SS400 SS490 H qismli po'lat ustun

Mahsulot: SS400 SS490 H qismli po'lat ustun
Standart: EN
Tolerantlik: ± 1%
So'rov yuborish
Hozir chat
Ta'rif
Texnik parametrlar

SS400 SS490 H qismli po'lat ustun


SS400 po'lat H nur birinchi S dedi po'lat (Po'lat), ikkinchi S "tuzilish" (Struktura), 400 400 valentlik kuchi pastki chegarasi uchun 400 MPa dedi, butun 400 MPa oddiy strukturaviy po'lat valentlik kuchi dedi. SS400 H po'lat po'latning o'zi nafaqat yuqori quvvatga ega, balki ma'lum pishiqlik, charchoqqa chidamlilik, zarba qarshiligi, korroziyaga chidamlilik, past{6}}harorat ta'siriga chidamlilik, payvandlash va oson ishlov berish va boshqa po'lat plitalarning keng qamrovli sifat ko'rsatkichlariga ega.


SS490 metall H nuri Yaponiya standarti uglerodli po'latdir, S dedi po'lat (Po'lat), ikkinchi S "tuzilish" (Tuzilish), 285 MPa kuchlanishning pastki chegarasi uchun 490, butun oddiy strukturaviy po'latning 490 MPa kuchlanish kuchi dedi. SS490 H shaklidagi po'lat yaxshi payvandlanish, ishlov berish va plastiklikka ega. SS490 H qismli nur yaxshi payvandlanishi, qayta ishlanishi va plastikligiga ega.

 

 
SS400 po'lat h ustunli kimyoviy tarkibi

 

C Maks. 16 mm dan kam yoki unga teng C>16 mm maksimal Si maks Mn maks P max. S maks.
0.17 0.20 – 1.40 0.045 0.045

 

 
SS490 strukturaviy h nurining kimyoviy tarkibi

 

Kimyoviy elementlar C Maks. 16 mm dan kam yoki unga teng C>16 mm maksimal Si
maks
Mn maks P
maks.
S
maks.
%, massa bo'yicha 0.24 0.24 0.55 1.60 0.045 0.045

 

 
h bo'limi po'lat nurlar o'lchamlari

 

Belgilash
Imperator
(x lb/ftda)

Chuqurlik
h
(in)
Kengligi
w
(in)
Veb qalinligi
tw
(in)
Flanj qalinligi
tf
(in)
Seksiya maydoni
(in2)
Og'irligi
(funtf/ft)
Statik parametrlar
Inersiya momenti Elastik kesim moduli
Ix
(in4)
Iy
(in4)
Sx
(in3)
Sy
(in3)
W 27 x 178 27.8 14.09 0.725 1.190 52.3 178 6990 555 502 78.8
W 27 x 161 27.6 14.02 0.660 1.080 47.4 161 6280 497 455 70.9
W 27 x 146 27.4 14 0.605 0.975 42.9 146 5630 443 411 63.5
W 27 x 114 27.3 10.07 0.570 0.930 33.5 114 4090 159 299 31.5
W 27 x 102 27.1 10.02 0.515 0.830 30.0 102 3620 139 267 27.8
W 27 x 94 26.9 10 0.490 0.745 27.7 94 3270 124 243 24.8
W 27 x 84 26.7 9.96 0.460 0.640 24.8 84 2850 106 213 21.2
                     
W 24 x 162 25 13 0.705 1.220 47.7 162 5170 443 414 68.4
W 24 x 146 24.7 12.9 0.650 1.090 43.0 146 4580 391 371 60.5
W 24 x 131 24.5 12.9 0.605 0.960 38.5 131 4020 340 329 53.0
W 24 x 117 24.3 12.8 0.55 0.850 34.4 117 3540 297 291 46.5
W 24 x 104 24.1 12.75 0.500 0.750 30.6 104 3100 259 258 40.7
W 24 x 94 24.1 9.07 0.515 0.875 27.7 94 2700 109 222 24.0
W 24 x 84 24.1 9.02 0.470 0.770 24.7 84 2370 94.4 196 20.9
W 24 x 76 23.9 9 0.440 0.680 22.4 76 2100 82.5 176 18.4
W 24 x 68 23.7 8.97 0.415 0.585 20.1 68 1830 70.4 154 15.7
W 24 x 62 23.7 7.04 0.430 0.590 18.2 62 1550 34.5 131 9.8
W 24 x 55 23.6 7.01 0.395 0.505 16.2 55 1350 29.1 114 8.3

 

 
h shaklidagi temir nurli mahsulot tasviri

 

China H shaped steel makers

 

 
GNEE guruhi jamoasi fotosurati

 

China H column steel producers

 

 
GNEE guruhi mijozlariga tashrif buyurish

 

China h type steel beam producers

China Structural Steel Beams makers

Bizda professional onlayn xizmat xodimlari mavjud. Agar sizda SS400 SS490 H Section Steel Column haqida savollaringiz bo'lsa, iltimos, bizga so'rov yuboring va biz sizga bir ish kuni ichida javob beramiz.

 

Issiq teglar: ss400 ss490 h qismli po'lat ustun, Xitoy ss400 ss490 h qismli po'lat ustun ishlab chiqaruvchilar, etkazib beruvchilar, zavod