S355K2+N po'lat: Kimyoviy tarkibi, mexanik xususiyatlari, ekvivalent darajasi

Oct 20, 2025 Xabar QOLDIRISH

S355K2/+N po'latpast-qotishma, yuqori{1}}konstruktiv po'lat navi bo'lib, o'zining ajoyib mexanik xususiyatlari bilan mashhur bo'lib, uni muhim muhandislik va qurilish ilovalari uchun-mo'qullaydi. EN 10025 Yevropa standartining bir qismi, S355K2/+N ta'sirchan kuch va chidamlilikni taklif etadi.

 

S355K2+N po'latining kimyoviy tarkibi

 

  • S355K2+N SteelUglerod (C): Maksimal 0,20%
  • Silikon (Si): Maksimal 0,55%
  • Marganets (Mn): Maksimal 1,60%
  • Fosfor (P): Maksimal 0,035%
  • Oltingugurt (S): Maksimal 0,035%
  • Azot (N): Minimal 0,015%
  • Mis (Cu): Maksimal 0,50%
  • Chromium (Cr): Maksimal 0,30%
  • Molibden (Mo): Maksimal 0,10%
  • Nikel (Ni): Maksimal 0,50%

 

S355K2+N po'latining mexanik xususiyatlari (nominal qiymatlar)

 

  • Hosildorlik kuchi: Minimal 355 megapaskal (MPa)
  • Kuchlanish kuchi: 470-630 MPa
  • Uzayishi: Minimal 22% (200 mm da) / Minimal 17% (50 mm da)

 

S355K2+N Steel uchun ekvivalent baholar

 

  • ASTM A572-50
  • JIS SM490YB
  • EN 10025-2 S355K2+N
  • GB Q345D

 

S355K2 / + N po'latining asosiy xususiyatlari va ilovalari o'z ichiga oladi

 

S355K2+N SteelYuqori hosildorlik: S355K2/+N minimal oqish quvvati 355 MPa boʻlib, uni konstruktiv yaxlitlik va yuk koʻtarish qobiliyati- muhim boʻlgan ilovalar uchun mos qiladi. U odatda binolar, ko'priklar va sanoat mashinalarini qurishda qo'llaniladi.

Strukturaviy foydalanish: Ushbu po'lat navi asosan ishonchli strukturaviy yaxlitligi tufayli konstruktiv ilovalar uchun ishlatiladi. Bu og'ir yuklarni qo'llab-quvvatlash va qurilish loyihalarida barqarorlikni ta'minlashda hal qiluvchi rol o'ynaydi.

Payvandlash qobiliyati: S355K2/+N o'zining yaxshi payvandlanishi bilan mashhur bo'lib, payvandlangan konstruksiyalar va komponentlarni osonlik bilan ishlab chiqarishni osonlashtiradi. S355K2/+N dan foydalangan holda payvandlangan bo'g'inlar o'zlarining strukturaviy yaxlitligi va chidamliligini saqlaydi.

Shakllanuvchanlik: S355K2/+N shakllantirilishi mumkin, ya'ni bukish, dumalash va sovuq shakllantirish kabi jarayonlar orqali osongina shakllantirilishi mumkin. Ushbu xususiyat qurilish va ishlab chiqarishda zarur bo'lgan turli shakllar va profillarni yaratish uchun qimmatlidir.

Ko'p qirralilik: S355K2/+N po'lat plitalari avtomobilsozlik, qurilish, mashinasozlik va umumiy muhandislik kabi turli sohalarda qo'llaniladi. Ular to'sinlar va ustunlardan tortib mashina qismlarigacha bo'lgan keng turdagi komponentlar va tuzilmalarni ishlab chiqarish uchun ishlatiladi.

Standartlarga muvofiqligi: S355K2/+N po'lat Yevropa standartlariga (EN 10025) muvofiq bo'lib, talab qilinadigan strukturaviy ilovalarda barqaror sifat va ishlashni ta'minlaydi.

Korroziyaga qarshilik: S355K2/+N po'lati korroziyaga-xususiy chidamli bo'lmasa-da, dasturning atrof-muhit sharoitlariga qarab korroziyaga chidamliligini oshirish uchun ishlov berilishi yoki qoplanishi mumkin.

Ta'sirga chidamliligi: S355K2/+N po'lat o'zining yaxshi zarbaga chidamliligi bilan mashhur bo'lib, uni dinamik yuklarga yoki to'satdan zarbalarga duch kelishi mumkin bo'lgan ilovalar uchun mos qiladi.

