EN10028-6 P355QH Yuqori quvvatli karbonli po'lat plitalar

Oct 21, 2025 Xabar QOLDIRISH

c bosimli idishlar va yuqori-haroratda foydalanish uchun. "P" bosimni bildiradi, "355" 355 MPa oqim kuchini bildiradi va "QH" söndürme va haroratni bildiradi. Ekvivalent navlarga P355NH va A516 70-sinf kiradi. U qattiqlik, payvandlanish va issiqlikka chidamlilikni taklif etadi va neft, gaz, energetika va kimyo sanoatidagi qozonlarda, bosimli idishlarda va issiqlik almashtirgichlarda qo'llaniladi.

 

EN10028-6 P355QH bosimli idish va qozon po'lat plitalari kimyoviy tarkibi va mexanik xususiyatlari

 

P355QH Kimyoviy tarkibi

Baho

Maksimal element (%)

C

Si

Mn

P

S

N

B

P355QH

0.16

0.4

1.5

0.025

0.015

0.015

0.005

Mo

Cu

Nb

Ni

Ti

V

Zr

0.25

0.3

0.05

0.5

0.03

0.06

0.05

 

Baho

 

P355QH Mexanik xususiyat

Qalinligi

Yo'l bering

Kuchlanish

Cho'zilish

P355QH

mm

Min Mpa

Mpa

Min %

6-50

355

490-630

22%

50-100

335

490-630

22%

100-150

315

450-590

22%

 

EN10028-6 P355QH bosimli idish va qozon uchun po'lat plitalar ilovasi

 

EN10028-6 P355QH Pressure Vessel And Boiler Steel PlateKimyoviy reaktsiya idishlari

EN10028-6 P355QH qozon va bosimli idish po'lat plitasi sintez reaktsiyalarida (masalan, o'g'it zavodlarida ammiak sintez minoralari va kimyoviy zavodlarda polimerizatsiya reaktorlari) ishlatiladi. U yuqori harorat va bosimlarga (masalan, ammiak sintezi minorasi 30MPa bosim va 450 daraja haroratda ishlaydi) va o'rta korroziyaga (masalan, vodorod va kislota gazlari) qarshilik ko'rsatishi kerak, buning natijasida hech qanday oqish yoki struktura buzilishi sodir bo'lmaydi.

 

Neft-kimyo saqlash tanklari va minoralari

EN10028-6 P355QH past haroratli bosimli idish po'lat plitasi xom neft, suyultirilgan gaz (LNG) va suyultirilgan neft gazi (LPG) uchun saqlash tanklarida, shuningdek, neftni qayta ishlashda rektifikatsion minoralar va assimilyatsiya minoralarida qo'llaniladi. past-haroratli saqlash idishlari (masalan, -162 darajagacha past haroratli LNG saqlash tanklari) past haroratlarda po‘latning mo‘rt sinishiga yo‘l qo‘ymaslik uchun past haroratda mukammal mustahkamlikka ega po‘lat plitalarni talab qiladi; yuqori bosimli gidrogenatsiya minoralari (neft-kimyoni gidrotozalash jarayoni).

 

EN10028-6 P355QH Pressure Vessel And Boiler Steel PlateIssiqlik almashinuvi idishlari

EN10028-6 P355QH Yuqori-sifatli qozon po'lat plitasi o'rtacha issiqlik almashinuvi uchun uskunalarda (masalan, qobiqli va quvurli issiqlik almashtirgichlar va plastinka issiqlik almashinuvchilari) ishlatiladi. Ularning chig'anoqlari va quvurlari varaqlari o'zgaruvchan issiq va sovuq zarbalarga bardosh berishi, charchoqqa chidamliligini ta'minlashi va tez-tez harorat o'zgarishi natijasida payvand choki yorilishiga yo'l qo'ymaslik kerak.

 

Metallurgiya sanoati

Po'lat zavodlarida (0,5-1,5MPa bosim va 1200 daraja haroratda) yuqori haroratli issiq havoni saqlaydigan "domna pechkasi" yuqori haroratga chidamli EN10028-6 P355QH plitasi; rangli metall eritishda "avtoklav" (masalan, gidrometallurgik mis eritishda yuvish avtoklav) kislotali korroziyaga chidamli bo'lishi kerak va EN10028-6 P355QH bosimli idish po'lat plitasi odatda qo'llaniladi.

 

EN10028-6 P355QH bosimli idish va qozon po'lat plitasi Boshqa nom

 

EN10028-6 P355QH bosimli idish va qozon po'lat plitasi, EN10028-6 P355QH bosimli idish po'lat plitasi, EN10028-6 P355QH qozon po'lat plitasi

 

Qo'shimcha shart

 

UT (Ultratovush tekshiruvi), AR (Faqat issiq haddelenmiş holda), TMCP (Termal mexanik nazoratni qayta ishlash), N (Normallashtirilgan), Q+T (O'chirilgan va Temperlangan), Z yo'nalishi testi (Z15, Z25, Z35), Charpy V-Notch ta'siri testi, Uchinchi tomon SG testi va sinovlari (shu kabilar),

 

Narx so'rash

 

Agar siz GNEE mahsulotlari haqida ko'proq bilmoqchi bo'lsangiz, elektron pochta manziliga xat yuborishingiz mumkinalloy@gneesteelgroup.com.Biz sizga yordam berishdan xursandmiz.

