 | 14.8 |
| HP180x9 | 9 | 34 | 20.66 | 16.22 | |||
| HP 180x10 | 10 | 35 | 3 dan kichik yoki teng | 22.46 | 17.63 | ||
| HP180x11 | 11 | 36 | 24.26 | 19.04 | |||
| HP200x9 | 200 | 9 | 37 | 8 | 2 dan kichik yoki teng | 23.66 | 18.57 |
| HP200x10 | 10 | 38 | 3 dan kichik yoki teng | 25.66 | 20.14 | ||
| HP200x11 | 11 | 39 | 27.66 | 21.71 | |||
| HP200x12 | 12 | 40 | 29.66 | 23.28 | |||
| HP220x10 | 220 | 10 | 41 | 9 | 3 dan kichik yoki teng | 29.66 | 22.27 |
| HP220x11 | 11 | 42 | 29 | 24.5 | |||
| HP220x12 | 12 | 43 | 31.2 | 26.22 | |||
| HP240x10 | 240 | 10 | 40 | 10 | 3 dan kichik yoki teng | 33.49 | 25.5 |
| HP240x11 | 11 | 45 | 34.89 | 27.39 | |||
| HP240x12 | 12 | 46 | 37.29 | 29.27 | |||
| HP260x10 | 260 | 10 | 47 | 11 | 3 dan kichik yoki teng | 36.11 | 28.35 |
| HP260x11 | 11 | 48 | 38.71 | 30.39 | |||
| HP260x12 | 12 | 49 | 41.31 | 32.43 | |||
| HP280x11 | 280 | 11 | 51 | 12 | 3 dan kichik yoki teng | 42.68 | 33.5 |
| HP280x12 | 12 | 52 | 45.48 | 35.7 | |||
| HP280x13 | 13 | 53 | 48.28 | 37.9 | |||
| HP300x11 | 300 | 11 | 54 | 13 | 3 dan kichik yoki teng | 46.78 | 36.7 |
| HP300x12 | 12 | 55 | 49.79 | 39.09 | |||
| HP300x13 | 13 | 56 | 52.79 | 41.44 | |||
| HP320x12 | 320 | 12 | 58 | 14 | 3 dan kichik yoki teng | 54.25 | 42.6 |
| HP320x13 | 13 | 59 | 57.25 | 45.09 | |||
| HP320x14 | 14 | 60 | 4 dan kichik yoki teng | 60.85 | 47.6 | ||
| HP340x12 | 340 | 12 | 61 | 15 | 3 dan kichik yoki teng | 58.84 | 46.2 |
| HP340x13 | 13 | 62 | 62.24 | 48.86 | |||
| HP340x14 | 14 | 63 | 4 dan kichik yoki teng | 65.54 | 51.5 | ||
| HP370x13 | 370 | 13 | 66.5 | 16.5 | 3 dan kichik yoki teng | 69.7 | 54.7 |
| HP370x14 | 14 | 67.5 | 4 dan kichik yoki teng | 73.4 | 57.6 | ||
| HP370x15 | 15 | 68.5 | 77.1 | 60.5 | |||
| HP400x14 | 400 | 14 | 72 | 18 | 4 dan kichik yoki teng | 81.48 | 63.96 |
| HP400x15 | 15 | 73 | 85.48 | 67.1 | |||
| HP400x16 | 16 | 74 | 89.48 | 70.2 | |||
| HP430x14 | 430 | 14 | 76.5 | 19.5 | 4 dan kichik yoki teng | 89.7 | 70.6 |
| HP430x15 | 15 | 77.5 | 94.19 | 73.9 | |||
| HP430x17 | 17 | 79.5 | 102.79 | 80.7 | |||
| HP430x19 | 19 | 81.5 | 111.39 | 87.4 | |||
| HP430x20 | 20 | 82.5 | 115 | 90.8 | |||
Kema qurish tekis bar Mahsulotlar tasviri

GNEE guruhi jamoasi fotosurati

GNEE guruhi mijozlariga tashrif

GNEE Group po'lat ko'rgazmasi

Bizda sotuvdan keyingi-ajoyib xizmat mavjud. Kema qurish uchun lampochkaning tekis po'lati haqida savollaringiz bo'lsa, biz bilan bog'lanishingiz mumkin va biz sizga ikki soat ichida javob beramiz.
Issiq teglar: kema qurish uchun lampochkaning tekis po'lati, Xitoyning kema qurish uchun lampochkaning tekis po'lati ishlab chiqaruvchilar, etkazib beruvchilar, zavod