Mahsulot: 316L zanglamaydigan po'latdan yasalgan nurlar
Darajasi: 316L
Standart: ASTM JIS
Tolerantlik: ± 1%
So'rov yuborish
Hozir chat
Ta'rif
Texnik parametrlar

316L zanglamaydigan po'latdan yasalgan nurlar


316L zanglamaydigan po'latdan yasalgan H nuri oziq-ovqat xizmati, kimyo, farmatsevtika va boshqalarni o'z ichiga olgan turli sohalarda va ilovalarda qo'llanilishi mumkin. Zanglamaydigan po'latdan H-nurlar ekstrudirovka qilingan, issiq haddelenmiş yoki lazerli eritilgan bo'lishi mumkin. Zanglamaydigan po'latdan yasalgan H bo'limi yuqori haroratga, korroziyaga chidamliligi va past haroratlarda mukammal mustahkamligi va mustahkamligi tufayli turli sanoat va ilovalar uchun idealdir.

 

 
316L po'latdan yasalgan h nurning kimyoviy tarkibi

 

Baho   C Mn Si P S Cr Mo Ni N
316L Min - - - - - 16.0 2.00 10.0 -
Maks 0.03 2.0 0.75 0.045 0.03 18.0 3.00 14.0 0.10

 

 
316L h qismli po'latdan mexanik xususiyat

 

Baho Uzilish Str (MPa) min Hosildorlik Str 0,2% Proof (MPa) min Cho'zilish (% 50 mm) min Qattiqlik
Rokvell B (HR B) maks Brinell (HB) maks
316L 485 170 40 95 217

 

 
316L h shaklidagi po'latning jismoniy xususiyatlari

 

rade Zichlik (kg/m3) Elastik modul (GPa) Issiqlik kengayishining o'rtacha ko-effisi (mkm/m/daraja) Issiqlik o'tkazuvchanligi (Vt/mK) Maxsus issiqlik 0-100 daraja (J/kg.K) Elektr qarshiligi (nŌ.m)
0-100 daraja 0-315 daraja 0-538 daraja 100 daraja haroratda 500 daraja haroratda
316L 8000 193 15.9 16.2 17.5 16.3 21.5 500 740

 

 
316L konstruktiv po'lat h nurlarining o'lchamlari

 

Hajmi
(mm)
Nazariy vazn
(kg/m)
Hajmi
(mm)
Nazariy vazn
(kg/m)
Hajmi
(mm)
Nazariy vazn
(kg/m)
100*50*5*7 9.3 250*125*6*9 29 446*199*8*12 65.1
100*100*6*8 16.9 250*250*9*14 71.8 450*200*9*14 74.9
125*60*6*8 13.1 294*200*8*12 55.8 482*300*11*15 110.8
125*125*6.5*9 23.6 298*149*5.5*8 32 488*300*11*18 124.9
148*100*6*9 31.1 340*250*9*14 36.7 496*199*9*14 77.9
150*75*5*7 14 300*150*6.5*9 93 500*200*10*16 88.1
150*150*7*10 20.7 300*300*10*15 78.1 582*300*12*17 132.8
175*90*5*8 18 346*174*6*9 41.2 588*300*12*20 147
175*175*7.5*11 40.4 350*175*7*11 49.4 596*199*10*15 92.4
194*150*6*9 29.9 350*350*12*19 134.9 600*200*11*17 103.4
198*99*4.5*7 17.8 390*300*10*16 104.6 700*300*13*24 181.8
200*100*5.5*8 20.9 396*199*7*11 56.1 800*300*14*26 206.8
200*200*8*12 49.9 400*200*8*13 65.4 900*300*16*28 240.1
244*175*7*11 43.6 400*400*13*21 171.7    
248*124*5*8 25.1 440*300*11*18 120.8    

 

 
316L h nurli po'lat strukturasi Mahsulotlar tasviri

 

China H section steel makers

 

 
GNEE guruhi jamoasi fotosurati

 

China H shaped steel Distributors

 

 
GNEE guruhi mijozlariga tashrif

 

China h type steel beam producers

Bizda yetarlicha 316L zanglamaydigan po'latdan yasalgan nurlar mavjud va biz uni sizning ehtiyojlaringizga ko'ra sozlashimiz mumkin.

 

 

Issiq teglar: 316l zanglamaydigan po'latdan yasalgan nurlar, Xitoy 316l zanglamaydigan po'latdan yasalgan nurlar ishlab chiqaruvchilar, etkazib beruvchilar, zavod