 

GNEE tomonidan ta'minlangan bosimli idish plitalarining darajalari
ASTM ASTM A202/A202M ASTM A202 A darajasi ASTM A202 B darajasi    
ASTM A203/A203M ASTM A203 A darajasi ASTM A203 B darajasi ASTM A203 D darajasi ASTM A203 E darajasi
ASTM A203 F darajasi      
ASTM A204/A204M ASTM A204 A darajasi ASTM A204 B darajasi ASTM A204 C darajasi  
ASTM A285/A285M ASTM A285 A darajasi ASTM A285 B darajasi ASTM A285 C darajasi  
ASTM A299/A299M ASTM A299 A darajasi ASTM A299 B darajasi    
ASTM A302/A302M ASTM A302 A darajasi ASTM A302 B darajasi ASTM A302 C darajasi ASTM A302 D darajasi
ASTM A387/A387M ASTM A387 5-sinf 1-sinf ASTM A387 5-sinf 2-sinf ASTM A387 11-sinf 1-sinf ASTM A387 11-sinf 2-sinf
ASTM A387 12-sinf 1-sinf ASTM A387 12-sinf 2-sinf ASTM A387 22-sinf 1-sinf ASTM A387 22-sinf 2-sinf
ASTM A515/A515M ASTM A515 60-sinf ASTM A515 65-sinf ASTM A515 70-sinf  
ASTM A516/A516M ASTM A516 55-sinf ASTM A516 60-sinf ASTM A516 65-sinf ASTM A516 70-sinf
ASTM A517/A517M ASTM A517 A darajasi ASTM A517 B darajasi ASTM A517 E darajasi ASTM A517 F darajasi
ASTM A517 P darajasi ASTM A517 J darajasi    
ASTM A533/A533M ASTM A533 A sinfi 1 ASTM A533 B sinfi 1 ASTM A533 C sinfi 1 ASTM A533 D sinfi 1
ASTM A533 A sinfi 2 ASTM A533 B sinfi 2 ASTM A533 C sinfi 2 ASTM A533 D sinfi 2
ASTM A533 A sinfi 3 ASTM A533 B sinfi 3 ASTM A533 C sinfi 3 ASTM A533 D sinfi 3
ASTM A537/A537M ASTM A537 1-sinf ASTM A537 2-sinf ASTM A537 sinf 3  
ASTM A612/A612M ASTM A612      
ASTM A662/A662M ASTM A662 A darajasi ASTM A662 B darajasi ASTM A662 C darajasi  
UZ EN10028-2 EN10028-2 P235GH EN10028-2 P265GH EN10028-2 P295GH EN10028-2 P355GH
UZ10028-2 16MO3      
EN10028-3 EN10028-3 P275N EN10028-3 P275NH EN10028-3 P275NL1 EN10028-3 P275NL2
EN10028-3 P355N EN10028-3 P355NH EN10028-3 P355NL1 EN10028-3 P355NL2
EN10028-3 P460N EN10028-3 P460NH EN10028-3 P460NL1 EN10028-3 P460NL2
EN10028-5 EN10028-5 P355M EN10028-5 P355ML1 EN10028-5 P355ML2 EN10028-5 P420M
EN10028-5 P420ML1 EN10028-5 P420ML2 EN10028-5 P460M EN10028-5 P460ML1
EN10028-5 P460ML2      
EN10028-6 EN10028-6 P355Q EN10028-6 P460Q EN10028-6 P500Q EN10028-6 P690Q
EN10028-6 P355QH EN10028-6 P460QH EN10028-6 P500QH EN10028-6 P690QH
EN10028-6 P355QL1 EN10028-6 P460QL1 EN10028-6 P500QL1 EN10028-6 P690QL1
EN10028-6 P355QL2 EN10028-6 P460QL2 EN10028-6 P500QL2 EN10028-6 P690QL2
JIS JIS G3115 JIS G3115 SPV235 JIS G3115 SPV315 JIS G3115 SPV355 JIS G3115 SPV410
JIS G3115 SPV450 JIS G3115 SPV490    
JIS G3103 JIS G3103 SB410 JIS G3103 SB450 JIS G3103 SB480 JIS G3103 SB450M
JIS G3103 SB480M      
GB GB713 GB713 Q245R GB713 Q345R GB713 Q370R GB713 12Cr1MoVR
GB713 12Cr2Mo1R GB713 13MnNiMoR GB713 14Cr1MoR GB713 15CrMoR
GB713 18MnMoNbR      
GB3531 GB3531 09MnNiDR GB3531 15MnNiDR GB3531 16MnDR  
DIN DIN 17155 DIN 17155 HI DIN 17155 HII DIN 17155 10CrMo910 DIN 17155 13CrMo44
DIN 17155 15Mo3 DIN 17155 17Mn4 DIN 17155 19Mn6