GB 713 18 Mnmonbr bostrovi va qozon go'shti po'latdagi kimyoviy tarkibi va mexanik mulk:
| Baho | C% | Si% | Mn% | CR% | Ni% | Mo% | NB% | V% | P% | S% | Alt% |
| 18 million | O.22 dan kam yoki teng | 0.15-0.50 | 1.20-1.60 | 0.45-0.65 | 0.025-0.050 | 0,020 dan kam yoki unga teng | 0,010 dan kam yoki unga teng | ||||
| Po'lat nav | Qalinligi, mmda | Mustahkamlik chegarasi | Kuch berish kuchi, min | Cho'zish,%, min |
| 18 million | 30<> | 570-720 | 400 | 17 |
| 60<> | 390 |
1. Issiqlik bilan qanday davolash kerak?
Javob:
Majburiy ishlov berish:
Qondiradigan(900-930 daraja suv purkagich)
Chang(1hr / 25mm uchun 600-650 daraja)
Ixtiyoriy SR(580-620 darajasi stressni engillashtirish darajasi)
2
Javob:
Tanqidiy mulohazalar:
Qizdirmoq: 150-200 daraja (barcha qalinliklar uchun)
Sarflangan materiallar: GB / T 5117 E6015-g yoki unga teng
Issiqlik kiritish: 1.2-2.0 kj / mm (qat'iy nazorat)
Qaytmoq: Majburiy (600-630 daraja × + 30 min / 25mm)
Test: 100% RT + 0 darajaga ta'sir qiladi
3. 18 millionbrygacha qayerda ishlatiladi?
Javob:
Kritik qo'llanmalar:
Vodorod reaktorlari(10-25mpa)
Ko'mirni suyultirish tomirlari
Yadroviy bug 'generatorlari
Qalin - devor gidrovacerckers (>150 mm)
Yuqori - harorat qozonlari(500 darajadan kam yoki unga teng)
Issiq teglar: GB 713 18 Bosim Bosim uchun mnmonbr, Xitoy GB {{1} {1} {1} {1} {1} {1} {1} {1} {1} {1}713 18 mnmonbr