 

Yakunida,S355K2/+N po'lat - bu yuqori mustahkamligi, ishlab chiqarish qulayligi va sanoat standartlariga muvofiqligi bilan mashhur bo'lgan ko'p qirrali va keng qo'llaniladigan strukturaviy po'latdir. Uning ajoyib mexanik xususiyatlari va og'ir yuklarga va qiyin muhitlarga bardosh berish qobiliyati uni turli xil qurilish va muhandislik loyihalari uchun ishonchli va bardoshli materiallarni qidirayotgan muhandislar va ishlab chiqaruvchilar uchun afzal tanlov qiladi.

 

Narx so'rash

Agar siz GNEE mahsulotlari haqida ko'proq bilmoqchi bo'lsangiz, elektron pochta manziliga xat yuborishingiz mumkinalloy@gneesteelgroup.com. Biz sizga yordam berishdan xursandmiz.

 

GNEE tomonidan ta'minlangan uglerod va past{0}}qotishma yuqori-po'latlar navlari
ASTM/ASME ASTM A36/A36M ASTM A36      
ASTM A283/A283M ASTM A283 A darajasi ASTM A283 B darajasi ASTM A283 C darajasi ASTM A283 D darajasi
ASTM A514/A514M ASTM A514 A darajasi ASTM A514 B darajasi ASTM A514 C darajasi ASTM A514 E darajasi
ASTM A514 F darajasi ASTM A514 H darajasi ASTM A514 J darajasi ASTM A514 K darajasi
ASTM A514 M darajasi ASTM A514 P darajasi ASTM A514 Q darajasi ASTM A514 R darajasi
ASTM A514 S darajasi ASTM A514 T darajasi    
ASTM A572/A572M ASTM A572 42-sinf ASTM A572 50-darajali ASTM A572 55-sinf ASTM A572 60-sinf
ASTM A572 65-sinf      
ASTM A573/A573M ASTM A573 58-sinf ASTM A573 65-sinf ASTM A573 70-sinf  
ASTM A588/A588M ASTM A588 A darajasi ASTM A588 B darajasi ASTM A588 C darajasi ASTM A588 K darajasi
ASTM A633/A633M ASTM A633 A darajasi ASTM A633 C darajasi ASTM A633 D darajasi ASTM A633 E darajasi
ASTM A656/A656M ASTM A656 50-darajali ASTM A656 60-sinf ASTM A656 70-sinf ASTM A656 80-sinf
ASTM A709/A709M ASTM A709 36-sinf ASTM A709 50-darajali ASTM A709 50S darajasi ASTM A709 darajasi 50 Vt
ASTM A709 darajasi HPS 50W ASTM A709 darajasi HPS 70W ASTM A709 100-darajali ASTM A709 darajasi 100 Vt
ASTM A709 darajasi HPS 100W      
ASME SA36/SA36M ASME SA36      
ASME SA283/SA283M ASME SA283 A darajasi ASME SA283 B darajasi ASME SA283 C darajasi ASME SA283 D darajasi
ASME SA514/SA514M ASME SA514 A darajasi ASME SA514 B darajasi ASME SA514 C darajasi ASME SA514 E darajasi
ASME SA514 F darajasi ASME SA514 H darajasi ASME SA514 J darajasi ASME SA514 K darajasi
ASME SA514 M darajasi ASME SA514 P darajasi ASME SA514 Q darajasi ASME SA514 R darajasi
ASME SA514 S darajasi ASME SA514 T darajasi    
ASME SA572/SA572M ASME SA572 42-sinf ASME SA572 50-sinf ASME SA572 55-sinf ASME SA572 60-sinf
ASME SA572 65-sinf      
ASME SA573/SA573M ASME SA573 58-sinf ASME SA573 65-sinf ASME SA573 70-sinf  
ASME SA588/SA588M ASME SA588 A darajasi ASME SA588 B darajasi ASME SA588 C darajasi ASME SA588 K darajasi
ASME SA633/SA633M ASME SA633 A darajasi ASME SA633 C darajasi ASME SA633 D darajasi ASME SA633 E darajasi
ASME SA656/SA656M ASME SA656 50-sinf ASME SA656 60-sinf ASME SA656 70-sinf ASME SA656 80-sinf
ASME SA709/SA709M ASME SA709 36-sinf ASME SA709 50-sinf ASME SA709 50S darajasi ASME SA709 darajasi 50W
ASME SA709 darajasi HPS 50W ASME SA709 darajasi HPS 70W ASME SA709 100-sinf ASME SA709 darajasi 100 Vt
ASME SA709 darajasi HPS 100W      
EN10025 EN10025-2 EN10025-2 S235J0 EN10025-2 S275J0 EN10025-2 S355J0 EN10025-2 S355K2
EN10025-2 S235JR EN10025-2 S275JR EN10025-2 S355JR EN10025-2 S420J0
EN10025-2 S235J2 EN10025-2 S275J2 EN10025-2 S355J2  
EN10025-3 EN10025-3 S275N EN10025-3 S355N EN10025-3 S420N EN10025-3 S460N
EN10025-3 S275NL EN10025-3 S355NL EN10025-3 S420NL EN10025-3 S460NL
EN10025-4 EN10025-4 S275M EN10025-4 S355M EN10025-4 S420M EN10025-4 S460M
EN10025-4 S275ML EN10025-4 S355ML EN10025-4 S420ML EN10025-4 S460ML
EN10025-6 EN10025-6 S460Q EN10025-6 S460QL EN10025-6 S460QL1 EN10025-6 S500Q
EN10025-6 S500QL EN10025-6 S500QL1 EN10025-6 S550Q EN10025-6 S550QL
EN10025-6 S550QL1 EN10025-6 S620Q EN10025-6 S620QL EN10025-6 S620QL1
EN10025-6 S690Q EN10025-6 S690QL EN10025-6 S690Q1 EN10025-6 S890Q
EN10025-6 S890QL EN10025-6 S890QL1 EN10025-6 S960Q EN10025-6 S960QL
JIS JIS G3101 JIS G3101 SS330 JIS G3101 SS400 JIS G3101 SS490 JIS G3101 SS540
JIS G3106 JIS G3106 SM400A JIS G3106 SM400B JIS G3106 SM400C JIS G3106 SM490A
JIS G3106 SM490YA JIS G3106 SM490B JIS G3106 SM490YB JIS G3106 SM490C
JIS G3106 SM520B JIS G3106 SM520C JIS G3106 SM570  
DIN DIN 17100 DIN17100 St52-3 DIN17100 St37-2 DIN17100 St37-3 DIN17100 RSt37-2
DIN17100 USt37-2      
DIN 17102 DIN17102 StE315 DIN17102 ESTE315 DIN17102 TStE315 DIN17102 WStE315
DIN17102 StE355 DIN17102 ESTE355 DIN17102 TStE355 DIN17102 WStE355
DIN17102 StE380 DIN17102 ESTE380 DIN17102 TStE380 DIN17102 WStE380
DIN17102 StE420 DIN17102 ESTE420 DIN17102 TStE420 DIN17102 WStE420
DIN17102 StE460 DIN17102 ESTE460 DIN17102 TStE460 DIN17102 WStE460
DIN17102 StE500 DIN17102 ESTE500 DIN17102 TStE500 DIN17102 WStE500
DIN17102 ESTE285      
GB GB/T700 GB/T700 Q235A GB/T700 Q235B GB/T700 Q235C GB/T700 Q235D
GB/T700 Q275      
GB/T1591 GB/T1591 Q345A GB/T1591 Q390A GB/T1591 Q420A GB/T1591 Q420E
GB/T1591 Q345B GB/T1591 Q390B GB/T1591 Q420B GB/T1591 Q460C
GB/T1591 Q345C GB/T1591 Q390C GB/T1591 Q420C GB/T1591 Q460D
GB/T1591 Q345D GB/T1591 Q390D GB/T1591 Q420D GB/T1591 Q460E
GB/T1591 Q345E GB/T1591 Q390E    
GB/T16270 GB/T16270 Q550C GB/T16270 Q550D GB/T16270 Q550E GB/T16270 Q550F
GB/T16270 Q620C GB/T16270 Q620D GB/T16270 Q620E GB/T16270 Q620F
GB/T16270 Q690C GB/T16270 Q690D GB/T16270 Q690E GB/T16270 Q690F
GB/T16270 Q800C GB/T16270 Q800D GB/T16270 Q800E GB/T16270 Q800F
GB/T16270 Q890C GB/T16270 Q890D GB/T16270 Q890E GB/T16270 Q890F
GB/T16270 Q960C GB/T16270 Q960D GB/T16270 Q960E GB/T16270 Q960F
GB/T16270 Q500